MnS in iron
Figure 1: Sulfide particles in iron after an addition of Mn only (left Fig.) and after adding Mn+Al (right Fig.), Arnold and Bolsover, Mag. 225 X.
Inclusion name: Manganese sulfide
Record No.: 204
Inclusion formula: MnS
Inclusion type (Macro/Micro/Nano): No data
Inclusion type (Exogenous/Indigenous): No data
Inclusion classification: Sulfide
Inclusion composition in weight %: No data
Sample: Iron
Steel composition in weight %: No data
Note: No data
Reference: Not shown in this demo version.