Steel Index

0.1% Si steel
0.28% carbon aluminum killed steel
0.3% C steel, 31-ton polygonal steel ingots
0.3% C steel, 31-ton polygonal steel ingots
0.5% C rimming steel, as cast
0.5% C rimming steel, as cast
0.5Cr-0.5Mo-0.25V steel
1.0037 steel
1.0301 steel
1.0330 steel, yeear of production: 1957
1.0715 steel
1.1191
1.1191
1.1191
1.1201, 1.7139, 1.7225 steels
1.2312 steel
1.2343 steel
1.2375 steel
1.3302 steel
1.3343 steel
1.3346 steel
1.3520 (100CrMn6/100CrMnSi6-4) steel
1.4016 steel
1.4105 steel (X4CrMoS18/X6CrMoS17)
1.4301 (X5CrNi18-10/X4CrNi18-10) steel
1.4301 steel
1.4512 steel
1.4529
1.4718 (X45CrSi9-3) steel
1.4872 (X25CrMnNiN25-9-7) steel
1.4938 + Zr steel
1.4938 steel
1.5919 (15CrNi6) steel
1.7225 steel
1.7225 steel
1.7225 steel
1.7707 (30CrMoV9) steel
1.8519 steel
100Cr6 (1.3505) steel
100Cr6 rolling bearing steel
100Cr6 rolling bearing steel
100Cr6 rolling bearing steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100Cr6 steel
100CrMo7 bearing steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S billet sample, high strength low alloy (HSLA) steel
1018S furnace tap sample, high strength low alloy (HSLA) steel
1018S furnace tap sample, high strength low alloy (HSLA) steel
1018S furnace tap sample, high strength low alloy (HSLA) steel
1018S high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle sample, high strength low alloy (HSLA) steel
1018S ladle tap sample, A529 tundish sample, high strength low alloy (HSLA) steel
1018S ladle tap sample, high strength low alloy (HSLA) steel
1018S ladle tap sample, high strength low alloy (HSLA) steel
1018S ladle tap sample, high strength low alloy (HSLA) steel
1018S tundish sample, high strength low alloy (HSLA) steel
10CrMo9-10 steel
10CrMo9-10 steel
10G2FB low-alloy high strength steel
11SMn37steel, free-cutting steel
11SMnPb37 steel
12 wt% Cr steel (3CR12)
12Cr steel
12Cr13 stainless steel
12Cr2Mo1 steel
13HMF and 316L steels
142W13 steel
145Cr6 steel
150 kg test ingots of resulphurized 18Cr2MoTi steel with different Mn and Ti contents
16MnCr5 steel
16MnCr5 steel
16MnCr5 steel
16MnCr5 steel
16MnCr5 steel
16MnCr5 steel
16MnCrB steel
17CrMo4 steel
17CrMo4 steel
17CrMo4 steel
18Cr8Ni stainless steels (1.4301 and 1.4305)
18CrNi8 steel
18G2A steel
2.25Cr1Mo steel
2000 MPa grade spring steel
20Mn6 steel (Mat. No. 1.1169)
20MnCrS5 steel
20NiCrMo steel
21% Cr ferritic stainless steel
21Cr–11Ni austenitic heat-resistant stainless steel
21NiCrMo2 steel
22GYu, 10G2FB, 09GSF steels
25% Cr duplex stainless steel
25Cr-20Ni steel
25MnCrSiVB6 steel
25MnCrSiVB6 steel
280 and 316L steels
280M and 280R steels
30%Ni–19%Cr steel
300M (40CrNi2Si2MoVA) steel
304 stainless steel
304 stainless steel
304 stainless steel
304 stainless steel
304L, 316L and S32304 steels
304L, 316L and S32304 steels
304L, 316L and S32304 steels
30CrMoV9 steel
30CrMoV9 steel
30CrNiMo8 steel
30CrNiMo8 steel
30CrNiMo8 steel
30CrNiMo8 steel
30MnVS6 steel
316 type stainless steel
316Ca and 316R steels
316F stainless steel
316F stainless steel
316L austenitic stainless steel powder
316L austenitic stainless steel powder
316L austenitic stainless steel powder
316L industrial steel
316L stainless steel
316L stainless steel
316L stainless steel
316LC stainless steel
316LC stainless steel
32CrMoV12-10 steel
32CrMoV12-10 steel
347 stainless steel
34CrMo4 steel
34CrMo4 steel
34CrNiMo6 steel
34CrNiMo6 steel
34CrNiMo6 steel
35B2+Cr steel
35B2+Cr steel
35CrNi3MoV steel
35CrNi3MoV steel
35MnVS steel
36MnVS4 steel
38MnS6 steel
39Mn2V steel
3Cr-Mo steel, cold work tool steel
409L stainless steel
409L stainless steels
409L stainless steels
409L stainless steels
40CrMnMoS8-6 steel
40CrMnMoS8-6 steel
40CrMnMoS8-6 steel
40CrMnMoS8-6 steel
40CrMnMoS8-6 steel
410L stainless steel
4120 and 4140 steels
4140 steel
41CrAlNi7 steel
41CrAlNi7 steel
41CrAlNi7 steel
42CD4 steel
42CD4 steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo alloyed structural steel
42CrMo steel
42CrMo4 and 157C steels
42CrMo4 and 157C steels
42CrMo4 steel
42CrMo4 steel
42CrMo4 steel
42CrMo4 steel
42CrMo4 steel
42CrMo4 steel
42CrMoS4 steel
42CrMoS4 steel
