Alphabetical Index
Browse by Elements
Keyword Search
ASTM Electrolytes
Macro Etchants
Micro Etchants
Named Etchants
New Etchants
Al and Al Alloys
Cu and Cu Alloys
Fe and Fe Alloys
Ni and Ni Alloys
Carbide Etchants
Fluoride Etchants
Nitride Etchants
Other Etchants
Oxide Etchants
Phosphide Etchants
Single Crystal Etchants
Thin Film Etchants
Wafer Etchants
Help
Home
Named Etchants
1 + 2 Tucker’s etchant - All except high Si castings - Chemical etching - General macrostructure
100 etchant - Ge (100) wafers - Chemical etching
111 etchant - Ge (111) and Si (111) wafers - Chemical polishing/etching
3:2:1 etchant - Nickel superalloys
50% HCl electrolytic - Nickel superalloys
6.6.1 etchant - For etch pits on InP, InPAs, GeInPAs
92.5.3 etchant - Steel for high temperatures
A etchant
A/B etchant - Al2O3 clear fused sapphire blanks and (0001) single crystal oriented blanks
A/B etchant - GaAs (111) wafers with zinc diffusion - Chemical etching
A/B etchant - GaSb (100) wafers Te-doped - Chemical etching
A/B etchant - InAs (111), (110) and (100) wafers - Chemical etching
A/B etchant - InP (TTT)B wafers - Chemical etching
AB etchant (RCA) - Glass-thin film deposition and growth - Chemical cleaning
AB etchant, diluted - Alminium gallium arsenide (Al(x) Ga(1-x) As) - Dislocation etching
AB etchant, modified - Gallium arsenide
AB etchant, modified - Indium phosphide (InP) - Chemical etching
AG-21's etchant for superalloy - Chemical etching
AHA etchant - For GaAs
AI-7 etchant - For macro etching ferrous cast alloys - Chemical etching
ASTM dislocation etchant - Dislocation etching
ASTM etchant No. 1 - For Al base alloys
ASTM etchant No. 10 - Beryllium - Chemical etching
ASTM etchant No. 10 - For Be
ASTM etchant No. 10 - Ni superalloys - Chemical etching
ASTM etchant No. 100 - Fe + 12-20 Cr + 4-10 Ni + <7% steels - Chemical etching
ASTM etchant No. 100 - Ferric chloride - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No. 100 - Non stainless maraging steels - Chemical etching
ASTM etchant No. 101 - Chrome regia - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No. 101 - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Chemical etching
ASTM etchant No. 102 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No. 102 - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Electrolytic etching
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 103 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Fe + 16-25 Cr + 3-6 Ni + 5-1C steels - Chemical etching
ASTM etchant No. 104 - Frank's etchant - Fe + 16-25 Cr + 3-6 Ni + 5-1C
ASTM etchant No. 105 -2-5-3 etchant - Steel for high temperatures
ASTM etchant No. 105 - High temperature steels - Chemical etching
ASTM etchant No. 105 - Ni superalloys - Chemical etching
ASTM etchant No. 106 - High temperature steels - Chemical etching
ASTM etchant No. 106 - Steel for high temperatures
ASTM etchant No. 107 - E-etchant (EI-IR etchant) - Steel for high temperatures
ASTM etchant No. 107 - High temperature steels - Electrolytic etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni superalloys - Electrolytic etching
ASTM etchant No. 107 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 108 - High temperature steels - Electrolytic etching
ASTM etchant No. 108 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 108 - Steel for high temperatures
ASTM etchant No. 109 - HCl-HNO3-CuCl2 x H2O - Non stainless maraging steels
ASTM etchant No. 109 - Non stainless maraging steels - Chemical etching
ASTM etchant No. 11 - Beryllium - Chemical etching
ASTM etchant No. 11 - For Be allloys
ASTM etchant No. 11 - Ti alloys - Chemical etching
ASTM etchant No. 110 - Tool steels
ASTM etchant No. 110 - Tool steels - Chemical etching
ASTM etchant No. 111 - Fe superalloys - Electrolytic etching
ASTM etchant No. 111 - Iron
ASTM etchant No. 111 - Ni superalloys - Chemical etching
ASTM etchant No. 112 - Pb + Ca alloys - Chemical etching
ASTM etchant No. 112 - Pb+Ca alloys
ASTM etchant No. 113 - Pb + Ca alloys - Chemical etching
ASTM etchant No. 113 - Acetic/nitric - Pb + <2 Sb alloys
ASTM etchant No. 113 - Pb + >2 Sb alloys - Chemical etching
ASTM etchant No. 114 - Acetic/nitric - Pb + <2 Sb alloys
ASTM etchant No. 114 - Pb + >2 Sb alloys - Chemical etching
ASTM etchant No. 114Pb + <2 Sb alloys - Chemical etching
ASTM etchant No. 115 - Pb + <2 Sb alloys
ASTM etchant No. 115 - Pb + <2 Sb alloys - Chemical etching
ASTM etchant No. 116 - Pb alloys
ASTM etchant No. 116 - Pb alloys - Chemical etching
ASTM etchant No. 116 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 117 - Sn-Fe
ASTM etchant No. 117a - Sn-Fe alloys - Chemical etching
ASTM etchant No. 117b - Pb alloys - Chemical etching
ASTM etchant No. 118 - Glycol - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 118 - Magnesium - Chemical etching
ASTM etchant No. 118 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 118 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 118 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 119 - Acetic glycol - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 119 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 119 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 119 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 119 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 119 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 119 - Pure magnesium - Chemical etching
ASTM etchant No. 12 - Aqua Regia - For chromium base alloys
ASTM etchant No. 12 - Chromium - Chemical etching
ASTM etchant No. 12 - Ni superalloys - Chemical etching
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 120 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 120 - Mg-Rare Earth-Zr alloys - Chemical etching
ASTM etchant No. 120 - Mg-Zn-Th-Zr alloys - Chemical etching
ASTM etchant No. 120 - Pure magnesium - Chemical etching
ASTM etchant No. 121 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 121 - Mg-Rare Earth-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Zn-Th-Zr alloys - Chemical etching
ASTM etchant No. 121 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 121 - Phospho picral - Mg-Al, Mg-Al-Zn (Al + Zn >5%
ASTM etchant No. 121 - Pure magnesium - Chemical etching
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 122 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 122 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 122 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 122 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 122 - Pure magnesium - Chemical etching
ASTM etchant No. 123 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 123 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Electrolytic etching
ASTM etchant No. 123 - Pure magnesium - Electrolytic etching
ASTM etchant No. 124 - Acetic-picral - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 124 - Mg-Mn alloys - Chemical etching
ASTM etchant No. 124 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 124 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 125 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 126 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 127 - Acetic-picral - Mg-Al, Mg-Al-Zn (Al + Zn <5%
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn <5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn 5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Al, Mg-Al-Zn (Al + Zn >5% alloys - Chemical etching
ASTM etchant No. 127 - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 127 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 128 - Mg-Zn-Zr
ASTM etchant No. 128 - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 129 - Molybdenum
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Molybdenum - Chemical etching
ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 129 - Niobium - Chemical etching
ASTM etchant No. 13 - Oxalic acid - For Cr base alloys
ASTM etchant No. 130 - Molybdenum
ASTM etchant No. 130 - Molybdenum - Chemical etching
ASTM etchant No. 130 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Molybdenum
ASTM etchant No. 131 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Molybdenum - Electrolytic etching
ASTM etchant No. 131 - Tungsten - Electrolytic etching
ASTM etchant No. 131 - Tungsten - Electrolytic etching
ASTM etchant No. 132 - Molybdenum
ASTM etchant No. 132a - As cast molybdenum - Chemical etching
ASTM etchant No. 132a - As cast tungsten - Chemical etching
ASTM etchant No. 133 - Ni superalloys - Chemical etching
ASTM etchant No. 133 - Ni-Ti
ASTM etchant No. 133 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 133 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 134 - Ni-Cr
ASTM etchant No. 134 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 134 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No. 134 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 135 - Pure Ni and high Ni alloys
ASTM etchant No. 135 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 136 - Pure Ni and high Ni alloys
ASTM etchant No. 136 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 137 - Pure Ni and high Ni alloys
ASTM etchant No. 137 - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 138 - Carapella's etchant - Ni-Ag
ASTM etchant No. 138 - Ni superalloys - Chemical etching
ASTM etchant No. 138 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 139 - Ni-Ag
ASTM etchant No. 139 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 13a - Fe + 15-30 Cr + 6-40 Ni + <5% - Electrolytic etching
ASTM etchant No. 13a - Ni superalloys - Electrolytic etching
ASTM etchant No. 13a - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 13b - Fe + 15-30 Cr + 6-40 Ni + <5% steels - Electrolytic etching
ASTM etchant No. 13b - Rhenium - Electrolytic etching
ASTM etchant No. 13c - Chromium - Electrolytic etching
ASTM etchant No. 14 - For Co
ASTM etchant No. 14 - Tool steels - Chemical etching
ASTM etchant No. 140 - Ni-Al
ASTM etchant No. 140 - Ni-Al alloys - Chemical etching
ASTM etchant No. 140 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 141 - Contrast etchant - Ni-Al
ASTM etchant No. 141 - Ni-Al alloys - Chemical etching
ASTM etchant No. 141 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 142 - Ni-Al
ASTM etchant No. 142 - Ni-Al alloys - Electrolytic etching
ASTM etchant No. 143 - Ni-Al
ASTM etchant No. 143 - Ni-Al alloys - Chemical etching
ASTM etchant No. 143 - Ni-Mo alloys - Chemical etching
ASTM etchant No. 143 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 144 - Ni-Cr
ASTM etchant No. 144 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 145 - Ni-Cr
ASTM etchant No. 145 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No. 146 - Ni-Cr
ASTM etchant No. 146 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 147 - Ni-Cr
ASTM etchant No. 147 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 148 - Ni-Fe
ASTM etchant No. 148 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 149 - Ni-Fe
ASTM etchant No. 149 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 15 - For Co
ASTM etchant No. 150 - Ni-Fe
ASTM etchant No. 150 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 151 - Ni-Ti
ASTM etchant No. 151 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 152 - Ni-Zn
ASTM etchant No. 152 - Ni-Zn alloys - Chemical etching
ASTM etchant No. 153 - Ni superalloys
ASTM etchant No. 153 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 154 - Ni superalloys - Chemical etching
ASTM etchant No. 155 - Beraha's E etchant - Ni superalloys
ASTM etchant No. 155 - Ni superalloys - Chemical etching
ASTM etchant No. 156 - Ni superalloys
ASTM etchant No. 156 - Ni superalloys - Electrolytic etching
ASTM etchant No. 157 - Hastelloy-W - Chemical etching
ASTM etchant No. 157 - Ni Hastelloy-W
ASTM etchant No. 158 - Niobium
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 158 - Niobium - Chemical etching
ASTM etchant No. 158 - Ta alloys - Chemical etching
ASTM etchant No. 158 - Tantalum - Chemical etching
ASTM etchant No. 158 - Ti alloys - Chemical etching
ASTM etchant No. 159 - Niobium
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 159 - Niobium - Chemical etching
ASTM etchant No. 159 - Ta alloys - Chemical etching
ASTM etchant No. 159 - Tantalum - Chemical etching
ASTM etchant No. 16 - Co high temperature alloys - Electrolytic etching
ASTM etchant No. 16 - Hydrochloric acid - For Co, high temperature alloys
ASTM etchant No. 16 - Fe as residual metal in vacuum systems - Chemical cleaning
ASTM etchant No. 160 - Niobium
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 160 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 161 - Niobium - Chemical etching
ASTM etchant No. 161 - Ta alloys - Chemical etching
ASTM etchant No. 161 - TaN thin films - Chemical etching
ASTM etchant No. 161 - Tantalum - Chemical etching
ASTM etchant No. 162 - Niobium
ASTM etchant No. 162 - Niobium - Chemical etching
ASTM etchant No. 162B - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 163 - Niobium - Chemical etching
