Slag inclusion in AISI H13 steel


Figure 1: Slag inclusion in steel, scale bar: 50 µm.

Inclusion name: Slag inclusion
Record No.: 1515
Inclusion formula: No data
Inclusion type (Macro/Micro/Nano): Macro
Inclusion type (Exogenous/Indigenous): Exogenous
Inclusion classification: Oxide
Inclusion composition in weight %: No data
Sample: AISI H13 steel
Steel composition in weight %: 0.40% C, 1.02% Si, 0.38% Mn, 0.014% P, 0.002% S, 5.12% Cr, 0.10% Ni, 1.25% Mo, 1.02% V, 0.15% Cu, 0.0135 Al.
Note: Hot work tool steel
Reference: Not shown in this demo version.