Oxide scale in X45NiCrMo4 steel


Figure 1: Oxide scale in steel, scale bar: 500 µm.

Inclusion name: Iron oxide
Record No.: 1490
Inclusion formula: No data
Inclusion type (Macro/Micro/Nano): Macro
Inclusion type (Exogenous/Indigenous): Exogenous
Inclusion classification: Oxide
Inclusion composition in weight %: No data
Sample: X45NiCrMo4 steel
Steel composition in weight %: 0.45% C, 0.24% Si, 0.27% Mn, 0.011% P, 0.005% S, 1.31% Cr, 4.00% Ni, 0.18% Mo, 0.11% Cu, 0.008% Al.
Note: Nickel cold work tool steel
Reference: Not shown in this demo version.