Tantalum Sulfide - TaS2
Classification: Sulfide
Atomic numbers: 73 & 16
Atomic weight: 400
Melting point (C): 1300 del.
Boiling point (C):
Density (g/cm3):
Refractive index (n=):
Hardness (Mosh-scratch): 4-5
Crystal structure: Isometric-normal: (100) cube
Color (solid): Grey black