42CrMoVNb steel
430 stainless steel
430 stainless steel
430 stainless steel
430 stainless steel
430 stainless steel
430 stainless steel
430 stainless steel
4340 steel
440 MPa-class plain carbon steel
44MnSiVS6 steel
45H3M1F steel
4J43 alloy (42% nickel-iron binary alloy)
4J43 alloy (42% nickel-iron binary alloy)
4J43 alloy (42% nickel-iron binary alloy)
4J43 alloy (42% nickel-iron binary alloy)
4J43 alloy (42% nickel-iron binary alloy)
4LR60 stainless austenitic steel
5% Cr steel
50CrMoV13-1 steel
50CrMoV13-1 steel
50CrMoV13-1 steel
50CrMoV13-1 steel
50CrMoV13-1 steel
51CrV4 (1.2241), spring steel
51CrV4 spring steel
51CrV4 spring steel
51CrV4 spring steel
51CrV4 spring steel
51CrV4 steel
51CrV4 steel
55SiCr6 steel
57SiCr6D, 3613, 100Cr6 steels
60Si2CrV steel
803J bearing steel
803J bearing steel
803J bearing steel
803J bearing steel
86CrMoV7 steel
86CrMoV7 steel
86CrMoV7 steel
18Ch2MFA steel
9%Cr-Mo-Co-B (CB2) steel
90MnCrV8 steel
90MnCrV8 steel
90MnCrV8 steel
9Cr-1Mo steel
9Cr3W3CoVNbBN steel
9SMn28 steel
A broken steel roll
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 billet sample, high strength low alloy (HSLA) steel
A529 furnace tap sample, high strength low alloy (HSLA) steel
A529 furnace tap sample, high strength low alloy (HSLA) steel
A529 ladle sample, high strength low alloy (HSLA) steel
A529 ladle tap sample, high strength low alloy (HSLA) steel
A529 ladle tap sample, high strength low alloy (HSLA) steel
A529 steel, high strength low alloy (HSLA) steel
A529 steel, high strength low alloy (HSLA) steel
A529 tundish sample, high strength low alloy (HSLA) steel
A529 tundish sample, high strength low alloy (HSLA) steel
A529 tundish sample, high strength low alloy (HSLA) steel
A533B pressure vessel steel
A537 steel
ABNT 4133 modified steel (API 5CT)
Acid open hearth steel, killed (ballbearing steel)
Advanced high-strength steels (AHSS), 3Mn, 3MnNb, 5Mn, 5MnNb steels
AH36 steel
AISI 1005
AISI 1020 electrode
AISI 1020 electrode
AISI 1020 electrode
AISI 1020 ESR steel electrode
AISI 1020, 304 steels
AISI 1035 steel
AISI 1040 steel
AISI 1095 steel (1.1275), high carbon steel
AISI 10B22 steel
AISI 1144 steel
AISI 1213 free-machining carbon steel, free-machining austenitic stainless steel
AISI 1214 free-machining steel
AISI 12L14(JIS SUM24L) steel
AISI 12L14, JIS SUM24L
AISI 1536 steel
AISI 303 austenitic stainless steel
AISI 303 stainless steel
AISI 303 steel
AISI 303 steel
AISI 303 type steel
AISI 303, 315 and 319 steels
AISI 304 stainless steel
AISI 304 stainless steel
AISI 304 stainless steel
AISI 304 stainless steel
AISI 315 and 319 steels
AISI 316 L stainless steel
AISI 316 steel
AISI 316L stainless steel
AISI 316L stainless steel
AISI 316L stainless steel
AISI 4137-H steel
AISI 416 stainless steel
AISI 4335 steel
AISI 4335 steel
AISI 4340 steel
AISI 52100 steel, 100Cr6
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI 8620 carburizing steel
AISI A2 steel
AISI A2 steel
AISI D2 Steel
AISI D2 Steel
AISI D2 steel
AISI D2 steel
AISI D2 steel
AISI D2 steel
AISI D2 steel
AISI D2 tool steel
AISI D3 steel
AISI H11 hot work tool steel
AISI H13 hot work tool steel
AISI H13 hot work tool steel
AISI H13 steel
AISI H13 steel
AISI H13
AISI H13
AISI O1 steel
AISI O2 steel
AISI S7 steel
AISI stainless steel
AISI T42 steel
AK steel
Al deoxidized ESR ingots
Al killed steel
Al-deoxidized steel ingot
Al-Fe alloy
Al-killed steel
Al-killed Ti bearing steel
Al2O3-CaO
Al2O3-CaO
Al2O3-CaO
Al2O3-CaO
Alloyed tool steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium killed steel
Aluminium-killed low carbon (0.05% C) steel
Aluminium-killed low carbon (0.05% C) steel
Aluminum killed steels (LCAK)
API 5L X65 steel
API 5LX65 steel
API X70 linepipe steel
Armco steel
Armor steel
As-cast Fe-Mn-Al-C-Si alloy
As-cast gray iron
As-cast gray iron
ASI 416 steel
ASTM 235-55 low-carbon steel
ASTM A216 steel
ASTM A36 steel grade
ASTM A36 steel
ASTM A504 rail steel
ASTM A516 steel plate
ASTM A533 GrB (UNS K12539) low-alloy steel
Austenitic manganese steel, as-cast
Austenitic manganese steel, as-cast
Austenitic manganese steel, as-cast
