Carbides in Hot Work Tool Steels

(Cr,Fe)23C6 carbides in AISI H13 hot work tool steel
Carbide microstructures in cold work tool steels
Carbide network on the grains in 1.2344 steel
Carbides distribution in cold work tool steels
Carbides in 1.2344 steel
Carbides in 4Cr5MoSiV1 steel
Carbides in AISI 2367 steel
Carbides in AISI H13 steel
Carbides in Vanadis 23 and AISI M3;2 PM steels
Carbides in Vanadis PM steel
Carbides in heat affected zone of tool (HAZ) (1.2379 and 1.4718 steels)
Carbides in hot work tool steel
Carbides in hot work tool steels
Carbides in spray-formed AISI M32 high-speed steel
Carbides in steel 1.2344
Carbides in steel 1.2345
Carbides in steel 1.2581
Carbides in steel 1.2606
Carbides in steel 1.2714
Carbides in steel 1.2885
Chromium carbides in high speed tool steel
Cr and Mo concentration profiles in 1.2344 steel
Epsilon, M3C, M2C carbides in 30CrMoNiV10-25-6-2 steel
Epsilon, M3C, MC and M2C carbides in 0.30C-2.50Cr-2.60Mo-1.59Ni-0.18V hot work tool steel
Epsilon, M3C, MC and M2C carbides in 30CrMoNiV10-25-6-2 hot work tool steel
Fe3C and V4C3 carbides in 60CrV7 steel
Fe3C, M23(C,B)6 carbides in microalloyed constructional steels
M(C,N), M2C, M6C carbides in AISI M2 steel
M23(C,B)6 carbides in microalloyed constructional steel
M23C6 carbides in X11CrMoWVNb9-1 (T/P911) steel
M23C6 carbides in X11CrMoWVNb9-1 (T/P911) steel
M2C and M3C carbides in the cryogenic quenching of AISI A2 steel
M2C and M6C carbides in M42 steel
M2C, M3C and M7C3 carbides in Caldie hot work tool steel
M3C, M7C3 and M4C3 carbides in X40CrMoV5-1 steel
M7C3 carbides in AISI D2 steel (bar diameters of 25.4, 70 and 210 mm)
M7C3, M8C7, M23C6 carbides in 4Cr5MoSiV1 steel
M7C3, MC, M23C6 and M3C carbides in AISI H11 steel
MC (or M4C3), M23C6 and M6C carbides in AISI M2 steel
MC and M6C carbides in HS 6-5-3 steel
MC and M6C carbides in PM Sinter 23 tool steel
MC and M6C carbides in SINTER 23 PM steel
MC and M7C3 carbides in tool steels made by spray forming
MC, M23C6 carbides in hot work tool steel
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C, M7C3 carbides in Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C cast steel
MC, M6C and M23C6 carbides in H13 hot work tool steel
MC, M6C and M23C6 carbides in AISI H13 hot work tool steel
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M7C3 and M6C carbides in THG2000, MCG2006 and QRO90 steels
MC, M7C3 carbides in ROLTEC,TOUGHTEC, WEARTEC, AISI A2, D2 and D6 steels
Mo2C carbides in AISI H13 steel
Mo2C carbides in AISI H13 steel implanted with molybdenum ions
NbC in cast irons
Network of eutectic carbides in alloyed white cast iron
Precipitates in 1.6368 steel
Precipitates in X2NiCoMo13-15-10 steel
Primary and secondary carbides in 1.2344 steel
Primary and secondary carbides in the HAZ of 1.2379-1.4718 steels
Primary carbide particles of MC type in H11 steel
Retained austenite in steel 1.2581
Segregations in hot work tool steel
Some properties of metallic hard materials
Spheroidized pearlite, Ti(C,N) and carbides in 1.2344 steel
VC, M23C6 and M7C3 carbides in Dievar hot work tool steel
VC, Mo2C, (Fe,Cr)3C and (Cr,Fe)7C3 carbides in a new hot work tool steel
Vanadium carbides in H13 steel

Copyright © 2024 by Steel Data. All Rights Reserved.