Hauerite



Chemical formula: MnS2
Melting point: No data
Density: 3.463 g/cm3
Microhardnes: No data
Hardness (Moh's): 4
Luminescence: No data
Crystal system: Cubic
Cell dimensions: a=6.097 A
PDF number: 00-002-0616
ICSD number: 036547