Austenitic manganese steel, as-cast
Austenitic manganese steel
Austenitic stainless steel, after forging and annealing
Austenitic stainless steel, CaSi deoxidized
Austenitic stainless steel, CaSi-deoxidized
Austenitic stainless steel, cold-rolled steel
Austenitic stainless steel, deoxidized and titanium stabilized
Austenitic stainless steel, multi-phase high-temperature alloys
Austenitic stainless steel, niobium stabilized, as cast
Austenitic stainless steel, rolled billet
Austenitic stainless steel, vacuum cast
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic stainless steel
Austenitic steel
AWS E 11018M type electrode
Bainitic steel
Basic arc-melted Cr-steel
Basic Bessemer steel during the blow
Basic Bessemer steel
Basic Bessemer steel
Basic electric austenitic stainless steel
Basic electric steel, Al and ferro-silicon killed
Basic electric steel, Al-killed
Basic electric steel, Al-killed
Basic electric steel, from billet
Basic electric steel, killed
Basic electric steel, Si-killed with a limited Al addition
Basic electric steel, Si-killed with a limited Al addition
Basic electric steel, Si-killed with a limited Al-addition
Basic electric steel, Si-killed with a limited Al-addition
Basic electric steel, Si-killed, from ingot
Basic electric steel, Si-killed, inclusion isolated from the lower central part of a top cast 6 ton ingot
Basic electric steel, Si-killed, inclusion isolated from the lower central part of a top cast 6 ton ingot
Basic electric steel, Si-killed, inclusion isolated from the lower central part of top cast 6 ton ingot
Basic electric steel, Si-killed. Inclusion isolated from ingot
Basic electric steel, Si-killed. Inclusion isolated from ingot
Basic electric steel, Si-killed. The inclusions have been isolated from the lower central part of a top cast 6 ton ingot
Basic electric steel. From a surface of crack in the ingot
Basic electric steel. From billet
Basic high-speed steel. From billet
Basic Kaldo steel, sem-killed. From ingot
Basic Kaldo steel, semi-killed. From ingot
Basic open hearth steel, Al-killed. From rolled plate
Basic open hearth steel, ferro-silicon killed before tapping and aluminium killed in the ladle
Basic open hearth steel, ferro-silicon killed before tapping and aluminium killed in the ladle
Basic open hearth steel, ferro-silicon killed before tapping, after killed with aluminium
Basic open hearth steel, ferrosilicon killed before tapping, after killed with aluminium
Basic open hearth steel
Basic open-heart steel, ferrosilicon killed before tapping and aluminium killed in the ladle
Basic open-hearth steel, ferrosilicon killed before tapping, after killed with aluminium
Basic open-hearth steel, ferrosilicon-killed before tapping and aluminium-killed in the ladle
Bearing steel
Bearing steel
Bearing steel
Bearing steel
Bearing steel
Bearing steel
Bearing steel
Blast furnace pig iron
Blister sample
BN1 steel
BOF slag
BOF slag
BOF slag
BOF slag
Boron steel
Brick (refractory)
C-Mn-B steel
C-Mn-B steel
C-Mn-Si steel with Nb and Ti
C300 maraging steel
C45 steel
C45BN steel
Ca-modified weathering steel
Ca-modified weathering steel
Ca-treated Al killed low carbon steel (CaLCAK)
Ca-treated Al killed low carbon steel (CaLCAK)
Calcium treated Al-killed steel
Calcium treated steel
Calcium-Modified Weathering Steel
Carbon constructional steel, as cast
Carbon manganese steels
Carbon steel casting. Manganese silicon killed carbon steel
Carbon steel casting
Carbon steel casting
Carbon steel ingot, cast from the bottom
Carbon steel ingot, cast from the bottom
Carbon steel steel
Carbon steel, annealed in oil-gas-heated furnace
Carbon steel, annealed in oil-gas-heated furnace
Carbon steel, annealed in oil-gas-heated furnace
Carbon steel, annealed in oil-gas-heated furnace
Carbon steel, CaSi deoxidized, from ingot
Carbon steel, deoxidized with CaSi
Carbon steel, deoxidized with SiCa in the ladle and Al in the mould
Carbon steel, from ingot
Carbon steel, killed
Carbon steel. From a forged chain link
Carbon steel. From a hot-rolled billet
Carbon steel. From rolled plaste steel
