Carbides in Carbon Steels

Carbides in 0.17C-1.6Mn-0.52Si-0.083Cr steel
Carbides in 1.4110 stee
Carbides in 100Cr6 steel
Carbides in 12Cr and 8Cr steels
Carbides in AISI 1045, 5150 and 52100 steels
Carbides in C45 carbon steel
Carbides in DC01EK and DC04EK low alloyed carbon steels
Carbides in DC01EK and DC04EK low carbon steels
Carbides in SAE 8620 steel
Carbides in UHCS-10Al-1.5C steel
Carbides in X70, X80 and Grade 100 steels
Carbides in carbon, chromium and high speed steel recoreded by AFM
Carbides in hot bands in low carbon steel
Carbides in hot work tool steels
Cementite (Fe3C) in C130W2 steel
Cementite (Fe3C) in carbon steel
Cementite in Fe –0.16% C –1.26% Mn–0.22% Si–0.15% Cr steel
Cementite in 0.17C-0.74Mn steel
Cementite in 0.30% C carbon steel
Cementite in 0.37C-0.22Si-0.80Mn-0.12Cr-0.27Mo steel
Cementite in 09G2S steel
Cementite in 1.2 wt% C steel
Cementite in C45 steel
Cementite in DP-980 steel
Cementite in Fe –0.11% C –0.85% Mn–0.21% S steel
Cementite in Fe-1% C
Cementite in Fe-1% C steel
Cementite in Fe-13Mn-0.8C steel
Cementite in JIS-SCM440 steel
Cementite in S10C low carbon steel
Cementite in XC50 steel
Cementite in eutectoid steel
Cementite in eutectoid steel
Cementite in eutectoid steel
Cementite in high carbon steel
Cementite in hyper-eutectoid steel
Cementite in hyper-eutectoid steel
Cementite in low-carbon steel
Cementite in spheroidize annealed W1 tool steel
Cementite particles in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Cementite particles in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Cementite particles in AISI 1045 steel
Cementite particles in AISI 4340 and Fe-0.3C-4.08Cr steels
Cementite particles in AISI 4340 steel
Cementite particles in SAE 52100 steel
Cementite phases in carbon steel
Cementite precipitation in quench-aged iron
Chi carbides in austenite
Chromium carbides in 3% chromium steel for rolls
Coarse intergranular and intragranular proeutectoid cementite in Fe – 1.4% C binary alloy
Coarse intergranular proeutectoid cementite in a hot-rolled Fe –1.2% C binary alloy
Cr23C6 and Cr3C2 carbides in low carbon steel
Cr23C6 and Cr3C2 carbides in low carbon steel
Cr23C6, VC, Fe3C, Mo2C, Nb4C3 carbides in R7, R47, R102A, R147, R191, R192 and R206N steels
Cr3C2, Cr23C6 and Cr19Fe4C6 carbides in 0.022C-0.15Mn-0.78Cr steel
Epsilon and M3C carbides in 35MnCrMoV8-6-4-1 steel
Epsilon and cementite phases in carbon steel
Epsilon carbides in Fe–0.8C steels
Epsilon carbides in austenite
Epsilon-carbide (Fe2C) in unalloyed steel
Eta carbides in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Fe3C and NbC carbides in 0.14C-1.48Mn-0.78Si-0.052Nb steel
Fe3C carbides in 0.33C-1.12Mn-0.24Ni-0.11Cr steel
Fe3C carbides in Fe–0.17C steel
Fe3C carbides in Fe–0.8C steel
Fe3C carbides in Fe–0.8C steel
Fe3C carbides in S55C, SUP9, SUP7, SUP12 steels
Fe3C carbides in bainite steel
Fe3C carbides in carbon steel
Fe3C carbides in low carbon steel with Cu
Fe3C carbides in unalloyed tool steels
Fine transition carbides in medium carbon steel
Influence of the normalizing temperature upon the grain size and microstructure of 1040 carbon steel
Intergranular carbide network in Fe –1.31% C –0.35% Mn–0.25% Si steel
Intergranular cementite film in hypereutectoid steel
Intergranular cementite films in Fe-1.31% C–0.35% Mn–0.25% Si steel
Intergranular cementite grain boundary networks in Fe –1.31% C –0.35% Mn–0.25% Si steel
Intergranular proeutectoid cementite in Fe – 1.0% C binary alloy
Iron carbides in Fe-Mn-C alloy
Iron carbides in low-carbon steel
Iron carbides in open hearth mild steel
Iron carbides in steel with niobium addition
Kappa carbides in Fe-C-Mn-Al steel with high silicon
M23C6 carbides in Fe–12Cr–0.2C steel
M23C6 carbides in P91 creep resistant steel
M2C, MC carbides in M42 high speed steel
M3C and epsilon carbides in 1.22C-1.93Mn-1.52Cr-0.36Mo steel
M3C carbides in low alloyed carbon steel
M3C, M7C3 and M23C6 carbides in X20CrMoV12-1 creep resistant steel
M7C3 and M23C6 carbides in 0.5C-25Cr-24.5Ni-1.8W-1.9Si-1.9Mn alloy
M7C3 carbides in AISI 440C martensitic stainless steel
M7C3 carbides in Fe-2C-12Cr tool steel
M7C3, MC and M2C carbides in hardfacing steel
MC carbides in 0.17C-1.37Mn-0.24Cr-0.48Mo steel
Microstructures in a eutectoid steels
Mo2C carbides in Fe–4Mo–0.2C steel
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC carbides in steel with Nb addition
NbC, TiC, V4C3, ZrC, Mo2C, Fe3C, M7C3, M6C, M23C6 carbides in carbon steel and stainless steel
Nucleation of a cleavage crack at a carbide particle in a low-carbon steel
Precipitates in low carbon steel
Proeutectoid cementite in Fe-1% C steel
Proeutectoid cementite in hot rolled Fe-1% C steel
Retained austenite in steel 1.7262
Silicon-manganese nitrides ((Si,Mn)N2) in unalloyed steel
TiC carbides in 0.42C–0.30Ti steel
Undissolved carbides in 0.062C-1.56Mn-0.36Cr low carbon steel
VC carbides in medium carbon steel with higher V
VC carbides in vanadium steel

Copyright © 2024 by Steel Data. All Rights Reserved.