Molybdenum - Dislocation etching

Material Name: Molybdenum
Recipe No.: 10210
Primary Chemical Element in Material: Mo
Sample Type: Bulk
Uses: Etching
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Dislocation etching
Etchant (Electrolyte) Composition: 100 ml methanol, 20 ml H2SO4.
Note: No data
Procedure (Condition):  Etch at less than 5 V dc and up to 100 mA/cm2. Pink.
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 724.