ASTM etchant No. 163 - Ta alloys - Chemical etching
ASTM etchant No. 163 - Tantalum - Chemical etching
ASTM etchant No. 164 - Niobium
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 164 - Niobium - Chemical etching
ASTM etchant No. 164 - Ta alloys - Chemical etching
ASTM etchant No. 164 - Tantalum - Chemical etching
ASTM etchant No. 164 - Tantalum - Chemical etching
ASTM etchant No. 165 - Vanadium
ASTM etchant No. 165a - Osmium - Electrolytic etching
ASTM etchant No. 165a - Osmium - Electrolytic etching
ASTM etchant No. 165a - Pd alloys - Electrolytic etching
ASTM etchant No. 165a - Pure palladium - Electrolytic etching
ASTM etchant No. 165b - Pure vanadium - Electrolytic etching
ASTM etchant No. 166 - Pd alloys
ASTM etchant No. 166 - Pd alloys - Chemical etching
ASTM etchant No. 166 - Pure palladium - Chemical etching
ASTM etchant No. 167 - Pt alloys
ASTM etchant No. 167 - Pt alloys - Chemical etching
ASTM etchant No. 167 - Pure platinum - Chemical etching
ASTM etchant No. 168 - Pt-10% Rh
ASTM etchant No. 168 - Pt-10% Rh alloy - Chemical etching
ASTM etchant No. 169 - Plutonium
ASTM etchant No. 169 - Plutonium - Electrolytic etching
ASTM etchant No. 17 - For Co
ASTM etchant No. 170 - Rhenium
ASTM etchant No. 170a - Rhenium - Chemical etching
ASTM etchant No. 170a - Ti alloys - Chemical etching
ASTM etchant No. 170a - U Beryllides - Chemical etching
ASTM etchant No. 170b - Pure vanadium - Chemical etching
ASTM etchant No. 171 - Hydrochloric acid - Rhodium
ASTM etchant No. 171 - Rhodium - Electrolytic etching
ASTM etchant No. 172 - Pure Ag
ASTM etchant No. 172 - Pure silver - Chemical etching
ASTM etchant No. 173 - Ag solders
ASTM etchant No. 173 - Ag solders - Chemical etching
ASTM etchant No. 173 - Ag-Pd alloys - Chemical etching
ASTM etchant No. 173 - Pure Ag - Chemical etching
ASTM etchant No. 174 - Ag alloys
ASTM etchant No. 174 - Ag alloys - Chemical etching
ASTM etchant No. 175 - Ag alloys
ASTM etchant No. 175 - Ag alloys - Chemical etching
ASTM etchant No. 176 - Ag solders
ASTM etchant No. 176 - Ag solders - Chemical etching
ASTM etchant No. 177 - Pure tantalum - Chemical etching
ASTM etchant No. 177 - Tantalum
ASTM etchant No. 177 - Tantalum - Chemical etching
ASTM etchant No. 177 - Zn-Co alloys - Chemical etching
ASTM etchant No. 178 - Ta alloys
ASTM etchant No. 178 - Ta alloys - Chemical etching
ASTM etchant No. 178 - Tantalum - Chemical etching
ASTM etchant No. 178 - Ti alloys - Chemical etching
ASTM etchant No. 179 - Ta alloys
ASTM etchant No. 179 - Ta alloys - Chemical etching
ASTM etchant No. 18 - Chromic acid - For Co alloys, high temperature alloys
ASTM etchant No. 18 - Hard-Facing and tool metals - Electrolytic etching
ASTM etchant No. 18 - High temperature alloys - Electrolytic etching
ASTM etchant No. 18 - Ni superalloys - Electrolytic etching
ASTM etchant No. 18 - Pure titanium - Electrolytic etching
ASTM etchant No. 180 - Pure tin - Chemical etching
ASTM etchant No. 180 - Tin
ASTM etchant No. 181 - Pure tin
ASTM etchant No. 181 - Pure tin - Chemical etching
ASTM etchant No. 182 - Sn-Pb
ASTM etchant No. 182 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 183 - Sn coatings (on steel)
ASTM etchant No. 183 - Sn coatings (on steel) - Chemical etching
ASTM etchant No. 183 - Sn-Pb alloys - Chemical etching
ASTM etchant No. 184 - Babbitts
ASTM etchant No. 184 - Sn babbitts - Chemical etching
ASTM etchant No. 185
ASTM etchant No. 186 - Pure titanium
ASTM etchant No. 186 - Pure titanium - Chemical etching
ASTM etchant No. 186 - Ti alloys - Chemical etching
ASTM etchant No. 187 - Kroll's etchant - Ti alloys
ASTM etchant No. 187 - Ti alloys - Chemical etching
ASTM etchant No. 188 - Mg-Al, Mg-Al-Zn (Al + Zn <5 alloys - Chemical etching
ASTM etchant No. 188 - Pure titanium
ASTM etchant No. 188 - Pure titanium - Chemical etching
ASTM etchant No. 188 - Ti alloys - Chemical etching
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn
ASTM etchant No. 189 - Ti-5 Al-2.5 Sn alloys - Chemical etching
ASTM etchant No. 19 - Co Hard-Facing and tool metals - Chemical etching
ASTM etchant No. 19 - Co high temperature alloys - Chemical etching
ASTM etchant No. 19 - Groesbeck's etchant - For Co alloys, high temperature alloys
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn
ASTM etchant No. 190 - Ti-6 Al-6V-2 Sn alloys - Chemical etching
ASTM etchant No. 191 - Ti-Al-Zr
ASTM etchant No. 191 - Ti-Al-Zr alloys - Chemical etching
ASTM etchant No. 192 - Kroll's etchant - Ti alloys
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti alloys - Chemical etching
ASTM etchant No. 192 - Ti-13V-11Cr3 Al (aged) alloys - Chemical etching
ASTM etchant No. 192 - Ti-8Mn alloys - Chemical etching
ASTM etchant No. 193 - Ti-Si
ASTM etchant No. 193 - Ti-Si alloys - Chemical etching
ASTM etchant No. 194 - Ti alloys
ASTM etchant No. 194 - Ti alloys - Chemical etching
ASTM etchant No. 195 - Pure uranium
ASTM etchant No. 195 - Pure uranium - Electrolytic etching
ASTM etchant No. 195 - U alloys - Electrolytic etching
ASTM etchant No. 196 - Pure uranium
ASTM etchant No. 196 - Pure uranium - Chemical etching
ASTM etchant No. 196 - U alloys - Chemical etching
ASTM etchant No. 197 - Pure vanadium
ASTM etchant No. 197 - Pure vanadium - Electrolytic etching
ASTM etchant No. 198 - Pure vanadium
ASTM etchant No. 198 - Pure vanadium - Chemical etching
ASTM etchant No. 198 - V alloys - Chemical etching
ASTM etchant No. 199 - V alloys
ASTM etchant No. 199 - V alloys - Chemical etching
ASTM etchant No. 19b - Ni superalloys - Chemical etching
ASTM etchant No. 1a - Aluminum 1000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 2000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 3000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 4000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 5000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 6000 series - Chemical etching
ASTM etchant No. 1a - Aluminum 7000 series - Chemical etching
ASTM etchant No. 1a - Pure aluminum - Chemical etching
ASTM etchant No. 1b - Pure aluminum - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 1c - Ti alloys - Chemical etching
ASTM etchant No. 1d - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 1d - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 2 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 2 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 2 - NaOH (Hatch's etchant) - Al alloys
ASTM etchant No. 2 - Pure aluminum - Chemical etching
ASTM etchant No. 20 - Co Hard-Facing and tool metals - Chemical etching
ASTM etchant No. 20 - Co high temperature alloys - Chemical etching
ASTM etchant No. 20 - For Co alloys, high temperature alloys
ASTM etchant No. 200 - Potassium etchant - Pure zinc
ASTM etchant No. 200 - Pure zinc - Chemical etching
ASTM etchant No. 201 - Zn-Cu
ASTM etchant No. 201 - Zn-Cu alloys - Chemical etching
ASTM etchant No. 202 - Zinc die castings
ASTM etchant No. 202 - Zn Die castings - Chemical etching
ASTM etchant No. 203 - Zn-Cu
ASTM etchant No. 203 - Zn-Cu alloys - Electrolytic etching
ASTM etchant No. 204 - Zirconium
ASTM etchant No. 204 - Zirconium - Chemical etching
ASTM etchant No. 205 - Zirconium
ASTM etchant No. 205 - Zirconium - Chemical etching
ASTM etchant No. 206 - Zirconium
ASTM etchant No. 206 - Zirconium - Chemical etching
ASTM etchant No. 207 - U alloys
ASTM etchant No. 207 - U alloys - Chemical etching
ASTM etchant No. 208
ASTM etchant No. 209 - Molybdenum - Chemical etching
ASTM etchant No. 209 - Tungsten - Chemical etching
ASTM etchant No. 209 - W-Th
ASTM etchant No. 209 - W-Th alloys - Chemical etching
ASTM etchant No. 21 - Co high temperature alloys - Chemical etching
ASTM etchant No. 21 - For high temperature alloys
ASTM etchant No. 22 - HCl+H2O2 - For high temperature alloys
ASTM etchant No. 220 - Stainless steels - Chemical etching
ASTM etchant No. 22a - Ni superalloys - Chemical etching
ASTM etchant No. 22b - Co high temperature alloys - Chemical etching
ASTM etchant No. 23 - HCl-methanol
ASTM etchant No. 24 - Co high temperature alloys - Chemical etching
ASTM etchant No. 24 - HCl-HNO3-FeCl3 - For high temperature alloys
ASTM etchant No. 25 - Co high temperature alloys - Chemical etching
ASTM etchant No. 25 - High temperature steels - Chemical etching
ASTM etchant No. 25 - Marble's etchant - For high temperature alloys
ASTM etchant No. 25 - Ni superalloys - Chemical etching
ASTM etchant No. 25 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 25 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 26 - Cu alloys - Chemical etching
ASTM etchant No. 26 - For Cu and alloys
ASTM etchant No. 26 - Pure copper - Chemical etching
ASTM etchant No. 27 - Cu alloys - Chemical etching
ASTM etchant No. 27 - For Cu and alloys
ASTM etchant No. 27 - Pure copper - Chemical etching
ASTM etchant No. 28 - Cu alloys - Chemical etching
ASTM etchant No. 28 - Cu alloys - Chemical etching
ASTM etchant No. 28 - Ferric nitrate - For Cu and alloys
ASTM etchant No. 28 - Pure copper - Chemical etching
ASTM etchant No. 28 - Pure copper - Chemical etching
ASTM etchant No. 29 - Cu alloys - Chemical etching
ASTM etchant No. 29 - Potassium dichromate - For Cu and alloys
ASTM etchant No. 29 - Pure copper - Chemical etching
ASTM etchant No. 3 - Aluminum 000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 4000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 3 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 3 - Keller's etchant - For Al and alloys
ASTM etchant No. 3 - Pure aluminum - Chemical etching
ASTM etchant No. 30 - Ag-Cu alloys - Chemical etching
ASTM etchant No. 30 - Cu alloys - Chemical etching
ASTM etchant No. 30 - NH4OH+H2O - For Cu and alloys
ASTM etchant No. 30 - Pure copper - Chemical etching
ASTM etchant No. 31 - Amonium persulphate - For Cu, Cu-Al, Cu-Ni-Zr, Cu alloys
ASTM etchant No. 31a - Fe + C - Chemical etching
ASTM etchant No. 31b - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No. 31c - Fe + 12-20 Cr + 4-10 Ni + <7% - Electrolytic etching
ASTM etchant No. 31c - Fe + 12-20 Cr + 4-10 Ni + 7% - Electrolytic etching
ASTM etchant No. 31c - Pure Ni and high Ni alloys - Electrolytic etching
ASTM etchant No. 31d - Pure copper - Chemical etching
ASTM etchant No. 31d - Cu alloys - Chemical etching
ASTM etchant No. 31d - Cu-Al (aluminum bronze) - Chemical etching
ASTM etchant No. 31d - Nickel silver - Chemical etching
ASTM etchant No. 32 - Chromic acid - For Cu, Cu-Ni-Zn, Cu alloys
ASTM etchant No. 32 - Cu alloys - Chemical etching
ASTM etchant No. 32 - Nickel silver - Chemical etching
ASTM etchant No. 32 - Pure copper - Chemical etching
ASTM etchant No. 33 - Chromic/hydrochloric - For Cu, Cu-Al, Cu-Ni, Cu alloys
ASTM etchant No. 33 - Cu alloys - Chemical etching
ASTM etchant No. 33 - Nickel silver - Chemical etching
ASTM etchant No. 33 - Pure copper - Chemical etching
ASTM etchant No. 34 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 34 - For Cu, Cu-Al, Cu-Ni, Cu alloys
ASTM etchant No. 34b - Cu alloys - Chemical etching
ASTM etchant No. 34b - Cu-Al (aluminum bronze) - Chemical etching
ASTM etchant No. 34b - Pure copper - Chemical etching
ASTM etchant No. 35 - Cu alloys - Chemical etching
ASTM etchant No. 35 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 35 - Grard's No.1 etch - For Cu, Cu-Al, Cu alloy
ASTM etchant No. 35 - Pure copper - Chemical etching
ASTM etchant No. 36 - Cu alloys - Chemical etching
ASTM etchant No. 36 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 36 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 36 - Pure copper - Chemical etching
ASTM etchant No. 37 - Cu alloys - Chemical etching
ASTM etchant No. 37 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 37 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 37 - Pure copper - Chemical etching
ASTM etchant No. 38 - Cu alloys - Chemical etching
ASTM etchant No. 38 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 38 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 38 - Pure copper - Chemical etching
ASTM etchant No. 38- For Cu, Cu-Al, Cu alloys
ASTM etchant No. 39 - Cu alloys - Chemical etching
ASTM etchant No. 39 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 39 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 39 - Pure copper - Chemical etching
ASTM etchant No. 3a - Ti alloys - Chemical etching
ASTM etchant No. 3b - Aluminum 7000 series - Chemical etching
ASTM etchant No. 4 - For Al and Al base alloys
ASTM etchant No. 4 - Pure aluminium - Electrolytic etching
ASTM etchant No. 40 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 40 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 40 - For Cu, Cu-Al, Cu alloys
ASTM etchant No. 40 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 40 - Pure copper - Chemical etching
ASTM etchant No. 41 - Cu alloys - Chemical etching
ASTM etchant No. 41 - Cu-Be alloys - Chemical etching
ASTM etchant No. 41 - Cu-Cr alloys - Chemical etching
ASTM etchant No. 41 - Cu-Mn alloys - Chemical etching
ASTM etchant No. 41 - Cu-Si alloys - Chemical etching