Carbon steel. Welded cross test piece with cracks in the welding zone
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steel
Carbon steels
Case carburising steels
CaSi ferroalloy
Cast hot work tool steel
Cast ingot
Cast iron
Cast niobium microalloyed steel
Cast of carbon steel, high in sulfur
Cast steel, Al-deoxidized
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
Cast steel
CC040A grade steel
Ck45 steel
Clogging samples
Co-free low-Ni maraging steel
Cold rolled 0.5% Si steel
Cold rolled steel sheet
Cold rolled steel sheet
CON and CAT steels
Constructional steel
Constructional steel
Constructional steel
Constructional steel
Constructional steel
Constructional steel
Constructional steel
Continuous casting silicon steel
Convertor steel, from rolled bar
Corus and Uddeholm steels
Cr steel
Cr-Co and Cr-Cu-Ni steels
Cr-Mn steel
Cr-Mn steel
Cr-Mn steel
Cr-Mo alloy steel
Cr-Mo plastic mold steel
Cr-Mo steel, Al killed, as cast
Cr-Mo steel
Cr-Mo-V-B steel
Cr-Mo-V-B steel
Creep resistant steels
CRM 035-2 certified reference material
CRM 059-2 certified reference material
CrMo and CrMoV steels
CrMo and CrMoV steels
Cu bearing duplex stainless steel
CuLC steel
C–Mn ship structural steel
C–Mn–Si steel
Degasalt sample
DEW steel
DIEVAR steel
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Different steels. Medium carbon aluminium killed (MCAK), low carbon silicon-aluminium killed (LCSAK), low carbon aluminium killed (LCAK) steels
Diffusion bonded sponge or water atomized metal powder
Dolomite, refractory
DP-Type and TRIP-Type cold rolled steel sheet
DP-Type and TRIP-Type cold rolled steel sheet
Drawn wire steel
Ductile cast iron
Ductile cast iron
Ductile cast iron
Ductile cast iron
Ductile iron
Ductile iron
Ductile iron
Ductile iron
Ductile iron
E911, CB2, FB2, 1.4910 (X3CrNiMoN17-13) steels
EAF 1 slag
EAF slag 1
EAF slag 1
EAF slag 1
EAF slag/Chromium containing spinel
EAF slag
EAF slag
EAF slag
EAF slag
Electric quality sheet steels
Electric steel
Electric steel
Electrical steel, 50CS1300
Electrical steel
Electrical steel
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron + Ti (Fe-Ti melt)
Electrolytic iron with
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic iron
Electrolytic pure iron
Electrolytic pure iron
Electrolytic pure iron
Electrolytic pure iron
Electrolytic pure iron
Electrolytically precipitated iron (Orkla iron)
Electrosteel, CaSi deoxidized
ESR ingots Al-deoxidized
ESR ingots Al-deoxidized
ESR ingots Al-deoxidized
ESR slag
ESR steel
ESR steel
ESR steel
ESR steel
ESR steel
ESR steel
Experimental steel
F82H-IEA steel
F82H-IEA steel
Fe-10% Ni alloy
Fe-10mass% Ni alloy
Fe-30Mn-9Al-1Si-0.9C-0.5Mo steel
Fe-30Mn-9Al-1Si-0.9C-0.5Mo steel
Fe-Al alloys
Fe-Al alloys
Fe-Cr steel, induction melted and remelted in a high vacuum consumable arc furnace
Fe-Cr-Ni stainless steel
Fe-Cr-Ni stainless steel
Fe-Cu-Sn alloy
Fe-Mn-S alloy
Fe-Ni alloy
Fe-Ni alloy
Fe-Ni alloy
Fe-Ni-Mn alloy
Fe-Ni-Mn alloy
Fe-O alloy
Fe-O alloy
Fe-O alloy
Fe-O alloy
Fe-P alloy
Fe-P-C alloy
Fe-S alloys
Fe-S-C alloy
Fe-S-C alloy
Fe-S-C alloy
Fe-S-C alloy
Fe-S-O specimen
Fe-Si-O specimen
Fe-Ti alloy
Fe-Ti alloy
Ferritic stainless stee
Ferritic stainless stee
Ferritic stainless steel
Ferritic stainless steel
Ferritic stainless steels
Ferroalloy FC800-ferrochromium
Ferroalloy FeTi70R
Ferroalloy
Ferroalloys
Ferrochromium affine
Ferrochromium suraffine
Ferrochromium suraffine
Ferrochromium suraffine
Ferrochromium suraffine
Ferrochromium surafine
Ferrochromium
Ferrochromium
Ferromanganese
Ferromanganese
Ferromanganese
Ferromanganese
Ferrotitanium
Ferrovanadium
Fe–10Cr alloy
Fe–Al–Ti steels
Fe–Al–Ti–O specimens
Fe–Al–Ti–O specimens
Fe–Al–Ti–O specimens
Fe–Ni alloy
Free-cutting steel
Free-cutting steel
Flange cracked can, steel
Forged steel
Forged wrought steel
Free cutting higher sulphur steel
Free cutting steels
Free cutting steels
Free-cutting steel, rolled bar
Free-cutting steel
Free-machining steel treated with the bismuth
Free-machining steel
Free-machining steel
Free-machining steel
Free-machining steel
Free-machining steel
Free-machining steel
Furnace slag
