Merwinite



Chemical formula: 3CaO x MgO x 2SiO2
Melting point: No data
Density: 3.15 g/cm3
Microhardnes: No data
Hardness (Moh's): 6
Luminescence: Non-fluorescent
Crystal system: Monoclinic
Cell dimensions: a=13.254 A, b=5.293 A, c=9.328 A
PDF number: 00-025-0161
ICSD number: 026002
Note: No data