ASTM etchant No. 41 - For Cu, Cu-Be, Cu-Cr, Cu-Mn, Cu-Si, Cu-Ni-Zn, Cu alloys
ASTM etchant No. 41 - Nickel silver - Chemical etching
ASTM etchant No. 41 - Pure copper - Chemical etching
ASTM etchant No. 42 - Cu alloys - Chemical etching
ASTM etchant No. 42 - For Cu, Cu-Ni-Zn, beta-brass
ASTM etchant No. 42 - Nickel silver - Chemical etching
ASTM etchant No. 42 - Pure copper - Chemical etching
ASTM etchant No. 43 - Cu alloys - Chemical etching
ASTM etchant No. 43 - For Cu and alloys
ASTM etchant No. 43 - Pure copper - Chemical etching
ASTM etchant No. 44 - Ammonium/peroxide - For Cu-Al, Cu alloys
ASTM etchant No. 44 - Cu alloys - Chemical etching
ASTM etchant No. 44 - Cu-Al (Aluminum bronze) - Chemical etching
ASTM etchant No. 45 - Cu-Al (Aluminum bronze) - Electrolytic etching
ASTM etchant No. 45 - Cu-Be alloys - Electrolytic etching
ASTM etchant No. 45 - For Cu-Al, Cu-Be
ASTM etchant No. 46 - Cu-Be
ASTM etchant No. 46 - Cu-Be alloys - Chemical etching
ASTM etchant No. 47 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 47 - Cyanide/persulphate - For Cu-Ni
ASTM etchant No. 47 - Pure Ni and high Ni alloys - Chemical etching
ASTM etchant No. 48 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 48 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No. 48 - For Cu-Ni
ASTM etchant No. 49 - Cu alloys - Electrolytic etching
ASTM etchant No. 49 - Cu alloys - Electrolytic etching
ASTM etchant No. 49 - Cu-Ni alloys - Electrolytic etching
ASTM etchant No. 49 - For Cu-Ni, Cu-Ni-Zn, Cu alloys, beta-brass
ASTM etchant No. 49 - Nickel silver - Electrolytic etching
ASTM etchant No. 5 - Aluminum 1000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 3000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 5000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 6000 series - Electrolytic etching
ASTM etchant No. 5 - Aluminum 7000 series - Electrolytic etching
ASTM etchant No. 5 - Barker's etchant - For Al base alloys and brass
ASTM etchant No. 5 - Pure aluminum - Electrolytic etching
ASTM etchant No. 50 - Cu-Ni alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ag alloys - Chemical etching
ASTM etchant No. 50 - Ni-Al alloys - Chemical etching
ASTM etchant No. 50 - Ni-Cr alloys - Chemical etching
ASTM etchant No. 50 - Ni-Fe alloys - Chemical etching
ASTM etchant No. 50 - Ni-Ti alloys - Chemical etching
ASTM etchant No. 50 - Nitric/acetic - For Cu-Ni
ASTM etchant No. 51 - Cu-Sn (Tin bronze) - Chemical etching
ASTM etchant No. 51 - For Cu-Sn
ASTM etchant No. 51 - Pure tin - Chemical etching
ASTM etchant No. 52 - Cu-Sn (Tin bronze) - Chemical etching
ASTM etchant No. 52 - Cu-Sn (tin bronze)
ASTM etchant No. 53 - Cu alloys - Chemical etching
ASTM etchant No. 53 - For Cu alloys (polish)
ASTM etchant No. 54 - Cu alloys - Electrolytic etching
ASTM etchant No. 54 - For brass
ASTM etchant No. 55 - Dysprosium - Chemical etching
ASTM etchant No. 55 - Erbium - Chemical etching
ASTM etchant No. 55 - For Dy, Er, Gd, Ho
ASTM etchant No. 55 - Gadolinium - Chemical etching
ASTM etchant No. 55 - Holmium - Chemical etching
ASTM etchant No. 56 - Dysprosium - Chemical etching
ASTM etchant No. 56 - Erbium - Chemical etching
ASTM etchant No. 56 - For Dy, Er, Gd, Ho
ASTM etchant No. 56 - Gadolinium - Chemical etching
ASTM etchant No. 56 - Holmium - Chemical etching
ASTM etchant No. 57 - Acetic acid/peroxide - For Gd
ASTM etchant No. 57 - Gadolinium - Chemical etching
ASTM etchant No. 57 - Pb + <2 Sb - Chemical etching
ASTM etchant No. 57 - Pure lead - Chemical etching
ASTM etchant No. 58 - For Ge
ASTM etchant No. 58 - Germanium - Chemical etching
ASTM etchant No. 59 - For Ge
ASTM etchant No. 59 - Germanium - Chemical etching
ASTM etchant No. 6 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 3000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 5000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 6 - Aluminum 7000 series - Chemical etching
ASTM etchant No. 6 - For Al base alloys
ASTM etchant No. 60 - CP4 etchant - For Ge
ASTM etchant No. 60 - Germanium - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - >90% noble metals - Chemical etching
ASTM etchant No. 61 - Ag alloys - Chemical etching
ASTM etchant No. 61 - For Au and noble metals (>0%)
ASTM etchant No. 61 - Pure gold - Chemical etching
ASTM etchant No. 61 - Pure palladium - Chemical etching
ASTM etchant No. 62 - Ag alloys - Chemical etching
ASTM etchant No. 62 - Au alloys - Chemical etching
ASTM etchant No. 62 - For Au and alloys
ASTM etchant No. 62 - Pd alloys - Chemical etching
ASTM etchant No. 62 - Pure Ag - Chemical etching
ASTM etchant No. 62 - Pure gold - Chemical etching
ASTM etchant No. 62 - Pure palladium - Chemical etching
ASTM etchant No. 63 - Au alloys - Chemical etching
ASTM etchant No. 63 - For Au (polish) and Au alloys
ASTM etchant No. 63 - Pure gold - Chemical etching
ASTM etchant No. 64 - For Au alloys
ASTM etchant No. 64a - Pd alloys - Chemical etching
ASTM etchant No. 64a - Pure platinum - Chemical etching
ASTM etchant No. 64b - Au alloys - Chemical etching
ASTM etchant No. 64b - Pt alloys - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - <90% noble metals - Chemical etching
ASTM etchant No. 65 - Ag alloys - Chemical etching
ASTM etchant No. 65 - For noble metals (<0%)
ASTM etchant No. 66 - For Hf alloys
ASTM etchant No. 66 - Hafnium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
ASTM etchant No. 66 - Niobium - Chemical etching
ASTM etchant No. 66 - Ta alloys - Chemical etching
ASTM etchant No. 66 - Tantalum - Chemical etching
ASTM etchant No. 66 - Zirconium - Chemical etching
ASTM etchant No. 67 - For Hf base alloys
ASTM etchant No. 67 - Hafnium - Chemical etching
ASTM etchant No. 67 - Pure titanium - Chemical etching
ASTM etchant No. 67 - Pure uranium - Chemical etching
ASTM etchant No. 67 - Ti alloys - Chemical etching
ASTM etchant No. 67 - U alloys - Chemical etching
ASTM etchant No. 67 - Zirconium - Chemical etching
ASTM etchant No. 68 - For Hf base alloys
ASTM etchant No. 68 - Hafnium - Electrolytic etching
ASTM etchant No. 68 - Pure titanium - Electrolytic etching
ASTM etchant No. 68 - Ti alloys - Electrolytic etching
ASTM etchant No. 68 - U + Zr alloys - Electrolytic etching
ASTM etchant No. 68 - Zirconium - Electrolytic etching
ASTM etchant No. 69 - For Hf base alloys
ASTM etchant No. 69 - For Hf base alloys
ASTM etchant No. 69 - Hafnium - Electrolytic etching
ASTM etchant No. 69 - Pure titanium - Electrolytic etching
ASTM etchant No. 69 - Pure uranium - Electrolytic etching
ASTM etchant No. 69 - Ti alloys - Electrolytic etching
ASTM etchant No. 69 - U alloys - Electrolytic etching
ASTM etchant No. 69 - Zirconium - Electrolytic etching
ASTM etchant No. 7 - Aluminum 1000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 2000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 3000 series - Chemical etching
ASTM etchant No. 7 - Aluminum 6000 series - Chemical etching
ASTM etchant No. 7 - For Al base alloys
ASTM etchant No. 70 - For Hf base alloys
ASTM etchant No. 70 - Hafnium - Chemical etching
ASTM etchant No. 71 - For Hf base alloys
ASTM etchant No. 71 - Hafnium - Chemical etching
ASTM etchant No. 71 - Zirconium - Chemical etching
ASTM etchant No. 72 - For Hf base alloys
ASTM etchant No. 73 - For Ir base alloys
ASTM etchant No. 73a - Pt alloys - Electrolytic etching
ASTM etchant No. 73a - Pure platinum - Electrolytic etching
ASTM etchant No. 73b - Ruthenium - Electrolytic etching
ASTM etchant No. 73b - Ruthenium - Electrolytic etching
ASTM etchant No. 73c - Iridium - Electrolytic etching
ASTM etchant No. 74 - Nital - For steels
ASTM etchant No. 74a - Fe + C - Chemical etching
ASTM etchant No. 74a - Fe + C - Chemical etching
ASTM etchant No. 74a - Mg-Al, Mg-Al-Zn (Al + Zn <5% - Chemical etching
ASTM etchant No. 74a - Mg-Al, Mg-Al-Zn (Al + Zn >5% - Chemical etching
ASTM etchant No. 74a - Mg-Mn alloys - Chemical etching
ASTM etchant No. 74a - Mg-Th-Zr alloys - Chemical etching
ASTM etchant No. 74a - Mg-Zn-Zr alloys - Chemical etching
ASTM etchant No. 74a - Pure iron - Chemical etching
ASTM etchant No. 74a - Pure magnesium - Chemical etching
ASTM etchant No. 74a - Tool steels - Chemical etching
ASTM etchant No. 74a - Zn-Fe alloys - Chemical etching
ASTM etchant No. 74b - Pb + <2 Sb - Chemical etching
ASTM etchant No. 74b - Pb + >2 Sb - Chemical etching
ASTM etchant No. 74b - Pb Babbitt - Chemical etching
ASTM etchant No. 74b - Sn-Pb alloys - Chemical etching
ASTM etchant No. 74d - Pure tin - Chemical etching
ASTM etchant No. 74d - Sn-Cd alloys - Chemical etching
ASTM etchant No. 74d - Sn-Fe alloys - Chemical etching
ASTM etchant No. 74e - Ni-Fe alloys - Chemical etching
ASTM etchant No. 74e - Ni-Mn alloys - Chemical etching
ASTM etchant No. 75 - Gorsuch's etchant - Iron
ASTM etchant No. 75 - Pure iron - Chemical etching
ASTM etchant No. 76 - Fe + C - Chemical etching
ASTM etchant No. 76 - Picral - Fe + C
ASTM etchant No. 77 - Fe + C - Chemical etching
ASTM etchant No. 77 - Fe + C - Chemical etching
ASTM etchant No. 77 - Super picral - Fe + C
ASTM etchant No. 78 - Fe + <1C + <4% additions
ASTM etchant No. 78 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No. 78 - Fe + 1C + <4% additions - Chemical etching
ASTM etchant No. 78 - Fe + C - Chemical etching
ASTM etchant No. 79 - Fe + C - Chemical etching
ASTM etchant No. 79 - Fry's etchant - Fe + C
ASTM etchant No. - For Al-Cu, Al-Mg, Al-Si, Cu
ASTM etchant No.0 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.0 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.0 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.0 - Tool steels - Chemical etching
ASTM etchant No.0 - Vilella - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + <1C + <4% additions
ASTM etchant No.1 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.1 - Steels, carbon and alloy types - Chemical etching
ASTM etchant No.2 - Acid ferric chloride - Fe + <1C + <4% additions
ASTM etchant No.2 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.3 - Fe + <1C + <4% additions
ASTM etchant No.3 - Fe + <1C + <4% additions - Electrolytic etching
ASTM etchant No.3 - Ni-Cr alloys - Electrolytic etching
ASTM etchant No.3 - Ni-Fe alloys - Electrolytic etching
ASTM etchant No.3a - Fe + 15-30 Cr + 6-40 Ni + <5% - Electrolytic etching
ASTM etchant No.3b - Non-stainless maraging steels - Electrolytic etching
ASTM etchant No.4 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.4 - Howarth's etchant - Fe + <1C + <4% additions
ASTM etchant No.5 - Alkaline sodium picrate - Fe + <1C + <4% additions
ASTM etchant No.5 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.6 - Fe + <1C + <4% additions - Chemical etching
ASTM etchant No.6 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.6 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.6 - Fe + 16-25 Cr + 3-6 Ni + 5-1C - Chemical etching
ASTM etchant No.6 - High temperature steel - Chemical etching
ASTM etchant No.6 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.6 - Tool steels - Chemical etching
ASTM etchant No.7 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - Glyceregia - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.9 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.9 - High temperature steels - Chemical etching
ASTM etchant No.9 - Ni-Al alloys - Chemical etching
ASTM etchant No.9 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.a - Aluminum 2000 series - Chemical etching
ASTM etchant No.a - Aluminum 3000 series - Chemical etching
ASTM etchant No.a - Aluminum 5000 series - Chemical etching
ASTM etchant No.a - Aluminum 6000 series - Chemical etching
ASTM etchant No.a - Aluminum 6000 series - Chemical etching
ASTM etchant No.b - Admiralty metal - Electrolytic etching
ASTM etchant No.b - Pure copper - Electrolytic etching
ASTM etchant No. - Beryllium - Chemical etching
ASTM etchant No. - For Be
ASTM etchant No. - Pure cobalt - Chemical etching
ASTM etchant No.0 - HNO3-HF in glycerol - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.1 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.1 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.2
ASTM etchant No.3
ASTM etchant No.4 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.4 - Kalling's etchant No. 2 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.4 - Ni superalloys - Chemical etching
ASTM etchant No.5 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.5 - Kalling's etchant No. 1 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.6 - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.6 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.7 - High temperature steels - Chemical etching
ASTM etchant No.7 - Potassium hydroxide - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Fe + 15-30 Cr + 6-40 Ni + <5% - Chemical etching
ASTM etchant No.8 - Murakami's etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
ASTM etchant No.8 - Ni-Cr alloys - Chemical etching
ASTM etchant No.8c - Molybdenum - Chemical etching
ASTM etchant No.8c - Pure tungsten - Chemical etching
