Protoenstatite



Chemical formula: MgO x SiO2
Melting point: No data
Density: No data
Microhardnes: No data
Hardness (Moh's): No data
Luminescence: No data
Crystal system: Orthorhombic
Cell dimensions: a=9.25 A, b=8.74 A, c=5.32 A
PDF number: 00-003-0523
ICSD number: Data not found
Note: No data