Marcasite



Chemical formula: FeS2
Melting point: No data
Density: 4.89 g/cm3
Microhardnes: No data
Hardness (Moh's): 6.2
Luminescence: Non-fluorescent
Crystal system: Orthorhombic
Cell dimensions: a=4.445 A, b=5.425 A, c=3.388 A
PDF number: 00-003-0799
ICSD number: 026756
Note: No data