ASTM etchant No.8c - Rhenium - Chemical etching
ASTM etchant No.9 - Beraha's etchant - Fe + 12-20 Cr + 4-10 Ni + <7%
ASTM etchant No.9 - Fe + 12-20 Cr + 4-10 Ni + <7% - Chemical etching
ASTM etchant No.9 - Fe + 16-25 Cr + 3-6 Ni + 5-1C - Chemical etching
ASTM etchant No.9 - Non-stainless maraging steels - Chemical etching
ASTM etchant No.57 - Pb + >2 Sb - Chemical etching
Abraham's AB etchant - - Gallium arsenide
Accary etchant - U-C alloys - Electrolytic etching
Accary etchant - Uranium - Chemical etching
Accary etchant - Uranium - For etching U carbide
Acetic glycol etchant - Magnesium - Chemical etching
Acetic glycol etchant - Rare earth - Chemical etching
Acetic-glycol etchant - Mg and alloys - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Acetic-picral etchant - Magnesium - Chemical etching
Adcock etchant - Lead - Electrolytic etching
Adcock etchant - Pb-Sb alloys - Electrolytic etching
Adler's etchant - Stainless steel - Chemical etching
Adler's etchant - Co and Co-Al alloys - Chemical etching
Adler's etchant - For iron and steels - General macrostructure
Adler's etchant - For the investigation of the cast structure and the heat-affected zone in welds in steels
Adler's etchant - High-alloy, corrosion-resistant steels, Co and Ni alloys
Adler's etchant - Ni alloys - General macrostructure
Adler's etchant - Ni brazing alloys when brazed to steels - Galvanic Ni coatings - Chemical etching
Adler's etchant - Ni-base foundary alloys - Chemical etching
Adler's etchant - Pd-Ga alloy (Pd5Ga2) - Chemical etching
Adler's etchant - Stainless steel
Adler's etchant - Stainless steel
Adler's etchant - Steel for turbine blades - Chemical etching
Adler's etchant - Welded steel - Chemical etching
Aqua Regia - Au-Al alloys - Chemical etching
Aqua Regia - Austenitic stainless steels
Aqua Regia - Austenitic stainless steels - Chemical etching
Aqua Regia - Austenitic stainless steels - Chemical etching
Aqua Regia - Aluminium - Chemical etching - Electrolytic polishing
Agua Regia - Au thin films and specimens - Chemical etching
Agua Regia - AuSn (20%) alloy as an evaporated thin film - Chemical etching
Aqua Regia - Chromium - Chemical etching
Aqua Regia 6% - Cemented carbides (Co) - Electrolytic etching
Aqua Regia 5% - 73 J (Co-20Cr-6Mo) alloy - Chemical etching
Agua Regia - Cr and Cr alloys - Chemical etching
Agua Regia - Ir crystalline specimens as wire, rod, sheet - Chemical etching
Agua Regia - Ir thin films deposited on silicon (100), n-type - Chemical etching
Agua Regia - IrPt as alloy mixtures - Chemical etching
Agua Regia - IrV and Ir80V20 thin films - Chemical etching
Aqua Regia - Fe-Ni-Cr heat resistant casting alloys - Etchant for delineating general structure
Aqua Regia - Gold - Chemical etching
Aqua Regia - Heat resistant alloys - Chemical etching
Aqua Regia - Lead sulphide (PbS) - Chemical polishing
Aqua Regia - Lead sulphide-selenide (PbS(1-x) x Se(x)) - Chemical etching
Aqua Regia - Molybdenum - Chemical etching
Aqua Regia - Ni and Ni alloys
Aqua Regia - Ni-Cr-Fe alloys (Inconel) - Chemical etching
Agua Regia - Mo specimens - Chemical polishing
Agua Regia - Ni alloys - General macrostructure
Agua Regia - Ni superalloys, Ni-Cr alloys - Chemical etching
Agua Regia - Ni-Cr thin films evaporated on (111) and (100) oriented Si - Chemical etching
Aqua Regia - Pd thin film - Chemical cleaning
Aqua Regia - PdAu deposited as a 11 mixture on glass, quartz, and aapphire substrates - Chemical etching
Aqua Regia - Platinum - Chemical etching
Aqua Regia - Pt and alloys - Chemical etching
Aqua Regia - Pt-Tb alloys (20-35 at.% Tb) - Etch for TbPt3
Aqua Regia - Pure Au and alloys
Aqua Regia - Pure gold - Chemical etching
Agua Regia - Pd-H as powdered "Palladium Black" with absorbed hydrogen
Agua Regia - PdAg alloy - Chemical etching
Agua Regia - PdNiP, PtNiP, and PtCuP metallic glasses - Chemical etching
Agua Regia - Pt and Au evaporated on silicon (111) - Chemical etching
Agua Regia - PtRh (2-15%) as thermocouple wires - Chemical cleaning
Agua Regia - Pure Au, Au-Pt and Au-Ag alloys with more than0% Au - Chemical etching
Aqua Regia - Refactaly steel - Chemical etching - General microstructure
Aqua Regia - Rh alloys - Chemical etching
Aqua Regia - Rh specimens as wire, rods, sheets, and plated coatings - Chemical etching
Aqua Regia - Rhodium - Chemical etching
Aqua Regia - Ru specimens - Chemical etching
Agua Regia - Rare earth nickelides - Chemical etching
Aqua Regia - Se Chemical etching
Aqua Regia - Selenium - Chemical etching
Aqua Regia - SnGe (1%) thin films - Chemical etching
Aqua Regia - Stainless steel - Chemical etching
Aqua Regia - Stainless steel - Chemical etching
Aqua Regia - Si (111) and (100) wafers - Chemical cleaning
Agua Regia - Si3N4, oxynitrides, SiO2 as thin films or glass and quartzware - Chemical cleaning
Agua Regia - SiO2 as single crystal natural quartz, artificial quartz, and vitreous silica (fused glass)
Agua Regia - Sn (100) single crystal - Chemical etching
Agua Regia - Te (10T0) cleaved wafers - Chemical polishing/etching
Agua Regia - Th specimen - Chemical polishing
Aqua Regia - Ti0.3W0.7Si2 thin films - Chemical polishing
Agua Regia - Ti3W7Si2 thin films on silicon wafers, (111), (110) and (100) - Chemical etching
Agua Regia - TiO2 single crystal natural rutile crystals - Chemical cleaning
Agua Regia - TiW (1% Ti) thin films - Chemical etching
Agua Regia - TlBiTe2 single crystal n-type - Chemical polishing/etching
Agua Regia - V specimens - Chemical ething
Agua Regia - W specimens - Chemical etching
Aqua Regia - Wrought heat-resistant steels - Chemical etching
Aqua Regia - ZnTe thin film deposits - Chemical etching
Agua Regia - Zr specimens - Chemical etching
Agua Regia - a-Zr2Pd thin films - Chemical polishing/etching
Agua Regia - a-Zr3Rh amorphous thin films - Chemical polishing/etching
Agua Regia, dilute - Pd thin films - Chemical cleaning
Agua Regia, modified - Ni specimens - Chemical etching
Aqua Regia plus acetic acid etchant - Ferritic stainless steels - Chemical etching
Aqua Regia, dilute - Alloy steels - General macrostructure
Aqua Regia, dilute - Austenitic stainless steels - Chemical etching
Aqua Regia, dilute - High speed steels
Aqua Regia, dilute - Pb-Te-Co system - Lead telluride-Cobalt section
Aqua Regia, modified - GaP (111) wafers - Chemical etching
Alcoholic ferric chloride etchant - Cu and Cu alloys
Aldridge's etchant - Chemical etching
Alexander's etchant - Chemical etching
Alkaline sodium picrate etchant - Chemical etching
Alkaline sodium picrate etchant - High carbon steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Chemical etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - Tool steels - Electrolytic etching
Alkaline sodium picrate etchant - W-Co eutectic alloys - Chemical etching
Allen's etchant - InSb (111) wafers - Chemical polishing
Amberg's etchant - High speed steels - Chemical etching
Amberg's etchant - Martensitic stainless steels - Chemical etching
Ambler and Slattery's etchant - UO2 - Chemical etching
Ambler and Slattery's etchant - Uranium - Electrolytic etching
Ambler's etchant - Zr3Al alloys - Chemical etching
Ambler's etchant - Zr3Al-based alloys - Chemical etching
Amine Gallate etching of silicon wafers I - Chemical etching
Ammonium persulphate etchant - Steels - Chemical etching
Amyl nital - Iron and steels - Chemical etching
Amyl nital etchant - Steels - etching
Anderson's etchant - For etching pure Mn and lean alloys - Chemical etching
Anderson's etchant - Manganese - Chemical etching
B etchant - For Ti
B etchant - Silicon - Chemical etching
BCK-111 etchant - InP (100) wafers - Chemical etching
BF3 etchant - Si single crystal spheres - Chemical ecthing
BHF etchant - NxSiO2 thin films - Chemical etching
BHF etchant - Si (100), p-type, 2 Ohm cm resistivity wafers - Chemical etching
BHF etchant - Si thin film epitaxy grown on (100) silicon wafer substrates
BHF etchant - Si3N4 thin film amorphous deposits - Chemical etching
BHF etchant - Si3N4 thin films RF plasma grown on silicon - Chemical etching
BHF etchant - Si3N4 thin films deposited on (100) silicon wafers - Chemical cleaning
BHF etchant - SiO2 thin films thermally evaporated - Chemical etching
BHF etchant - Ta (111) and (100) wafers - Chemical etching
BHF etchant - TiN thin films - Chemical etching
BHF etchant - TiN thin films deposited on poly-Si epitaxy layers - Chemical etching
BHF etchant - Zr specimens used for electroplating
BHF etchant, modified - Si3N4 and Si3NxOy thin films - Chemical etching
BHF etchant, modified - Si3N4 thin films - Chemical etching
BJ etchant - Ge (111) wafers - Chemical polishing
BPK-221 etchant - InP (100) wafers - Chemical etching
BRM etchant - InP (100) n-type wafers - Chemical polishing
BRM etchant - WS2 single crystal specimens - Chemical polishing
BRM etchant - WSe2 single crystal specimens - Chemical polishing
BRM etchant - p-GaSb (111) wafers - Chemical etching
BSG as borosilicate glass on silicon - Metal diffusion
BSG etchant - SiO22 as a BSG glassy layer on silicon - Chemical etching
Bain-Vilella's etchant - Steel specimens - To reveal the prexisting austenite grain boundaries and tempered steels
Baker's etchant - Pure Al, Al-Zn, Al-Mn, Al-Mg-Si, Al-Zn-Mg and Al-Mn-Mg alloys - Electrolytic etching
Barber's etchant - NaCl (100) wafers - Chemical etching
Barker's anodizing solution for grain structure - Al and Al alloys - Chemical etching
Barker's etchant - 1000 series aluminium
Barker's etchant - Aluminium alloys - 1xxx, 3xxx, 5xxx, 6xxx series alloys, most casting alloy
Baumann print - Sulfur print, unalloyed steels, sulfide inclusions
Beaujard and Tordeux's tint etchant - Tint etchant for steels
Beaujard and Tordeux`s tint etchant - Reveals grain boundaries and ferrite orientations
Beaujard's tint etchant - Tint etchant for steels
Beaujard's tint etchant - Tint etchant for steels
Bechet and Beaujard's etchant - Martensitic and bainitic steels - Chemical etching
Beck's solution - Aluminium
Beck's solution - Aluminium - Dislocation etching
Beraha's E etchant - Ni superalloys
Beraha's I etchant - Unalloyed and low alloy steels
Beraha's II etchant - Austenitic CrNi steels - Chemical etching
Beraha's II etchant - High-alloy steels
Beraha's III I etchant - Ni-base alloys, Hastelloy X, Hastelloy
Beraha's III etchant - Ni base casting alloys - Chemical etching
Beraha's III etchant - Ni-base alloys with more thanMo, Hastelloy X, Hastelloy C - Chemical etching
Beraha's III etchant - Ni-base and Co-base alloys
Beraha's cadmium sulfide tint etchant - For Fe, steel, and ferritic and martensitic stainless steel - Chemical etching
Beraha's etchant - Al and Al alloys - Chemical etching
Beraha's etchant - Cu alloys, cast irons, ferritic and martensitic stainless steels
Beraha's etchant - Iron, steels, cast irons - Tint etchant for pure iron and carbon steels, cast iron, and alloyed steels
Beraha's etchant - Martensitic chromium steels - Tint etching
Beraha's etchant - Martensitic chromium steels - Tint etching
Beraha's etchant - Steels specimen - Sulfides are colored yelow and matrix dark
Beraha's lead sulfide tint etchant - Iron and steels - Chemical etching
Beraha's martensite etchant - Color etching for ADI iron
Beraha's selenic acid etchant for copper
Beraha's selenic acid etchant for steels and superalloys
Beraha's sodium molybdate etchant - For steels
Beraha's tint etchant - For Al alloys - Chemical etching
Beraha's tint etchant - Al and Al alloys - Tint etching
Beraha's tint etchant - Austenitic stainless steels, maraging steels, PH gredes
Beraha's tint etchant - Brass and Cu-Be alloys - Tint etching
Beraha's tint etchant - Cast Ti alloys - Tint etching
Beraha's tint etchant - Co-based alloys - Tint etching
Beraha's tint etchant - Cu and Cu alloys - Tint etching
Beraha's tint etchant - Cu, brass, bronze alloys - Tint etching
Beraha's tint etchant - Ferritic and martensitic stainless steels, Mn steels, tool steels
Beraha's tint etchant - For cast irons, steels, tool steels, Mn steels, and ferritic and martensitic stainless steels - Chemical etching
Beraha's tint etchant - For ferrite - Chemical etching
Beraha's tint etchant - For irons, steels, tool steels
Beraha's tint etchant - For pearlitic steels and and cast irons - Chemical etching
Beraha's tint etchant - For stainless steels
Beraha's tint etchant - For stainless steels
Beraha's tint etchant - Ni superalloys - Tint etching
Beraha's tint etchant - Ni-base alloys
Beraha`s lead sulfide tint etchant - Chemical etching - General macrostructure
Beraha`s tint etchant - For iron and steels
Beraha`s tint etchant - For stainless steels
Beraha`s tint etchant - For Fe, Ni, or Co base heat resistant alloys
Beraha`s tint etchant - For cast iron and steels
Beraha`s tint etchant - For stainless steels
Bichromate finish dip etchant - Brass (70Cu-30Zn), bronze, and copper parts - Chemical etching
Billig's etchant - For Ge, Si
Bish's etchant - For iron and steels - General macrostructure
Blackburn and William's solution - A286 stainless steel - Standard and modified
