Cracked upset forged EX33 - Forging defects
Figure 1: The cracking was located by oxide inclusions in the steel.
Defect name: Cracks
Record No.: 2222
Type of defect (Internal/Surface): Internal, surface
Defect classification: Forging defects
Steel name: Steel
Steel composition in weight %: No data.
Note: Materials problems.
Reference: Not shown in this demonstration version.