Zirconium - Attack polishing

Material Name: Zirconium
Recipe No.: 9775
Primary Chemical Element in Material: Zr
Sample Type: Bulk
Uses: Polishing
Etchant Name: None
Type (Macro/Micro): Micro
Etching Method: Attack polishing
Etchant (Electrolyte) Composition: 1% HF, 0.5% HNO3 in distilled water.
Procedure (Condition): No data
Note: Roth
Reference: Vander Voort, Metallography Principles and Practice, McGraw-Hill, Inc., 1984, p. 550.