Blackburn and William's solution - Ti-Mo alloy - Alloy with 11.6% Mo
Blackburn and William's solution - Ti-Mo-Al-Sn-Zr alloy - Titanium 6246-6Al-2Sn-4Zr-6 Mo
Blackburn and Williams's solution - Ti-Mo alloys
Blackburn-William's electrolyte - Ti-Al-Nb alloy - Ti3Al-Nb
Boss's etchant - Al and Al alloys - Chemical etching
Bossert's etchant - Al and Al alloys - Chemical etching
Bright dip etchant - Brass, bronze, and copper alloy
Bright-field etchant for U - Electrolytic etching
Brilliant's etchant - Cu and Cu alloys
Brilliant's etchant - Cu and Cu alloys - Chemical etching
Brite dip etchant - Aluminium and alloys
Bromine etchant - As (111) specimens - Dislocation etching
Canada's etchant - Nickel superalloys
CP4 etchant - LiF - Dislocation etching
CP4 etchant - Antimonium - Dislocation etching
CP4 etchant - For Si, Ge, Sb, TiC, InSb, InAs
CP4 etchant - InSb (111) wafers - Chemical polishing
CP4 etchant - LiF (10O) cleaved wafers - Dislocation etching
CP4 etchant - Si wafers - Chemical etching
CP4 etchant - Si-Ge single crystal ingots - Chemical etching
CP4 etchant - Silicon - Chemical polishing
CP4 etchant - Te (0001) cleaved wafers - Chemical etching
CP4 etchant - ZnO thin film deposit - ZnO thin film deposit formed by oxidation of ZnSe
CP4 etchant, modified - InAs (111) wafers used in a polarity study - Chemical etching
CP4 etchant, modified - Silicon specimens - Chemical etching
CP4 etchants, dilute CP4, modified - Ge (111), (100), (110), and (211) wafers - Chemical etching
CP4, variety CP4A etchant - InSb (111) wafers and other orientation - Chemical polishing
CP4A etchant - FeGe2 (100) and (110) wafers - Chemical etching
CP4A etchant - InSb (111) wafers - Chemical etching
CP4A etchant - Si (111) wafers and other orientations - Chemical polishing
CP4A or CP8 etchants - Silicon - Final chemical polishing
Cain's B etchant - For Hf
Cain's etchant - Hf, Zr and allloys - Chemical etching
Cain's etchant - Hf-W eutectoid alloys - Chemical etching
Camp No. 2 (Superoxol) etchant - Si (111) n-type wafers and p-doped with 60Co - Chemical etching
Camp No. 2 (Superoxol, CP2) etchant - Ge (111) wafers - Chemical etching
Camp No. 3 (CP3) etchant - Ge (111) wafers - Chemical etching
Camp No. 4 (CP4) etchant - Ge (100) wafers and other orientations - Chemical polishing/etching
Camp No. (CP8) etchant - Si (111) wafers - Chemical etching
Canada's etchant - Nickel superalloy 718 - Chemical etching
Canfield's etchant - For iron and steels - General macrostructure
Carapella's etchant - Fe-Ni, Ni-Cu, and Ag alloys, Ni-base superalloys, Monel metal
Carapella's etchant - Ni and Ni-Cu (Monel) alloys - Chemical etching
Caro's etch, modified - Si (111) p-type wafers used for diffusion of antimony from glass
Caro's etchant - GaAs (100) n-type wafers grown by LEC as ingots - Chemical etching
Caro's etchant - Si (111) wafers and other orientations - Chemical cleaning
Caro's etchant, modified - Si (111) wafers used in a study of ion bombardment cleaning - Chemical polishing
Carpella's etchant - Ni-B alloys - Chemical etching
Carpenter special #4 etchant - AerMet 310/340, AerMet 100 steels - Chemical etching
Carpenter special #5 etchant - Co-Ni alloys - Chemical etching
Caustic etchant - Al and Al alloys - General macrostructure
Chase's etchant - Ag-30% Zn alloy - Chemical polishing
Chen-Hendrickson's etchant - For Ag
Chrome etchant - Au thin films and specimens - Chemical etching
Chrome etchant - Au-Cr thin films - Chemical etching
Chrome etchant - Cr thin films - Chemical etching
Chrome etchant - Cr2O3 amorphous thin films - Chemical etching
Chrome etchant - For Cr thin films
Chrome etchants, modified - Cr thin film deposits on glass substrates
Chrome regia etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
Chrome regia etchant - Si wafers both float zone ingot material and epitaxy thin film deposit
Chrome regia etchant - Si3N4 oxynitrides and SiO2 thin films - Chemical cleaning
Chrome regia etchant - Stainless steels - Chemical etching
Coates's etchant - Pb-Sn-Te alloys
Coates's etchant - Pb-Sn-Te alloys (Pb(1-x)Sn(x)Te, x <= 0.03) - Chemical polishing and etching
Comstock's etchant - For iron and steels - General macrostructure
Contrast etchant - Ni-Al alloys
Cook's etchant - NaCl (100) wafers - Chemical etching
Coon's electrolytic etchant - Bi alloy and 5% Sb
Copper britte dip etchant - Cu specimens and parts - Chemical polishing
Copper dislocation etchant - Si single crystal wafers of different orientations - Chemical etching
Copper etchant - Si (111) wafers and other orientations - Chemical etching
Corke and Amelincky's electropolish solution - Cu-Pt alloy - Electrolytic etch
Crowell's etchant - Ag-Sn-Zn-Cu alloys, Cu-Sn-Ag dental alloys
Crowell's etchant - Ag-Sn-Zn-Cu dental amalgam alloys - Chemical etching
Crowell's etchant - Cu-Sn-Ag dental alloys - Chemical etching
Crowell's etchant - Cu-Sn-Ag dental alloys - Chemical etching
Curan's etchant - Stainless steels - Chemical etching
Czochralski's - Antimony specimens - Grain contrast etch
Czochralski's etchant - Antimony - Chemical etching
Czochralski's etchant - Sb alloys
DE-100 etchant - SiO2 thin films deposited by Silox system method on (100) silicon and GaAs-Cr (SI) wafers - Ionized gas etching
Dash etchant - Sb (0001) specimen
Dash etchant - Sb (0001) specimen cleaved in LN2
Dash etchant - Sb (0001) specimen cleaved in LN2
Dash etchant - Sb (OOO1) specimen
Dash etchant, modified - Sb (0001) specimen cleaved in LN2
Dash etchant, modified - Sb (0001) specimen cleaved in LN2
Dash's copper decoration etchant - Si (111) wafers - Metal difusion
Dash's etchant - Si (111) wafers and other orientations, both n- and p-type of different resistivity levels
Dash's etchant, modified - Si (100), (111), (110) and (112) wafers
Dash's etchant, modified - Si (111) wafers - Chemical etching
DeSy's etchant - For iron and steels - General macrostructure
Dickenson's etchant - Fe-As alloys - For alloys with 0.6 - 4.6 at.% As
Dickenson's etchant - For cast steels
Dickenson's etchant - For iron and steels - General macrostructure
Dix and Keller etchant - Al, Al-Cu alloys, Al-Si alloys - Chemical etching
Dix-Keller's etchant - Foamed Al, Al alloys, Al-Zr-Ti alloys
Dix-Keller's etchant - For most Al types and alloys except for Al alloys with high Si content, Al foils - Chemical etching
Dix-Keller's etchant - Pure Al and Al alloys
Doped ZnO-ZnO-0.5 mole % each of Bi2O3, CaO, MnO, SnO2
Dow's etchant
DuPont Nb etchant - Nb-Hf and Nb alloys - Chemical etching
Dual phase steel etchants - Chemical etching
E etchant - Ni superalloys
E etchant - Zn (0001) wafers - Chemical etching
EAg1 etchant - CdTe (100), (111) and (110) wafers - Chemical etching
EAg2 etchant - CdTe (100), (111), and (110) wafers - Chemical etching
EDTA etchant - CaCO3 r(1011) cleaved wafers - Acid cleaning
EDTA etchant - Li-alumina-silica glass - Li2O x Al2O3 x SiO2
EI-IR etchant - Steels for high temperatures
EPW etchant - Si (111) and (100), p-type 1 - 10 Ohm cm and n-type wafers - Chemical etching
Ellis's No. 1 etchant - Ge spheres and hemispheres - Chemical etching
Ellis's No. 5 etchant - Ge spheres and hemispheres - Chemical etching
Ellis's No. 7 etchant - Ge spheres and hemispheres - Ge spheres and hemispheres
Emanuel's etchant - Cast steels - Chemical etching
Emanuel's etchant - Fe-Ni-Cr heat resistant casting alloy - Attacks sigma phase with little or no effect on carbide particles
Ence and Margolin's etching solution (H-etch) - Ti alloys - Electrolytic etching
Erhard's etchant - Si (111) wafers - Dislocation etching
Etch pits etchant - Nickel oxide (NiO)
Etch pits etchant - Selenium
Etchant No. 2 - InSb (100) and (110) wafers - Chemical etching
Evans etchant - Inconel 617 - Chemical etching
F (Fast) etchant - Silicon - Chemical etching
F etchant - LiF - Dislocation etching
Ferric cyanide etchant - Ge hemispheres - Chemical etching
Finlay's A etchant (Remington's A etchant) - For Ti and Ti/Zr
Finlays B etchant - For Ti
Fisher-Marcinkowski's electropolish solution
Flat's etchant - Ni-Ti alloys
Flick's etchant - Al, cast alloys
Flick's etchant - Aluminium - Pure Al, Cu-Al alloys - General macrostructure
Flick's etchant - Aluminium and its alloys - For 2xxx Al alloys, high Cu aloys
Flick's etchant - Pure Al and Al alloys
Flick’s etchant - 2XXX, high Cu alloys - Chemical etching - General macrostructure
Flinn's etchant - For iron and steels - General macrostructure
Flint glass - Etching for revealing recrystallization effects
Fluor regia - Silicon - Chemical etching
Fluor regia etchant - Cr and Cr alloy - Chemical etching
Fluor regia etchant - Nb and alloys - Chemical etching
Fluor regia, modified - Beryllium - Chemical etching
Franchini's color etchant - Al-Si-Cu-Ni cast alloys - Chemical etching
Frank's etchant - Fe + 16-25 Cr + 3-6 Ni + 5-1C
Frey's etchant - Flow lines in low carbon N2 steels, convertor steels - Chemical etching
Fry's No. 1 etchant - For iron and steels - General macrostructure
Fry's No. 2 etchant - For iron and steels - General macrostructure - General macrostructure
Fry's No. 4 etchant - For iron and steels - General macrostructure
Fry's etchant (1) - Flow lines in low carbon N2 steels, Thomas steels
Fry's etchant (2)
Fry's etchant - Fe pure metal samples - Chemical etching
Fry's etchant - Fe-Si specimens and other iron alloys - Chemical etching
Fry's etchant - Iron - Dislocation etching
Fry's etchant - Iron and steel specimens - Mild steel specimens, Bessemer and high N2 steel specimens
Fry's etchant - Iron and steels - Chemical etching
Fry's etchant - Iron, steel specimens, cast irons - Flow lines in low carbon N2 steel specimens
Fry's etchant - Iron, steels, cast irons - Normalized steels
Fry's etchant - Ni-Ge alloys - Chemical etching
Fry's etchant - Ni-Pd-Ga alloys - Chemical etching
Fry's etchant - Ni-Pt-Ga alloys - Chemical etching
Fry's etchant - Nimonic alloys - Nimonic alloys PE7, PE11, and PE16, Nimonic Pk 31
Fry's etchant - Stainless steels - Chemical etching
Fry's etchant - Wrought stainless steels - General structure
Fry's etchant, modified - Fe, mild steel - Dislocation etching
Fry's etchant, modified - Iron and steel specimens - Plain and alloy steel specimens
Fry’s etchant - Steels
Fuss's etchant - Wrought aluminium alloy - Chemical etching
G etchant - For Fe/Ni
G etchant - Steels for high temperatures
GE Turbo-chrome etchant - Martensitic stainless steel and high-alloy steels - Chemical etching
GE Turbo-chrome etchant - P91 (X10CrMoV91) steel - Chemical etching
GE Turbo-chrome etchant - Stainless steels - Chemical etching
Gilman's etchant - Zinc - Chemical polishing and etching
Gilman's etchant I - For Cd
Gilman's etchant II - For Zn
Giometto and Capella's etchant - Martensitic chromium steels - Chemical etching
Glyceregia (1) - Austenitic stainless steels
Glyceregia (2) - Fe + 15-30 Cr + 6-40 Ni + <5%
Glyceregia - Austenitic stainless steels - Chemical etching
Glyceregia - Cr and Cr alloys - Chemical etching
Glyceregia - Fe-Ni-Cr heat resistant casting alloys - Etchant for delineating general structure
Glyceregia - High alloy steels, austenitic Mn steels, stainless steels - Chemical etching
Glyceregia - Ni superalloys and Ni-Cr alloys - Chemical etching
Glyceregia - Steel and SST vacuum system parts - Chemical cleaning
Glyceregia - Wrought stainless steels - General structure
Glyceregia etchant - Stainless steel castings - General structure
Glycol - Mg and alloys - Chemical etching
Goeren's amyl picral - Iron and steels - Chemical etching
Gorsuch's etchant - Pure iron
Graff and Sargent's etchant - 2XXX, 3XXX, 6XXX, 7XXX Al alloys - Chemical etching
Grard's No. 1 etchant - Cu alloys
Gray cast irons - Color etchant
Green's contrast etchant - Fe + 15-30 Cr + 6-40 Ni + <5%
Griffis and Spretnak's etchant - For iron and steels - General macrostructure
Groesbeck etchant - Alloys with Cr and or Co
Groesbeck's etchant - High alloy steels and castings - Chemical etching
Groesbeck's etchant - High-alloy steels, cast steels
Groesbeck's etchant - Iron and steels - Chemical etching
Groesbeck's etchant - Stainless steels - Chemical etching
Groesbeck's etchant - Stainless steels - Color etchant
H etchant - Ti alloys
H100 etchant - InSb (111) wafers - Chemical etching
Hall's etchant - Intergranular oxidation in 4150 steel
Hasson's etchant - For Mo
Hasson's etchant - Molybdenum, color etchant - Chemical etching
Hasson's etchant - Pure Mo
Heppenstall's etchant - Ni-based superalloys - General macrostructure
Heppenstall's etchant - Inconel 625 alloy - Chemical etching
Heppenstall' etchant - Nickel superalloys
Heyn's etchant - For iron and steels - General macrostructure
Heyn's etchant - Iron, steel specimens, cast irons - Phosphorus segregation in low carbon steel specimens
Heyn's etchant - Low-carbon steels
Heyn's etchant - Steel specimens and cast iron - To reveal phosphorus segregations
Hone and Pearson's anodizing solution - Pure Al - Chemical etching
Hone and Pearson's anodizing solution - Pure Al - Chemical etching
