Electroless nickel 2 plating

Material Name: Electroless nickel 2 plating
Recipe No.: 9687
Primary Chemical Element in Material: Ni
Sample Type: Bulk
Uses: Plating
Etchant Name: None
Type (Macro/Micro): Macro
Etching Method: Plating
Etchant (Electrolyte) Composition: Formula 2: 37.3 g nickelous sulfate, 26.4 g sodium hypophosphite, 15.9 g sodium acetate, 5-6 drops sulfuric acid, 1000 ml H2O.
Procedure (Condition): Use at 180-190 F, plating rate, 0.01 mm/h
Note: No data
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, pp. 538-539.