Demo Records (50 Non-Metallic Inclusions)

Al oxide, Ti-Al oxide, TiN, Al-Mg oxide inclusions in low carbon steel
Al2O3 cluster inside of bubble in ultra low carbon steel
A typical calcium aluminate inclusion surrounded with a CaS ring observed in a high carbon Si killed low aluminum steel
Big slag inclusion in 42CrMo4 steel
Calcium aluminate in A529 steel
Calcium sulfide and aluminium oxide inclusions in 51CrV4 spring steel
Calcium-aluminate inclusion in fracture surface of 51CrV4 steel
Complex inclusions in C-Mn-B steel
Cristobalite in manganese oxide-chromia-silica
Cristobalite in manganese-silicate
Element mapping of a complex oxy-sulfide inclusion in steel
Examples of faceted Al2O3 inclusion in steel
Fractures of wheel steel with nonmetallic inclusions
Furnace slag with the particles of chromite
Highly deformable MnS inclusion and non-deformable calcium aliminate inclusion
Globular oxide inclusion in high carbon wire rod steel
Hydrogenous cracks near sulfides in wheel steel
Inclusion in the liquid high carbon steel after ladle treatment
Iron oxide in 36MnVS4 steel
Manganese sulfide in A529 steel
Microbreaks near nonmetallic inclusions after plastic deformation of wheel steel
MnO x SiO2 x Al2O3 inclusion in high carbon wire rod steel
MnS in iron
Mullite and spessartite in glassy matrix of manganese oxide-alumina-silica
Multiphase inclusions in C-Mn-B steel
Multiphase inclusions in a Ce containing steel
Non-metallic inclusions in F82H-IEA steel
Oxide inclusions in low carbon Si-killed steel
Oxide scale in X45NiCrMo4 steel
Oxide stringers in high carbon wire rod steel
Plate-like overgrowth onto existing particles in steels
Round duplex inclusion in steel
Rust scale on the steel surface of 1.2343 steel
Silica based inclusions in steel
Slag inclusion in 1.3343 steel
Slag inclusion in AISI H13 steel
Slag samples from the 60 tons EAF furnace
Spinel inclusions in type 304 stainless steel
The copper sulfide coexisted with silicon oxide in sample H13L
The copper sulfide coexisted with silicon oxide in sample H13L
The iron sulfide coexisted with silicon oxide with different morphologies in sample H13L
The iron sulfide coexisted with silicon oxide with different morphologies in sample H13L
The iron sulfide coexisted with silicon oxide with different morphologies in sample H13L
Thermal stresses near nonmetallic inclusions and wear parts near nonmetallic inclusion in wheel steel
Titanium carbonitride in Nimonic 80A alloy
Transmission electron micrograph and diffraction patterns of cubic TiO particle from melt containing 1.38 mass% Ti
Type 7 inclusion in steel with 0.38C-5.29Cr-0.94V
(Mn,Fe)S inclusions in 1.0715 steel
(Ti, Ca)-oxide in 409L stainless steel
V(C, N) inclusion in Low C–Mn–V steel

Copyright © 2024 by Steel Data. All Rights Reserved.