Hordon's etchant - Al-Cu alloy - Alloy with 7.5 at.% Al
Howarth's etchant - Carbon and alloy steels - For detection of overheating and burning
Howarth's etchant - Carbon and alloy steels with medium carbon content - Detection of overheating and burning
Howarth's etchant - Fe + <1C + <4% additions
Huber and Linh's H etchant - For etch pits on InP
Hume-Rothery's etchant - Al-Si alloys
Humfrey's etchant - For iron and steels - General macrostructure
Humphrey’s etchant - Cast steels
Hydal's etchant - For InBiSn
Hypo etchant - AgCl (100) oriented material - Chemical etching
Iodate etchant- PbTe (100) wafers - Chemical etching
Iodine A etchant - Ba2TiO3 (111) and (100) wafers, single crystals - Chemical etching
Iodine etchant - Si (111) wafers, boron doped - Chemical etching
Jacquet's etchant - Al, single crystal
Jacquet's etchant - Aluminium - Etching for etch pits
Jacquet's solution - For Al - Electrolytic polishing
Jewitt-Wise's etchant - Ni specimens - Chemical etching
Jin's etchant - For iron and steels - General macrostructure
Jodid (high-purity, iodide-process) Ti - Chemical etching - General macrostructure
Jong's color etchant - OFHC copper - Tint etching
KKI etchant - InP (100) wafers - Chemical etching
Kalling's 1 etchant - Martensitic stainless steels
Kalling's 1 etchant - Martensitic, stainless steels - Chemical etching
Kalling's 2 etchant - Ni-Cu alloys and Ni-base superalloys - Chemical etching
Kalling's 2 etchant - Stainless steel castings - General structure
Kalling's 2 etchant - Stainless steels - Chemical etching
Kalling's 2 etchant - Stainless steels - Chemical etching
Kalling's 2 etchant - Stainless steels, Ni-Cu alloys, Ni-base superalloys
Kalling's I etchant - Stainless steels - Chemical etching
Kalling's etchant - Cr stainless steels - Chemical etching
Kalling's etchant - Ho2Fe17 and Ho2Co14Fe3 specimens - Chemical etching
Kalling's etchant - Nickel specimens T.D. grade - Chemical etching
Kalling's etchant - SST 400 series - Chemical etching
Kalling's etchant - UCe2 specimen - Chemical polishing
Kalling's etchant - UCo2 specimen - Chemical polishing
Kalling's etchant - UNi2 specimen - Chemical polishing
Kalling's etchant - UPt3 specimen - Chemical polishing
Kalling's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - General structure
Kalling's etchant - Wrought heat-resistant steels
Kalling's etchant - Y2(CoM)17 single crystal ingots - Chemical polishing
Kallings 2 etchant - Ni-Cu alloys and superalloys - Chemical etching
Kallings's etchant - Wrought stainless steels - General structure
Kallings's etchant - Wrought stainless steels - General structure
Keller and Geisler's anodizing solution - Al and Al alloys - Chemical etching
Keller' etchant, modified - Ni-Cr-Th alloy - Ni-20Cr-2ThO2
Keller's etchant - Al and Al alloys - Chemical etching
Keller's etchant - Al-Cu-Ag-Mg-Ti alloy - 4.7% Cu, 0.6% Ag, 0.3% Mg, 0.3% Al, 0.2% Ti
Keller's etchant - Al-Cu-Ti alloy - Alloy with 4% Cu, and 0.1% Ti
Keller's etchant - Al-Ni system - Al-Al3Ni eutectic
Keller's etchant - Al-Si alloys - Chemical etching
Keller's etchant - Al-Zn-Mg alloy
Keller's etchant - Al-Zn-Mg alloy - Chemical etching
Keller's etchant - Al-Zn-Mg-Cu alloy - 7075 alloy 5-3% Zn, 2-7% Mg, 1.6 Cu
Keller's etchant - Al-Zn-Mg-Cu alloys (+Cr, Ti) - Chemical etching
Keller's etchant - Aluminium (99.945%) - Dislocation etching
Keller's etchant - Aluminium
Keller's etchant - Deep-etching of Al-Si - For most aluminum and aluminum alloys
Keller's etchant - Determining grain structure in A356 aluminum
Keller's etchant - RE-Al alloys - Chemical etching
Keller's etchant - Sleeve bearing materials (Pb, Al)-Pb-Sn-Cu overlay on Al-Cd alloy
Keller's etchant - Ti alloys - Chemical etching
Keller's etchant - Ti alloys - Chemical etching
Keller's etchant - Ti, Ti-Al alloys - Dislocation etching
Keller's etchant - Ti-6% Al-4% V alloy, Ti-5% Al-2.75% Cr-1.25% Fe alloy, Ti-2.55% Al-3.75% Mn alloy - General macrostructure
Keller's etchant - Ti-Al-Mn, Ti-Al-V, and Ti-Al-Cr-Fe alloys, flow lines - Chemical etching
Keller's etchant 1 - Pure Al and Al alloys, Ti alloys, RE-Al alloys
Keller's etchant 2 - For Al and Al alloys
Keller's etchant, conc. - Al-Cu-Si alloys
Keller's etchant, concentrated - and Al alloys
Keller's etchant, diluted - Aluminium 7075, 7475 alloy - Al-5.1/5.7 Zn-2.1/2.3 Mg-1.5 Cu-0.2 Cr
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Al and Al alloys - Chemical etching
Keller's etchant, modified - Aluminium alloys - Alloy 7075, recrystalliyed
Keller’s etchant - Al and Al alloys - Chemical etching
Klemm's I etchant - Alpha and beta brass - Tint etching
Klemm's I etchant - Iron and steels - Chemical etching
Klemm's I etchant - Iron and steels - Chemical etching
Klemm's I etchant - Pure Zn and low-alloy Zn - Chemical etching
Klemm's I etchant - Tint etchant for steels
Klemm's I etchant - Zn and lean alloys - Chemical etching
Klemm's I tint etchant - Brass, bronze
Klemm's II etchant - Alpha brass - Tint etching
Klemm's II etchant - Tin - Chemical etching
Klemm's II etchant - Tint etchant for steels
Klemm's II tint etchant - Steels, alpha brass, tin alloys
Klemm's III etchant - Bronze alloys - Tint etching
Klemm's III etchant - Ni alloys - Tint etching
Klemm's III tint etchant
Klemm's etchant
Klemm's etchant - Iron, steel specimens, cast irons - Phosphorus distribution in cast steel specimens and cast iron
Klemm's etchant - Temper embrittlement in steels - Chemical etching
Klemm's etchant I - Etches segregations in unalloyed and low alloy steels - Chemical etching
Klemm's etchant I - Unalloyed and low-alloy steels, cast irons, Mn steels, pure Zn and low-alloy Zn
Klemm's etchant II - Cu and Cu alloys and soft solders
Klemm's etchant II - Cu and Cu alloys with soft solders - Chemical etching
Klemm's etchant III - Pure Cu and Cu alloys
Klemm's etchant III - Pure Cu, leaded bronze, bronzes, alpha/beta brasses, Al bronze, Be bronze - Chemical etching
Kodak's EB-5 etchant - Cr thin films - Chemical etching
Kroll's etchant - For most Ti materials, especially for Ti-Al-V-(Sn) alloys - Chemical etching
Kroll's etchant - Suited especially for Al-Cu alloys - Chemical etching
Kroll's etchant - Ti alloys - Chemical etching
Kroll's etchant - Ti and alloy - Ti-6Al-2Sn-1.5Zr-1Mo-0.35Bi-0.1Si
Kroll's etchant - Ti-Al-Mo alloy - 5.8-9.7% Al, 0.5-8.2% Mo
Kroll's etchant - Ti-Al-O alloy - Ti-6-10% Al-0.04-0.12% O
Kroll's etchant - Ti-Al-V alloy (6Al-4V) - Chemical etching
Kroll's etchant - Ti-Mo alloy - Ti-26Mo
Kroll's etchant - Ti-Mo-V-Al-Fe alloy - Ti-8Mn-8V-3Al-2Fe
Kroll's etchant - Ti-Mo-Zr-Sn alloy - Ti-11Mo-6.6Zr-4.6Sn
Kroll's etchant - Ti-Ni alloys - Chemical etching
Kroll's etchant - Ti-V-Cr-Zr-Mo-Al alloy - Ti-8V-6Cr-4Zr-4Mo-3Al
Kroll's etchant - Titanium - For many Ti raw materials, especially for Ti-Al-V alloys
Kroll's etchant - Titanium and titanium alloy
Kroll's etchant - Titanium and titanium alloys - General purpose etch - For most titanium alloys
Kroll's etchant 1 - Al-Cu alloys, Ti alloys, mainly Ti-Al-V (Sn) alloys
Kroll's etchant 2 - For Ti/Al
Krumm's etchant - Al thin films evaporated on GaAs, (100) wafer substrates
LBH etchant, modified - Steels - Chemical etching
LaPera's etchant - For steels
LaPera's etchant - Low alloy dual-phase and TRIP steels - Chemical etching
LaPera's etchant - TRIP steel - Chemical etching
Lacombe and Beaujard's etchant - Al and Al alloys - Chemical etching
Landyren's etchant - Si (111) wafers and other orientations - Chemical etching
LeChatelier's No. 1 etchant - For iron and steels - General macrostructure
LeChatelier's No. 2 etchant - For iron and steels - General macrostructure
Lead print I
Lead print II
Lead print III
Lenoir's etchant - Al-Zn-Mg alloy
Lenoir's etchant, modified - Cu-Al-Mn alloy - Alloys with 3-4% Cu, 0.5 Mn
Lenoir's solution - Ag-Al alloy - Alloy with 5% Ag
Lenoir's solution - Al-Zn-Mg alloy - Alloy with 6.86 wt.% Zn, 2.5 wt.% Mg
Lenoir's solution - For Al and U
Lenoir's solution - Nimonic PE16 alloy
Lenoir's solution, modified - Ag-Al-Cd alloy - 4.8 at.% Ag, 0.15 at.% Cd
Lenoir's solution, modified - Ag-Al-Cu alloy - 4.8 at.% Ag, 0.2 at.% Cu
Lenoir's solution, modified - Al-Cu alloy - Alloys with 1-5% Cu
Lenoir's solution, modified - Al-Cu-Mg alloy - Alloys with 1-5% Cu, 0.5-1.5% Mg
Lepito's No. 1 etchant - Austenitic stainless steels, Ni-based alloys - General macrostructure
Lepito's No. I etchant - Ni alloys - General macrostructure
Lepito's No. II etchant - Ni-Cr-Fe alloys - General macrostructure
Lepito's etchant
Lepito's etchant
Lepito's etchant - Ni and its alloys - Alloys containing Cr, Fe and other elements - Etchant for nickel welds
Lepito's etchant - Stainless and high temperature ateel specimens - Austenitic stainless steel specimens and Ni base alloys
Lepito's etchant - Stainless steel
Lepito’s etchant I - Austenitic stainless steels and nickel base alloys - Chemical etching
Lepito’s etchant II - Alloys containing Cr, Fe, and other elements II - Chemical etching
Levenstein-Robinson's etchant (and (Hen-Hen) Rickson's modification) - For Ag
Levenstein-Robinson's etchant - Silver single crystal - Chemical polishing and etching
Levinstein and Robinson's etchant - Silver - Chemical polishing
Livingstone's etchant - Al-Cu alloys - Electrolytic polishing and chemical etching
Livingstone's etchant - Chemical etching
Livingstone's etchant - For Al/Cu
Livingstone's etchant, Young's etchant - Copper single crystal - Etching for etch pits
Livingstone's solution - For Ni - Electrolytic polishing
M (Medium) etchant - Silicon - Chemical etching
Malette's etchant - Iron and steels - Chemical etching
Marble's etchant - Austenitic and high-temperature-resistant steels, Co superalloys
Marble's etchant - Austenitic stainless steels - General macrostructure
Marble's etchant - Co high-temeprature alloys - Chemical etching
Marble's etchant - Co superalloys - Chemical etching
Marble's etchant - Co-Cr-Mo-Si alloy - Tribaloy 400, Tribaloy00
Marble's etchant - Co-Mo-Si alloy - 55Co-35Mo-10Si
Marble's etchant - Etchant of M-type ferrites - Chemical etching
Marble's etchant - Fe-Ni and Fe-Co magnetic alloys - Chemical etching
Marble's etchant - Fe-Ni and Fe-Co magnetic alloys - Grain size
Marble's etchant - For iron-nickel and cobalt-base superalloys
Marble's etchant - Hard facing alloys - Chemical etching
Marble's etchant - In-Ni eutectoid (30% Ni) - Chemical ecthing
Marble's etchant - Iron and steel specimens - Austenitic stainless steel specimens
Marble's etchant - Ni and its alloys - Nickel - For grain structure
Marble's etchant - Ni, Ni-Cu and Ni-Fe alloys and superalloys - Chemical etching
Marble's etchant - Ni-Cr alloys - Chemical etching
Marble's etchant - Ni-Cr-Th alloy - Etch for TD Ni-Cr
Marble's etchant - Ni-Mo-Cr-Si alloy - 50Ni-31Mo-15Cr-3Si
Marble's etchant - Nickel - Attack polishing
Marble's etchant - Nickel - General macrostructure
Marble's etchant - Nickel superalloy 718 - Chemical etching
Marble's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Marble's etchant - Stainless and high temperature Steel specimens - Austenitic stainless steel specimens and high temperature alloys
Marble's etchant - Stainless steels - Chemical etching
Marble's etchant - Stainless steels - General etchant
Marble's etchant - Wrought Fe-Ni-Cr heat resisting alloy - U-700 (AISI 687) - Good for contrast
Marble's etchant, modified - For Ni-Nb alloys
Marble's etchant, modified - Ni alloys - General macrostructure
Marble's etchant, modified - Ni and its alloys - Alloys containing Cr, Fe and other elements
Marble's etchant, modified - Stainless steels - Chemical etching
Marble’s etchant - Austenitic stainless steels and high-temperature alloys - Chemical etching
Marble’s etchant - Nickel - Chemical etching - General macrostructure
Marshall's etchant -9.999% pure iron - For etching of all grain boundaries
Marshall's etchant - Galvannealed sample - Chemical etching
Marshall's etchant - Iron and steels - Chemical etching
Marshall's solution - Fe specimens - Chemical polishing
Marts and Capes's etchant - For iron and steels - General macrostructure
Matte's dip etchant - Cu and Cu alloy parts
Methanolic Aqua Regia - Austenitic stainless steels - Chemical etching
Meyer and Eichholz's No. 1 etchant - For iron and steels - General macrostructure
Meyer and Eichholz's No. 2 etchant - For etching nitrided layer in steel
Meyer and Eichholz's No. 2 etchant - For iron and steels - General macrostructure
Meyer and Eichholz's No. 2 etchant - Nitrided DIN 1.8550(34CrAlNi7) steel specimens - Macro etching for segregation
Modification of Lacombe and Beaujard's etchant - Aluminium (HP) - Dislocation etching
Moly's etchant - Mo discs - Chemical cleaning
Moran's etchant - NaCl (100) wafers, NaCl single crystal whiskers - Chemical etching
Morris's electrolytic polishing solution - Dislocation etching
Morris's electrolytic polishing solution - Fe-3% Si alloy - Dislocation etching
Murakami's etchant - W and W alloys - Chemical etching
Murakami's etchant - Alumina (Al2O3) - Aluminia with additives
