Anosovite



Chemical formula: Ti3O5
Modifications: Alpha-Ti3O5 Anosovite I, beta-Ti3O5 Anosovite II
Melting point: No data
Density: No data
Microhardnes: No data
Hardness (Moh's): XXX
Luminescence: No data
Crystal system: Tetragonal
Cell dimensions: a=9.474 A, b=9.734 A, c=3.754 A
PDF number: 00-009-0309
ICSD number: 020361
Note: Occurs in Ti-rich slags.