Ag-Th alloys - Chemical etching

Material Name: Ag-Th alloys
Recipe No.: 11016
Primary Chemical Element in Material: Ag
Sample Type: Bulk
Uses: General microstructure
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 2 g K2Cr2O7, 8 ml H2SO4, 100 ml distilled water.
Procedure (Condition): No data
Note: No data
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 685.