K
ISCC
.
Abbreviation for the critical value of the plane strain stress-intensity factor that will produce crack propagation by stress-corrosion cracking of a given material in a given environment. Knife-line attack.
Intergranular corrosion of an alloy, usually stabilized stainless steel, along a line adjoining or in contact with a weld after heating into the sensitization temperature range.

Kraft process.
A wood-pulping process in which sodium sulfate is used in the caustic soda pulp-digestion liquor. Also called kraft pulping or sulfate pulping.