Material | Knoop Hardness |
Talc | 20 |
Silver | 20 |
Copper | 163 |
Aluminium | 80-250 |
Annealed Steel | 200 |
Martensite | 500-800 |
Glass | 530 |
Carburized Steel | 730 |
Chromium Plating | 740 |
Quarz (Silicon Dioxide) | 820 |
White Cast Iron | 840 |
Nitrided Steel | 970 |
Cementite (Iron Carbide) | 1025 |
Zirconia | 1160 |
Zirconium Boride | 1550 |
Chromium Carbide | 1735 |
Molybdenum Carbide | 1800 |
Titanium Carbide | 1800 |
Tungsten Carbide | 1880 |
Tantalum Carbide | 2000 |
Alumina | 2100 |
Zirconium Carbide | 2100 |
Beryllium Carbide | 2410 |
Titanium Carbide | 2470 |
Silicon Carbide | 2480 |
Aluminium Boride | 2500 |
Vanadium Carbide | 2660 |
Boron Carbide | 2750 |
Titanium Diboride | 4400 |
Diamond | 7000 |