Cerium - Chemical etching

Material Name: Cerium
Recipe No.: 10950
Primary Chemical Element in Material: Ce
Sample Type: Bulk
Uses: General microstructure
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 10 ml HNO3, 100 ml methanol.
Procedure (Condition): Do not store.
Note: Rare earth metals and alloys. Etter and Selle.
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 679.