Murakami's etchant - Cast irons - 30% chromium irons
Murakami's etchant - Cast irons - High phosphorus irons
Murakami's etchant - Co-Cr-Mo-Ni-Fe-Si-C-Mn-Al-Ti alloy
Murakami's etchant - Co-Cr-Ni alloys - For identification of sigma phase
Murakami's etchant - Co-Sn0Sb alloys - For carbides
Murakami's etchant - Copper-Tungsten (Cu-W) - Electric contact material
Murakami's etchant - Cr and Cr alloys - Chemical etching
Murakami's etchant - Fe-Ni-Cr heat resistant casting alloys - Etchant for staining or film forming
Murakami's etchant - Gold-Plated Nickel-Iron (Au-Ni-Fe) - Electric contact material
Murakami's etchant - Iron - Selective carbides
Murakami's etchant - Iron and steels - Chemical etching
Murakami's etchant - Martensitic chromium steels - Chemical etching
Murakami's etchant - Mo and alloys - Chemical etching
Murakami's etchant - Mo specimens - Chemical etching
Murakami's etchant - Mo-C alloys - Chemical etching
Murakami's etchant - Mo-C alloys - Chemical etching
Murakami's etchant - Molybdenum - Chemical etching
Murakami's etchant - Molybdenum - Electric contact material
Murakami's etchant - Molybdenum-Silver (Mo-Ag) - Electric contact material
Murakami's etchant - Ni-Cu alloys and superalloys - Chemical etching
Murakami's etchant - Rhenium - Chemical etching
Murakami's etchant - Rhenium - Chemical etching
Murakami's etchant - Sb telluride - Chemical etching
Murakami's etchant - SiC alloy with 1% B4C - Chemical etching
Murakami's etchant - Silicon carbide (SiC) - For SiSiC
Murakami's etchant - Silver - Molybdenum (Ag-Mo) - Electric contact material
Murakami's etchant - Silver-Tungsten (Ag-W) - Electric contact material
Murakami's etchant - Silver-Tungsten carbide (Ag-WC) - Electric contact material
Murakami's etchant - Sn-Cd-Sb alloys - Chemical etching
Murakami's etchant - Stainless steel castings - General structure
Murakami's etchant - Stainless steel castings - General structure
Murakami's etchant - Stainless steels - Chemical etching
Murakami's etchant - Stainless steels - Color etchant
Murakami's etchant - Steels and other alloys
Murakami's etchant - Ta-Mo alloys - Chemical etching
Murakami's etchant - TiC coated steel - Chemical etching
Murakami's etchant - Tungsten - Electric contact material
Murakami's etchant - Tungsten - Mo, W and their alloys
Murakami's etchant - Tungsten-Copper (W-Cu) - Electric contact material
Murakami's etchant - Tungsten-Nickel (W-Ni) - Electric contact material
Murakami's etchant - Tungsten-rhenium-thoria system (O-Re-Th-W)-W - 3% Re-2% ThO2
Murakami's etchant - U-Zr alloys - Chemical etching
Murakami's etchant - U-Zr alloys, U-Fe-Co alloys, U-Al2-U3Si3 alloys - Chemical etching
Murakami's etchant - V and V-O alloys - Chemical etching
Murakami's etchant - Vanadium specimens - Chemical etching
Murakami's etchant - Vanadium-nitrogen system (V-N) - Electrolytic and chemical polishing
Murakami's etchant - W-Hf alloys (< 3% Hf) - Chemical etching
Murakami's etchant - W-Hf-N alloys alloy - < 3% Hf, nitrided
Murakami's etchant - W-Hf-Re alloys - Chemical etching
Murakami's etchant - W-Hf-Re-N alloys alloy - < 2% Hf, < 25% Re, nitrided
Murakami's etchant - W-Mo-Hf-Re alloy - < 20% Mo, < 2% Hf, < 30% Re
Murakami's etchant - W-Mo-Hf-Re-N alloy - < 20% Mo, < 2% Hf, < 30% Re, nitrided
Murakami's etchant - WC specimens - Chemical cleaning
Murakami's etchant - WC-Co, Eta phase appears multicolored; Co is white, WC-TiC-TaC-Co, WC-NbC-Co
Murakami's etchant - Wrought Fe-Ni-Cr heat resisting alloys - Inconel 706 and alloy 718, carbide particles
Murakami's etchant - Wrought stainless steels - General structure, sigma phase
Murakami's etchant, boiling - Aluminium nitride (AlN) - Chemical etching
Murakami's etchant, boiling - SiC-AlN specimens - SiC-10/80% AlN
Murakami's etchant, modified (Klemm) - Al-Si aloys - Chemical etching
Murakami's etchant, modified - AlN-Al2O3 - Chemical etching
Murakami's etchant, modified - Aluminium nitride (AlN) - AlN with Al2O3
Murakami's etchant, modified - Iron and steels - Chemical etching
Murakami's etchant, modified - Molybdenum - Mo, W and their alloys
Murakami's etchant, modified - Silicon carbide (SiC) - For RSiC - Reveals alpha/beta grain boundaries
Murakami's etchant, modified - Silicon carbide (SiC) - For alpha-SiC - Reveals alpha/alpha and alpha/beta grain boundaries
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Stainless steels - Chemical etching
Murakami's etchant, modified - Ti-V-Mo alloys - Chemical etching
Murakami's etchant, modified - Tungsten - Mo, W and their alloys
Murakami's etchant, modified - W and lean alloys - Chemical etching
Murakmi's etchant - Austenitic and ferritic-Austenitic stainless steels - Chemical etching
Murkami's etchant - Steel specimens - Carbide etching
Murkami's etchant - TiC specimens - Chemical cleaning
Nimonic Etch - Alloy 720Li
Nital (0.5-10%) - Yb-Zn system - Chemical etching
Nital (1%) - Co-Ce-Fe alloy - Co5CeFe02
Nital (1%) - Co-Dy-Mn alloy - Co5DyMn0.2
Nital (1%) - Co-Dy-Ni alloy - Co5DyNi0.2
Nital (1%) - Co-Dy-Pb alloy - Co5DyPb0.2
Nital (1%) - Co-Dy-Pd alloy - Co5DyPd0.2
Nital (1%) - Co-Dy-Pt alloy - Co5DyPt0.2- General microstructure
Nital (1%) - Co-Dy-Si alloy - Co5DySi0.2- General microstructure
Nital (1%) - Co-Er alloys - Chemical etching
Nital (1%) - Co-Er-Fe alloy - Co5ErFe0.2- General microstructure
Nital (1%) - Co-Fe-Y alloy - Y-Co(1-x)-Fe(x)- General microstructure
Nital (1%) - Co-Gd-Fe alloy - Co5GdFe0.2
Nital (1%) - Co-Ho system - Approx. HoCo5
Nital (1%) - Co-Ho-Fe alloy - Co5HoFe0.2
Nital (1%) - Co-La-Fe alloy - Co5LaFe0.2
Nital (1%) - Co-Lu alloy - Approx. LuCo5
Nital (1%) - Co-Nd-Fe alloy - Co5NdFe0.2
Nital (1%) - Co-Pr-Fe alloy - Co5PrFe0.2
Nital (1%) - Co-Sm-Al alloy - Co5SmAl0.2
Nital (1%) - Co-Sm-Fe alloy - Co5SmFe0.2
Nital (1%) - Co-Tb alloy - Approx. TbCo5
Nital (1%) - Co-Tb-Al alloy - Co5TbAl0.2
Nital (1%) - Co-Tb-Fe alloy - Co5TbFe0.2
Nital (1%) - Co-Tm alloy - Approx. Co5Tm
Nital (1%) - Co-Yb alloy - Aprox. YbCo5
Nital (1%) - Fe-Ni-Co alloy - Iron rich alloys
Nital (1%) - La-Cd alloys - Chemical etching
Nital (1%) - La-Ni alloys - Chemical etching
Nital (1%) - Mn-C alloys - Chemical etching
Nital (10%) - Magnesium - Chemical polishing
Nital (10%) - Nickel superalloy 718 - Electrolytic etching
Nital (10%) - Steels
Nital (2%) - Ce-Zn alloys - Chemical etching
Nital (2%) - Fe-Mo-Co alloy - Chemical etching
Nital (2%) - Mg-Li alloys - Chemical etching
Nital (2-10%) - Pr-Zn alloys - Chemical etching
Nital (3/4%) - Y-Mn alloys - Chemical etching
Nital - AISI 4340 annealed steel - Chemical etching
Nital - Carbon and alloy steels - Develops ferrite grain boundaries in low carbon steels
Nital - Carbon and alloy steels with medium carbon content - General structure (most used etchant for routine work)
Nital - Cast irons - Used to reveal macrostructure in white irons
Nital - Cd-Sc alloy - Alloy with 3% Sc
Nital - Co-Ce-Al alloy - Ce(1-x) Al (x) Co5, 0< x < 0.6
Nital - Co-Pr-Al alloy - Co5Pr(x)Al(1-x)
Nital - Dual-phase steel
Nital - Fe pure metal samples - Chemical etching
Nital - Fe-Ni (5%)-O (15%) specimens - Chemical etching
Nital - Iron and steels - Chemical etching
Nital - Iron, steels, cast irons - Most common etchant
Nital - Mg and alloys - Chemical etching
Nital - Permanent magnet materials - Rare earth (Co3Cu1.6Fe0.5Ce)
Nital - Pure Gd, RE-Co alloys, grain bounday etchant - Chemical ecthing
Nital - Pure iron, carbon steels, low-alloy steels, and gray cast irons and other alloys
Nital - Steel, carbon type - Chemical etching
Nital - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy00, general structure; grain boundaries
Nital - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy25, general structure; grain boundaries
Nital - Zn-Cd alloys - Chemical etching
Nital - Zn-Sn alloy - Zn-Sn alloys processed in a study of solidification in lamellar eutectic systems
Nital 1% - CaCO3 - Dislocation etching
Nital 1% - Co-Dy alloy - DyCo5 alloy
Nital 2% - Cast irons - Observation of ferrite grains boundaries at higher magnification
Nital etch procedures - Low alloy steels - Chemical etching
Nitrosulfuric (Wesley Austin's) etchant - Iron and steels - Chemical etching
Nitrosulfuric acid etchant - Fe and most steels
Noren's etchant - Steel weld - Chemical etching
Oberhoffer's etchant - For iron and steels - General macrostructure
Oberhoffer's etchant - For macro etching of steel specimens
Oberhoffer's etchant - Iron, steel specimens, cast irons - Blowhole segregation, primary structure, fiber orientation
Oberhoffer's etchant - Steel specimens and cast irons - Etching to reveal sgregations
Oberhoffer's etchant - Unalloyed and low-alloy steels
Osmond's etchant - Fe and most steels - General macrostructure
Oxygen sensing etchant for steels - This etchants is claimed as good for detection of oxygen penetration into steels
P etchant - SiO2 thin films deposited on (100) silicon wafers - Chemical etching
P-1 etchant - Zn (0001) wafers - Chemical etching
P-2 etchant - Zn (0001) wafers and cylinders - Chemical etching
P-3 etchant - Zn (0001) wafers and cylinders - Chemical etching
P-ED (EPW) etchant - Si (100) wafers within +/-1° of the plane - Chemical etching
P-Etchant - Chemical etching
PBr etchant - CdTe (111), (100), and (110) wafers - Chemical etching
Palmerton's etchant - Pure Zn and alloys - Chemical etching
Palmerton's etchant - Zinc specimens - Chemical etching
Palmerton's etchant - Zn alloys (with Cu) - General macrostructure
Palmerton's etchant 1 - Cu-containing Zn alloys
Palmerton's etchant 2 - Pure Zn and Zn alloys
Palmerton's etchant, modified - All Zn alloys, for pressure die-casting, Zn coatings - Chemical etching
Palmerton's etchant, modified - Zn die-casting alloys - Chemical etching
Palmerton's etchant, modified - Zn-Cu alloys - Chemical etching
Panseri's etchant - Al and Al alloys - Chemical etching
Pelleg's electrolytic polishing solution - Niobium - Dislocation etching
Phillip's anodizing solution - Pure Al and Al-Mg alloys - Chemical etching
Phoschromic etchant - Fe superalloys - Electrolytic etching
Phospho-picral etchant - Mg and alloys - Chemical etching
Picklesimer's anodizing solution - Nb and alloys - Electrolytic etching
Picklesimer's anodizing solution - Ta and alloys - Electrolytic etching
Picklesimer's anodizing solution - U alloys - Electrolytic etching
Picklesimer's anodizing solution - Zr and alloys - Electrolytic etching
Picklesimer's solution - For Zr, Nb/Sn, Nb/Ti
Picklesimer's solution - Nb-Ti alloy - Anodising
Picklesimer's solution - Nb-Ti alloys
Pickling's anodizing solution - Brass, bronze, and copper alloys - Chemical cleaning
Picral (4%) etchant - Cast irons - Used to reveal macrostructure in white irons
Picral etchant - Carbon and alloy steels - For general structure
Picral etchant - Carbon and alloy steels with medium carbon content - General structure
Picral etchant - Cast iron
Picral etchant - Cast irons - General purpose etching of all pearlitic gray, melleable and ductile cast irons
Picral etchant - Fe, single crystal iron whiskers - Dislocation etching
Picral etchant - Fe-Cr alloys - Chemical etching
Picral etchant - Iron and steels - Chemical etching
Picral etchant - Iron, steels, cast irons - Generally used for iron and heat treated steels
Picral etchant - Pure iron, carbon steels, low-alloy steels, and cast iron
Picral etchant - Steels - Chemical etching
Picral etchant - Steels, high carbon and high alloy types - Chemical etching
Picral etchant - Tin and tin alloys - For etching tin-coated steel and tin-coated cast iron
Polisar's etchant - For etch pits on CdTe, CdHgTe, HgTe
Pondo's etchant - Copper
Pondo's etchant - Cu and Cu alloys - Chemical etching
Pondo's etchant - Cu-Sn alloys - Chemical etching
Pondo's etchant - For Cu alloys
Poulton's etchant - 6005, 6063 and 6061 Al-Mg-Si alloys - Chemical and electrolytic etching
Poulton's etchant - Al alloys - General macrostructure
Poulton's etchant - Aluminium alloys - High purity Al, commercial purity Al, Al-Mn alloys, Al-Si alloys, Al-Mg alloys, Al-Mg-Si alloys
Poulton's etchant - High purity Al, commercial purity Al, Al-Mn alloys, Al-Si alloys
Precision No. 1 etchant - Ni alloys - Chemical etching
Precision No. 2 etchant - Ni alloys - Chemical etching
R etchant - For Ti/Al, Ti/Zr
R or A etchant - Ti-Zr alloys - Chemical etching
R-etchant - Ti-Al and Ti-Al-Zr alloys - Chemical etching
R.C. etchant
R.R.E. etchant - For InP, InPAs, GeInPAs
RC-1 etchant - GaAs (111) wafers - Dislocation etching
RCA etchant (AB) - SiO2 alpha-quartz frequency crystals - Chemical cleaning
RCA etchant - Si wafers of all major plane orientations - Chemical cleaning
RIE etchant - TiW thin films - Ionized gas etching
Ralph’s etchant - Stainless steel - Chemical etching
Reinhardt's etchant - Fe and most steels - General macrostructure
Remington A etchant - Ti alloys - Chemical etching
Remington B etchant - Titanium - Chemical etching
Remington's A etchant (Finlay's A etchant) - For Ti alloys
Retained austenite etchant I - Steels - Chemical etching
