Corner cracks - Slab defects
Figure 1: Corner cracks.
Defect name: Corner cracks
Record No.: 2006
Type of defect (Internal/Surface): Surface
Defect classification: Slab defects
Steel name: Steel
Steel composition in weight %: No data.
Note: Causes: Narrow face bulging, insufficient taper, insufficient cooling, reheating. Can extendto slabsurfaceand cause a breakout.
Reference: Not shown in this demonstration version.