TiC coated steel - Structure of titanium carbide layer

Material Name: TiC coated steel
Recipe No.: 595
Primary Chemical Element in Material: Ti
Sample Type: Bulk
Uses: Structure of titanium carbide layer
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Chemical
Etchant (Electrolyte) Composition: 50% glycerine, 25% HF, 25% HNO3.
Procedure (Condition): Up to 30 min.
Note: Structure of titanium carbide layer.
Reference: Practical Metallography, Vol. 4, No. 10, 1967, p. 527.