Fused together from equal parts FeS and MnO
FV520B steel
G42CrMo4 cast steel
Gas atomized high speed steel powder
Gas atomized metal powder
Gas atomized metal powder
Gas purging plugs
GCr15 steel
GP240GH and G17CrMo5-5 cast steels
Grade-X steel
Gray iron
Gray iron
Gray iron
Grey cast iron
Grey cast iron
Grey cast iron
Grey cast iron
GS-38 steel
GX2CrNiMo18-14-3 cast steel
GX3CrNiMoN17-13-5 cast steel
H11 tool steel
H13 (+Bi) steel
H13 tool steel
High carbon steel
High carbon steel
High carbon wire rod steel
High carbon wire rod steel
High carbon wire rod steel
High carbon wire rod steel
High chromium steel slab
High chromium steel with telluriumm ferritic Mild steel, resulphurized with Te
High manganese austenitic steel
High manganese TWIP steels
High Mn TWIP steels
High speed steel powder compacts, compacted from surface oxidized powder with 0.098% O
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder, Speedsteel ASP 23
High speed steel powder
High speed steel, from the centre of a rolled bar
High speed steel
High speed steel
High speed steel
High strength cast steel
High strength low alloy (HSLA) steel
High strength steel
High temperature austenitic stainless steel
High-carbon steel, 6 ton melts, convertor, deoxidation with Al and REM
High-Cr ferritic stainless steel
High-Cr ferritic stainless steel
High-Cr ferritic stainless steel
High-manganese and aluminum-alloyed austenitic steels
High-purity electrolytic iron
High-silicon non-calcium treated (HSiNC) stainless steel
High-speeed steels (I10CR8DV, I8CR10D)
High-strength low-alloy steel weld metals
HSLA and HR TRIP 800 steels
HSLA steel
HSLA steel
HSLA steel
HSLA-100 steel
HT780MPa class high strength steel
Hull rivet steel of RMS Titanic
Hull steel of RMS Titanic
Hull steel of RMS Titanic
IF steel, slab
IF steel
IF steel
IFHS steel
Ingot
Ingot
Ingot
Ingot
Ingot
Interface Ti3O5 crucible/Fe-Ni-Ti sample
Iron powder. Fe often with C, Cu, P, and/or Ni and Mo
Iron powder
Iron powder
Iron powder
Iron powder
Iron powder
Iron powder
Iron powder
Iron-Aluminium alloy
Iron-Aluminium alloy
Iron
Iron
Iron
Iron
Iron
Japanese sword
JIS S10C steel bar
JIS SCM435 steel
JIS SUM23 steel
JIS-SCM440 steel
JIS-SCM440 steel
K1040-type steel
Kaldo steel, CaSi killed in ladle
Kaldo steel, CaSi-killed in ladle
Kaldo steel, CaSi-killed in ladle
Lab samples
Laboratory 6 kg ingot of electrolytic iron
Laboratory melt of burnt dolomite in a pure alumina crusible
Laboratory steel ingot
Laboratory steel sample
Ladle refractory
Ladle slag
Ladle steel
Lancashire iron. Inclusion from the fining process
Lancashire iron. Inclusion from the fining process
Lancashire iron. Slag from tapping bar
Lancashire slag
Lancashire slag
LC-steel
LCAK (low carbon aluminium killed)steel
LCAK (low carbon aluminium killed)steel
LCAK and stainless steels
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LCAK steel
LF steel
LF steel
Line pipe steel
Line pipe steel
Line pipe steel
Low alloy steel
Low alloy steel
Low alloy steel
Low alloy steel
Low alloy steel
Low alloy steel
Low alloy steel
Low alloyed chromium steel
Low alloyed electric steel
Low alloyed steel
Low alloyed steel
Low alloyed steel
Low C-Mn steel
Low carbon AISI 316 nuclear grade stainless steel
Low carbon Al-killed steel (LCAK steel)
Low carbon Al-killed steel (LCAK steel)
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steel
Low carbon aluminium killed (LCAK) steels
Low carbon aluminium killed (LCAK) steels
Low carbon aluminium killed (LCAK) steels
Low carbon aluminium killed (LCAK) steels
Low carbon aluminium killed (LCAK) steels
Low carbon aluminium killed steel
Low carbon aluminum killed steel
Low carbon and ultra-low carbon steels
Low carbon free cutting steels
Low carbon grade of steel for CO2 welding wire rods
Low carbon grade of steel for CO2 welding wire rods
Low carbon high manganese steels
Low carbon Nb–Ti microalloyed steel
Low carbon steel (SS400)
Low carbon steel strip
Low carbon steel with Ce and As
Low carbon steel with higher Cu
Low carbon steel, 27MnSiVS steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low carbon steel
Low C–Mn–V steel