Retained austenite etchant II - Steels - Chemical etching
Retained austenite etchant III - Steels - Chemical etching
Retained austenite etchant IV - Steels - Chemical etching
Retained austenite in the steels V
Richard-Crocker's RC etchant - Gallium phosphide (GaP) - Chemical polishing
Richard-Crocker's etchant
Rolls Royce's etchant - Stainless steel - Chemical etching
Roman's etchant - Er, Dy, Gd, Ho, La - Chemical polishing
Roman's etchant - For R.E. alloys
Roman's etchant - Pr-Au alloy - Chemical etching
Roman's etchant - Pr-Ba alloys - Chemical etching
Roman's etchant - Pr-Bi alloys - Chemical etching
Roman's etchant - Pr-Cs alloys - Chemical etching
Roman's etchant - Pr-Hf alloys - Chemical etching
Roman's etchant - Pr-Hg alloys - Chemical etching
Roman's etchant - Pr-Ir alloy
Roman's etchant - Pr-Ir alloy - Chemical etching
Roman's etchant - Pr-Pt alloys - Chemical etching
Roman's etchant - Pr-Re alloys - Chemical etching
Roman's etchant - Pr-Ta alloys - Chemical etching
Roman's etchant - Pr-Tl alloys - Chemical etching
Roman's etchant - Pr-W alloys - Chemical etching
Romans's etchant - Praseodymium-lead alloys (Pr-Pb) - Chemical etching
Romans's etchant - Praseodymium-osmium alloys (Pr-Os) - Chemical etching
Rosenhain and Haighton's etchant - For iron and steels - General macrostructure
Rosenhain's etchant - Co-Sn alloys - Chemical etching
Rowland's etchant - Etchants for galvannealed steels
RNO etchant - For revealing secondary carbides in steel
Russell's etchant - Pb-Sb alloys - General macrostructure
Russell’s etchant - Pb and Pb alloys
Seven acid’s etchant - Alloy 945
SR4 etchant - Ge (111) wafers - Chemical polishing/etching
SR4 etchant - Si (111) wafers used in a study of the variations in surface conductivity of silicon and Germanium
SSA etchant - GaAs wafers - Electrolytic etching
Scale dip etchant - Cu and Cu alloys - Chemical cleaning
Schell's etchant
Schell's etchant - GaAs (111) wafers - Chemical etching
Schimmel's etch technique - Chemical etching
Schimmel's etchant
Schimmel's etchant - Si (111) and (100) wafers used as substrates for silicon epitaxy growth - Chemical etching
Schimmel's etchant - Silicon - Chemical etching
Schrader's etchant - For iron and steels - General macrostructure
Schrader's modification of Vilella's etchant - High alloy steels - Chemical etching
Schramm's etchant - Zn-Cu, Zn-Fe, Zn-Mg, Zn-Ni, and Zn-Pb alloys
Schumann's etchant
Schumann's etchant - Fe-Mn alloys - Chemical etching
Schumann's etchant - Mn-Ti-Fe system - Fe-19-27% Mn - up to 1.45% Ti
Scimmel's etchant - Silicon - Defects in epi layers on <100> silicon
Secco's etchant - Dislocation etching
Secco's etchant - For etch pits on Si (100)
Secco's etchant - Si (111) and (100), p-type, 1-10,000 Ohm cm resistivity wafers - Chemical etching
Seeco's etchant - SiO2 thin films grown on silicon, (100), n-type substrates - Chemical etching
Sirtl's etchant - Dislocation etching
Sirtl's etchant - For Ge
Sirtl's etchant - Si (111) wafers and other orientations - Chemical etching
Sirtl's etchant - SiC (0001) wafers - Chemical polishing
Sirtl's etchant - Silicon
Sirtl's etchant - Silicon specimens - Chemical etching
Sirtl's etchant, modified - Si (111), (110) and (211) wafers, ingots - Chemical etching
Sopori's etchant - Si (111) wafers and other orientations - Chemical etching
Stead No. 1 etchant - For iron and steels - General macrostructure
Stead's No. I etchant - For P in steel
Stead's No. I etchant - Steel specimens and cast irons - The etching solutions reveals phosphorus segregations
Stead's No. II etchant - For P in steel
Stead's No. II etchant - For iron and steels - General macrostructure
Stead's No. II etchant - Steel specimens and cast irons - To reveal phosphorus segregations and cell structures in cast iron
Stead's etchant - Iron and steel specimens - Plain and alloy steel specimens
Stead's etchant - Used to reveal the eutectic cell number in gray cast irons
Stead’s etchant - Steels
Struer's D-2 etchant - Copper and copper alloys - Electrolytic etching
Struers A2 electrolyte - Al and Al alloys - Electrolytic polishing
Struers electrolyte A2 - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A2-I - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A2-II - For Al, Fe, Ni, Ag, stainless steel, steel, Sn, Ti - Dislocation etching
Struers electrolyte A3-I - Martensitic steel, Mo, stainless steel, Ti, V, Zr - Dislocation etching
Struers electrolyte A3-II - Martensitic steel, Mo, stainless steel, Ti, V, Zr - Dislocation etching
Struers electrolyte A8-I - Cr, Hf, Ni, Ti - Dislocation etching
Struers electrolyte A8-II - Cr, Hf, Ni, Ti - Dislocation etching
Struers electrolyte AC2-I - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte AC2-II - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte AC2-III - Cast iron, Mg, Ni, stainless steel, steels - Dislocation etching
Struers electrolyte D2 - Brass, Cu, Au - Dislocation etching
Struers electrolyte E5-I - Brass, bronze, carbon steel, cast iron - Dislocation etching
Struers electrolyte E5-II - Brass, bronze, carbon steel, cast iron - Dislocation etching
Struers electrolyte E5-III - Brass, bronze, carbon steel, cast iron - Dislocation etching
Sulfide etchant of Kunkele - Iron and steels - Chemical etching
Sulphur printing - Steels
Super picral - Carbon and alloy steels with medium carbon content - General structure
Super picral - Iron and steels - Chemical etching
Super picral - Steels - Chemical etching
Superoxal etchant - Germanium - Etch pits etching
Superoxol - InP (100) Zn doped p-type wafers - Chemical polishing
Superoxol No. 2 etchant - Ge hemispheres - Chemical etching
Superoxol No. 2 etchant, dilute - Ge hemispheres - Chemical etching
Superoxol etchant - Antimonium - Dislocation etching
Superoxol etchant - For Ge - Chemical etching
Superoxol etchant - Ge (111) wafers - Chemical etching
Superoxol etchant - Ge (111) wafers lithium diffused - Chemical etching
Superoxol etchant - Ge specimens - Chemical etching
Superoxol etchant - Germanium - Dislocation etching
Superoxol etchant - InAs (111) wafers - Chemical etching
Superoxol etchant - InSb (111) wafers - Chemical etching
Superoxol etchant, modified - Germanium - Chemical etching
Superoxol etchant, varity - Ge hemispheres - Chemical etching
Taff's etchant - For Sn-Bi
Taff's etchant - Pure Sn and Sn-Bi alloys - Chemical etching
Taff's etchant - Sn-Bi alloy (12% Bi) - Chemical etching
Taub's etchant - For iron and steels - General macrostructure
Tri-iodide etchant - Au specimens and thin films - Chemical etching
Tri-iodine etchant - Au thin film deposits as a multilayer Au/Ni/Au/TiW/Si(100) substrate - Chemical etching
Tri-iodine etchant - AuGe (13%) alloy ribbon - Chemical etching
Tucker's etchant - 5052 Al alloy - Chemical etching
Tucker's etchant - Al and Al alloys
Tucker's etchant - Aluminium alloys - Commercial-purity alloys 1xxx series, Al-Mn alloys, Al-Si alloys, Al-Mg-Si alloys
Tucker's etchant - Aluminium and its alloys - For Al alloys except high Si castings
Tucker's etchant - Aluminium and its alloys - For high purity Al, 1xxx, 3xxx, 4xxx, 5xxx, 6 xxx Al alloys
Tucker's etchant - Determining grain structure in A356 aluminum
Tucker's etchant I - Pure Al, Mn-Al, Si-Al, Mg-Al, Mg-Si-Al alloys
Tucker's etchant II - For Al alloys
Tucker's etchant, dilute - Al alloys (except high Si-castings)
Tucker's etchant, modified - Al-3% Ag alloy, Al alloys
Tucker’s etchant - Al and Al alloys - Chemical etching
Tucker’s etchant - High purity A1, 1XXX, 3XXX, 4XXX, 5XXX, 6XXX alloys - Chemical etching
Uddeholm etchant - Fe and most steels - General macrostructure
V2A etchant
Vegesack's etchant - Steel specimens - To reveal lead inclusions
Velguth's etchant - X40 or No. 31 alloys - Chemical etching
Vermilyea's anodizing solution for Ta - Electrolytic etching
Vilella and Beregekoff's etchant - Pb and most Pb alloys - General macrostructure
Vilella and Beregekoff's etchant - Pb-Sn alloys
Vilella etchant - Stainless steel castings - General structure
Vilella's and Beregekoff's etchant - Pb-Sb alloys, grain boundary etchant - Chemical etching
Vilella's etchant - Al and Al alloys - Chemical etching
Vilella's etchant - Carbon and alloy steels - For contrast etching
Vilella's etchant - Carbon and alloy steels with medium carbon content - For austenite grain boundaries
Vilella's etchant - Cast irons - High chromium irons
Vilella's etchant - Cu-Pb alloys - Chemical etching
Vilella's etchant - Duplex stainless steel - Sigma phase
Vilella's etchant - Fe, most steels, stainless steels - General macrostructure
Vilella's etchant - Ferritic Cr steels, austenitic CrNi steels, austenitic cast alloys, Pd and its alloys
Vilella's etchant - High alloy steels
Vilella's etchant - High-alloy steels - General macrostructure
Vilella's etchant - In and lean alloys - Chemical etching
Vilella's etchant - In-Cd alloys - Chemical ecthing
Vilella's etchant - Indium specimens - Chemical etching
Vilella's etchant - Iron and steel specimens - Stainless and high Cr steel specimens
Vilella's etchant - Iron and steels - Chemical etching
Vilella's etchant - Iron and steels - Chemical etching
Vilella's etchant - Nickel superalloys - Production of thin foils for electron microscopy
Vilella's etchant - Pd dental alloys, Pd alloys with Al, Os, In, Sn, Fe, and Cu - Chemical etching
Vilella's etchant - Stainless steels - Chemical etching
Vilella's etchant - Stainless steels
Vilella's etchant - Steels, high carbon and alloys types - Chemical etching
Vilella's etchant - Wrought Fe-Ni-Cr heat resisting alloys - Incoloy25, general structure
Vilella's etchant - Wrought stainless steels - General structure
Vilella's etchant - Zirconium specimens - Chemical etching
Vilella's etchant, modified - N-155 alloy - Chemical etching
Vilella’s etchant - Stainless and high-Cr steels - Chemical etching - General macrostructure
Vitallium alloy - Vitallium is a pure cobalt chromium alloy free of nickel and beryllium
Vitallium alloys - Electrolytic etching
Voce's etchant - Pb-Sb alloys - General macrostructure
Vogel's etchant - Si (111) and other oriented wafers - Dislocation etching
WAg etchant - Ge (111) wafers - Chemical etching
WAg etchant - Ge hemispheres - Chemical etching
Walker's etchant
Walker's etchant - Ni alloys
Walker's etchant - Rene5 alloy
Walker's etchant - Rene5 alloy - Chemical ecthing
Walker's etchant - Rene5 alloy - Chemical etching
Wallner's etchant - Corrosion-resistant CrNi steels
Warekois etchant - ZnTe (111) wafers - Chemical etching
Warke amd McCall's etchant - For iron and steels - General macrostructure
Wassermann's etchant - For Mg-Al
Wassermann's etchant - Mg-7.5% Al-2.5% Zn alloy - Chemical etching
Wassermann's etchant - Mg-Al alloys
Waterbury's etchant
Waterbury's etchant - Silver-Cadmium (Ag-Cd) - Electric contact material
Waterbury's etchant - Silver-Cadmium (Ag-Cd) brazed to brass - Electric contact material
Waterbury's etchant - Silver-Copper (Ag-Cu) - Electric contact material
Waterbury's etchant - Silver-Graphite (Ag-C) - Electric contact material
Waterless Kallings's etchant - Nickel superalloy 718 - Chemical etching
Watertoen Arsenal's etchant - Fe and most steels - General macrostructure
Wazau's etchant - For iron and steels - General macrostructure
Weck's color etchant - Etchant/procedure to examine for overheated titanium - Chemical etching
Weck's etchant - Pure Ti and Ti alloys
Weck's etchant - Pure Ti and Ti alloys - Chemical etching
Weck's tint etch for alpha Ti - Chemical etching
Weck's tint etch for alpha Ti alloys - Chemical etching
Weck's tint etchant - Ti and alloys - Tint etching
Weck's tint etchant - Ti and alloys - Tint etching
Westinghouse W Ag etchant - Ge and Ge alloys - Chemical etching
Westinghouse silver etchant - Germanium - Dislocation etching
Westinghouse silver etchant WAG - Ge
Westinghouse's silver etchant WAG - Germanium - Etch pits etching
White cast irons - Color etchant
White's etchant - Ge (111) wafers - Chemical etching
White's etchant - Si (100) cleaved wafers - Chemical polishing
White's etchant - Si (111) wafers, n- and p-type - Chemical thinning
White's etchant - Si (111) wafers, n-type, 130 Ohm cm resistivity - Chemical sphere polishing
Whiteley's etchant - For iron and steels - General macrostructure
Whiteley's etchant - Method for coloring sulfides - Iron and steels - Chemical etching
Wiliams-Blackburn's etchant - Ti-Mo-Al-Cr alloy - Ti-4.5Al-5Mo-1.5Cr
Williams's solution - For Ti and alloys - Electrolytic polishing
Worner and Worner's etchant - Pb-Sb alloys - General macrostructure
Worner and Worner's etchant - Th
Worner and Worner's etchant - Thallium specimens - Chemical polishing
Wright's etchant - For Si stacking faults dislocations
Wright's etchant - Si (100), (111), p- and n-type, 0.2-20 Ohm cm resistivity wafers - Dislocation etching
Wright-Jenkins etchant - Dislocation etching
Young's etchant - For etch pits on Al
ZIP's etchant - Inconel 617 - Chemical etching
Zeerleder's etchant - Al-Cu-Mg-Ni alloys