Struers electrolyte E5-II - Brass, bronze, carbon steel, cast iron

Material Name: Brass, bronze, carbon steel, cast iron
Recipe No.: 10085
Primary Chemical Element in Material: Cu, Fe
Sample Type: Bulk
Uses: Polishing
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Electrolytic polishing
Etchant (Electrolyte) Composition: 80-95% cobalt nitrate, 5-20% ferric nitrate.
Procedure (Condition): No data
Note: Brass, bronze, carbon steel, cast iron, materials with strong varying structural elements.
Reference: Website Struers, 2011.