BaTiO3 - Dislocation etching

Material Name: BaTiO3
Recipe No.: 10122
Primary Chemical Element in Material: Ba
Sample Type: Bulk
Uses: Etching
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Dislocation etching
Etchant (Electrolyte) Composition: 4% HNO3, 2% HF (in distilled water).
Note: No data
Procedure (Condition):  Etch 10-40 s. Rothwell.
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 714.