Dolomite



Chemical formula: CaMg(CO3)2
Melting point: No data
Density: 2.84–2.86 g/cm3
Hardness (Moh's): 3.5-4
Luminescence: Non-fluorescent
Crystal system: Rhombohedral
Cell dimensions: a=4.811 A, b=4.811 A, c=16.02 A
PDF number: 00-011-0078
ICSD number: 031336
Note: No data