CODIXX AG produces dichroic glass polarizers resistent against UV-radiation, chemicals and temperatures up to 400 Celsius in the UV, VIS and IR range. CODIXX produces polarizers with patterns of neighbouring areas with a different orientation of the polarization and/or wavelength of maximum polarization.