Alligatoring in a rolled slab - Rolling defects
Figure 1: Alligatoring in a rolled slab. This defect is thought to be caused by
nonhomogeneous deformation and nonuniform recrystallization during
primary rolling.
Defect name: Alligatoring
Record No.: 3102
Type of defect (Internal/Surface): Surface
Defect classification: Rolling defects
Steel name: Steel
Steel composition in weight %: No data.
Note: Another rolling defect whose source is metallurgical is alligatoring
(Fig. 1).