Low-alloy chromium steel
Low-alloy steel weld
Low-alloy steel
Low-alloyed chromium steel
Low-carbon Al-killed steel
Low-carbon Al-killed steels
Low-carbon microalloyed steel
Low-carbon steel microalloyed with Nb, V and Ti
M2 steel
Magnesite brick (refractory)
Magnesite, refractory bricks
Magnetite electrode with approx. 90% Fe3O4 and 10% siliceous binder
Malleable iron
Manganese silicon killed carbon steel
Manganese silicon killed steel
Manganese steel, Al killed, after hot working
Manganese steel, Al killed, hot worked
Manganese-silicon killed carbon steel
Master alloys of Fe–30 mass% Cr and Fe–4 mass% Ti were made by melting high purity iron (99.99 mass% purity)
Master alloys of Fe–30 mass% Cr and Fe–4 mass% Ti were made by melting high purity iron (99.99 mass% purity)
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Medium carbon steel
Melt blister and Degas sample
Meseum specimen. From an old iron anchor
MgO-C brick
Micro-alloyed steel
Microalloyed steel
Mild steel, Armco steel
Mirrax steel
MMA weld metals
Mn-Si killed low carbon steel
Mn-Si killed low carbon steel
Mn-Si killed low carbon steel
Mn-silicate specimen
Mn-silicate specimen
Mn0silicate specimen
MnS in Fe-Mn-S alloy
MnS-MnO specimen
Molten iron
Molten iron
Mould steel
Museum specimen
Nb steel
Nb steel
Ni-based alloy 825
Ni-Cr-Mo steel, after forging and annealing
Ni-Cr-Mo steel, Ti killed, as cast
Nimax steel
Nimax steel
Nimax steel
Nimax steel
Nimax steel
Nimax steel
Nimax steel
Nimonic 80A nickel alloy
Nitriding steel
Nodular cast iron, inoculated with FeSi
Non-oriented electrical steel sheet
Non-oriented electrical steel
OH236NI steel
Open-hearth slag
Open-hearth slag
Open-hearth slag
ORVAR 2M and DIEVAR steels
ORVAR 2M and DIEVAR steels
ORVAR 2M and DIEVAR steels
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
Orvar 2M - a low alloyed high temperature tool steel
Orvar 2M - a low alloyed high temperature tool steel
Orvar 2M - a low alloyed high temperature tool steel
Orvar 2M steel, ingots of 5.8 tons
Orvar 2M steel, ingots of 5.8 tons
Orvar 2M steel, ingots of 5.8 tons
ORVAR 2M steel, liquid steel sample
ORVAR 2M steel, liquid steel sample
ORVAR 2M steel, liquid steel sample
ORVAR 2M steel, liquid steel sample
ORVAR 2M steel, liquid steel sample
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M steel
ORVAR 2M, STAVAX ESR, DIEVAR, SVERKER 21 steels
ORVAR SUPREME steel
Orvar2M steel
Ovako steel
Ovako steel
Ovako steel
Oxide rod
Oxide rod
Oxide samples
Oxides
P122 steel
P122 steel
P122 steel
P122 steel
P122 steel
P122 steel
P122 steel
P20 steel
P20 tool steel
P20 tool steel
Pb-free machinable ferritic stainless steel
Pearlitic gay cast iron
Pearlitic gay cast iron
Pearlitic gay cast iron
Pearlitic gay cast iron
Pearlitic grey cast iron
Pearlitic grey cast iron
Pig iron
Pig iron
Pig iron
Pipe line steels
Pipeline steel, 13XΦA steel
Pipeline steel, API-5L Grade X52
Pipeline steel
Pipeline steel
Pipeline steel
Pipeline steel
Pipeline steel
Plain carbon steel
Plain carbon steel
PM cold work tool steel
PM steel, JIS-SUJ2
PM steel
PM steel
PM superalloy U720
Polished steel moulds
Powder compacts: SS 2317, oxidized and HIPped
Powder compacts: SS 2317, unoxidized and oxidized
Puddled iron
Puddled iron
Pure Al2O3
Pure Al2O3
Pure iron
Pure iron
Pure iron
Pure iron
Pure iron
Pure iron
Pure iron
Pure TiO2
Pure TiO2
Pure TiO
Pure TiO
Q550 and Q690 steels
Rail steel
Railway steel
Reaction zone steel-slag-burnt dolomite
Reduced electric steel, Ca-deoxidized
Reduced electric steel, Ca-deoxidized
Reduced electric steel, CaSi-deoxidized
Refractories
Refractories
Refractories
Refractories
Refractories
Refractories
Refractory material
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-slag
Refractory-steel
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Refractory
Rhodonite sample
RIII-I1-S3-SLD: ESR ingots CaSi deoxidized
RIII-I1-S3-SLD: ESR ingots CaSi deoxidized
Rimmed carbon steel, rolled to 65 mm, longitudinal section
Rimmed carbon steel. Hot rolled billet
Rimming deep-drawing steel. From cold rolled sheet
RM NA-4 steel
Rolled carbon steel
