Melting points and density of non-metallic inclusion
Reference: 1.) T. Gladman, The Physical Metallurgy of Microalloyed
Steels, University Press, Cambridge, 1997. 2.) K. Bolanowski, Influence of rare-earth elements on the
structure and properties of steel, Metallurgical News 7-8, (2004) 323-325 (in Polish). 3.) M. Opiela, A. Grajcar, Modification of Non-Metallic Inclusions by
Rare-Earth Elements in Microalloyed Steels, ARCHIVES of FOUNDRY ENGINEERING Volume 12 , Issue 2/2012, 129-134.