Mg-ferrite



Chemical formula: MgO x Fe2O3
Melting point: No data
Density: 4.6 g/cm3
Microhardnes: No data
Hardness (Moh's): 6
Luminescence: Nodata
Crystal system: Cubic
Cell dimensions: a=8.383 A
PDF number: 00-001-1114
ICSD number: Data not found
Note: No data