Adhesion failure - Coating defects
Figure 1: Paintfails to adhere to substrate or underlying coats of paint.
Defect name: Adhesion failure
Record No.: 3057
Type of defect (Internal/Surface): Surface
Defect classification: Coating defects
Steel name: Steel
Steel composition in weight %: No data.
Note:
Probable causes: Surface contamination or
condensation, incompatibility between coating
systems, or exceeding the overcoating time.
Prevention: Ensure that the surface is clean, dry, and
free from any contamination and that the surface has
been suitably prepared. Use the correct coating
specification and follow the advised overcoating
times.
Reference: Not shown in this demonstration version.