Pick-up - Other defects
Figure 1: Pick-up.
Defect name: Pick-up
Record No.: 366
Type of defect (Internal/Surface): Surface
Defect classification: Other defects
Steel name: Steel
Steel composition in weight %: No data.
Note: Small tears in the sheet surface caused by similar
scores in the surface of the roller leveller and pinch
rolls. This defect is illustrated in Figs 1.
Reference: Not shown in this demonstration version.