Rolled industrial steel
Rolled steel sheet
Rolled steel
Rolled steel
Rolled steel
Rolled steel
Rolled steel
Rolled Steelmaker 4 continous-cast steel
Roller bearing steel, not deoxidized with Ca
Rotor steel
S235 steel
S235JR steel
S275 JRC steel
S355N steel
S390 PM high speed steel
S390 PM high speed steel
S390 PM high speed steel
S45C steel
S45C steel
SAE 1005 steel, low carbon steel, Si killed, LD convertor
SAE 1010 and 1005 steels
SAE 1010 steel, low carbon steel, Al killed, LD convertor
SAE 1015, aluminium killed steel
SAE 1015 steel
SAE 1050 steel
SAE 1141 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4140 steel
SAE 4145 steel
SAE 52100 steel
SAE 52100 steel
SAE 52100 steel
SAE 52100 steel
SAE 52100 steel
SAE 52100 steel
SAE 9254 spring steel
Sample from the border zone between ladle slag and ladle refractories
Sample polishing - Comet tails
Sample preparation - Inclusions pulled out
Sample
SCM415 steel
SEN port
SEN sample
SFVQ1A steel
Si steel
Si-killed electric steel, vacuum treated
Si-killed steel
Si-killed steel
Si-steel
Silicate melt
Silicon alloyed dynamo strip steel
Silicon killed electro-steel, vacuum treated. From railway rail
Silicon steel
Silicon-killed basic electric vacuum degassed in the ladle and rolled to rails
Silicon-killed carbon steel, which has been vacuum treated. Defect in the web of a railway rail
Silicon-killed SAE 1005 steel
SiMn alloy
Slag from the EAF furance. Capacity of both EAF and ladle furnace (LF) is 60 tons of steel
Slag inclusions in rolled steel
Slag particle in rolled steel
Slag, chemical processing
Slag, chemical processing
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
Slag
SOC-9 and SOC-14 steels
Soft magnetic steel
Soft magnetic steel
Special steel
Special steel
Special steel
Special steel
Special steel
Special steel
Specimen fused together from MnS+FeO(+SiO2) in a Fe crucible
Specimen, fused together from equal parts MnS and MnSiO3
Speedsteel ASP 23
Speedsteel ASP 23
Spring steel (UNS G92600)
Spring steel
Spring steel
Spring steels (S40C, SMn443, SCM435, SUP12, SWOSC-V)
SS 2343 steel
SS 2562 austenitic stainless steel
SS 2562 austenitic stainless steel
SS400 steel
St52-3N steel
St52-3N steel
Stainless heat resistant steel produced in a basic electric ste
Stainless steel casting
Stainless steel casting
Stainless steel casting
Stainless steel for surgical implants
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steel
Stainless steels
Staonless steel
Steel 1: 4LR60 stainless austenitic steel, steel 2: Sandwik SANMAC 2205
Steel 1: 4LR60 stainless austenitic steel, steel 2: Sandwik SANMAC 2205
Steel 1: 4LR60 stainless austenitic steel, steel 2: Sandwik SANMAC 2205
Steel 1: 4LR60 stainless austenitic steel, steel 2: Sandwik SANMAC 2205
Steel C belongs to grade X52, steels A and D to grade X65, and steel B to grade X70
Steel for cold sheets
Steel ingot, bottom cast. From a hot rolled sheet
Steel ingot
Steel pipe for water
Steel runner
Steel sample 2
Steel sample
Steel sheet
Steel sheet
Steel slab
Steel slab
Steel slab
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel was used for the experiments
Steel weld
Steel with a low C content, rolled
Steel with and without Ca
Steel with low and high sulfur
Steel with Sn
Steel with Sn
Steel with Sn
Steel with Sn
Steel with Sn
Steel with the rare earth elements
Steelmaking slag
Steels (20NiCrMo2-2, 20NiCrMo7, 16NiCr6-4 F)
Structural 20-KCX steel
Structural steel
Structural steel
Structural steel
Structural steel
Strømhard steel. This is a modified Hadfield steel
Submerged entry nozzle (SEN)
SUJ2 steel
SUJ2 steel
SUJ2 steel
Sulphur-based master alloy
Super austenitic stainless steels
SUS304 stainless steel
SUS410J1 and SUS440B steels. Martensitic stainless steel
SUS410J1 and SUS440B steels. Martensitic stainless steel
SUS410J1 and SUS440B steels. Martensitic stainless steel
SUS430 stainless steel
Synthetic MnS powder
Synthetic slag, prepared by melting a calcia-alumina-silica mixture
Synthetic slag, prepared from calcia-alumina mixture
Synthetic slag
Synthetic slag
Synthetic slag
Synthetic slag
Synthetic specimen of FeO+MnO
Synthetic sulfide
T-22 and T-91 steels
Tempered steel
The blind feeder (about 2 t in weight) of a 60 t sand mold casting was used for the observation of sulfide in a large steel casting
The blind feeder (about 2 t in weight) of a 60 t sand mold casting was used for the observation of sulfide in a large steel casting
The sample was taken from the slag lining of the ladle, remelted in the electron beam furnace
The steel sample used in this experiment is prepared in an induction heating furnace with electrolytic iron
The steel sheets are manufactured from low-carbon Al-killed steel slabs through the processes of hot rolling
Thermal spray coating
Ti steel
Ti-added steel
Ti-alloyed Al-killed steel grade
Ti-alloyed ultra-low carbon steel
Ti-bearing Al-killed steel
Ti-killed C-Mn steel
Ti-killed C–Mn steel
Ti-stabilized austenitic stainless steel
Tire cord steel
Tool steel
Tool steel
TOOLOX44 steel
TRIP steel
TRIP steel
TRIP steel
TRIP steel
TWIP steel
Type 203 stainless steel
Type 203 stainless steel
Type 301 and 316 stainless steels
Type 301 and 316 stainless steels
Type 301 and 316 stainless steels
Type 301 stainless steel
Type 303 stainless steel
Type 303 stainless steel
Type 303, 304 and 321 stainless steels
Type 303Se stainless steel
Type 304 stainless steel
Type 304 stainless steel
Type 304 stainless steel
Type 304 stainless steel
Type 316L stainless steel
Type 321 stainless steel
Type 403 martensitic stainless steel
Type 416 and 5F (modified 416) stainless steels
Type 416 stainless steel
Type 444 stainless steel
ULC steel
ULC steel
ULC teel
ULC, LC steels
Ultra high strength low carbon steel
Ultra high strength steel
Ultra low carbon steel (ULC), IF steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra low carbon steel
Ultra-high-strength steel (UHSLA)
Ultra-low carbon (ULC) steel
Ultra-thin cast strip (UCS) steel
Ultrahigh strength steel
Unalloyed steels
Unknown steel
Unknown steel
V-N, V-Ti-N steels
Water atomized metal powder, Hoganas A 4000
Water atomized metal powder, Hoganas A 4000
Water atomized metal powder, Hoganas AHC 10.29
Water atomized metal powder, Hoganas ASC 100.29
Water atomized metal powder, Hoganas Astaloy A
Water atomized metal powder, Hoganas Astaloy A
Water atomized metal powder, Hoganas Astaloy A
Water atomized metal powder, Hoganas Astaloy C
Water atomized metal powder, Hoganas Astaloy D
Water atomized metal powder, Hoganas Astaloy D
Water atomized metal powder
Water quenched BF slag
Weathering steel ingot
Weld material
Weld material
Weld material
Weld material
Weld material
Weld material
Weld metal deposit
Weld metal deposit
Weld metal deposit
Weld metal for high strength steel
Weld metal. Galaxite and rutile were added to the coatings of electrodes in order to prepare weld metals
Weld metal
Weld steel for arctic
Weld steel
Weld steel
Welded steel joints
Welding electrode
Wheel steel
Wheel steel
Wheel steel
Wheel steel
Wheel steel
Wheel steel
Wheel steel
Wheel steel
White cast iron
Sword blade from Chiusi, steel
Sword blade from Vetulonia, steel
Wrought iron
Wrought iron
Wrought steel
Wrought steel
Wrought steel
X-65 carbon steel
X-65 pipeline steel
X-65 pipeline steel
X-65 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X-70 pipeline steel
X100CrMoV5 steel
X12Cr13 steel
X12Cr13 steel
X12Cr13 steel
X12CrS13 steel
X12CrS13 steel
X19CrMoVNbN11-1 steel
X19CrMoVNbN11-1 steel
X19CrMoVNbN11-1 steel
X19NiCrMo4 steel
X19NiCrMo4 steel
X1CrNiMoCuN20-18-7 steel
X20Cr13 stainless steel (1.4021)
X20Cr13 steel
X20Cr13 steel
X20Cr13 steel
X20Cr13 steel
X20Cr13 steel
X20CrMoV11-1 steel
X20CrMoV11-1 steel
X20CrMoV11-1 steel
X20CrMoV11-1 steel
X20CrMoV12-1 creep-resistant steel
X22CrMoV12-1 steel
X2CrNiMo18-14-3 stainless steel
X30Cr13 steel
X38CrMoV5-1 steel
X39CrMo17-1 steel
X40CrMoV51 steel
X40CrMoV51 steel
X45NiCrMo4 steel
X46Cr13 steel
X46Cr13 steel
X46Cr13 steel
X50CrMoV15 steel
X52, 13Cr6Ni2.5Mo steels
X5CrNiCuNb16-4 steel
X65 grade line pipe steels
X65 linepipe steel
X6CrNiMoTi17-12-2 steel
X70 linepipe steel
ZRM 192-1 certified reference material

Copyright © 2024 by Steel Data. All Rights Reserved.