EDS Microanalysis of Carbides in Steels

(Cr, Fe)23C6 carbides in Cr25 cast steel
(Cr,Fe)23C6 and VX carbides in X20CrMoV12-1 steel
(Cr,Fe)23C6 carbides in 1.4510 steel
(Cr,Mn)C carbides in TRIP steel
(Cr15.58Fe7.42)23C6 and V8C7 carbides in PM AISI M2 steel
(Fe,Cr)3C and (Cr,Fe)7C3 carbides in air-hardening cast tool steel
(Fe,Cr)3C and (Fe,Cr)7C3 carbides in Cr-Mo-Mn-Cair-hardening cast tool steel
(Fe,Cr)7C3 carbides in ferritic stainless steel
(Fe2Cr)C, M23C6 and M7C3 carbides in X20CrMoV121 steel
(Ti,Mo)C, M23C6 carbides in AIM1 steel
C2C, Cr3C2, Cr7C2, Cr7C3 and Cr23C6 carbides in AISI 446 steel
Carbide precipitate in austenitic stainless steel
Carbides in 0.04C–1.5Mn–0.2Mo in ferritic steel steels
Carbides in 1.2379 steel
Carbides in 2.25Cr-1Mo steel
Carbides in 2.25Cr-1Mo weld/mild steel interface
Carbides in 4Cr5MoSiV1 steel
Carbides in AISI M42 steel
Carbides in AISI P91 steel
Carbides in Damascus steel
Carbides in Fe-30.8Ni-26.6Cr alloy
Carbides in Fe-5Cr-5W-5Mo-V-C cast high speed steel
Carbides in HP40 steel
Carbides in Rp5 high speed steel
Carbides in Strrmhard austenitic manganese steel
Carbides in X155CrVMo121 steel
Carbides in X70, X80 and Grade 100 steels
Carbides in heat affected zone of tool (HAZ) (1.2379 and 1.4718 steels)
Carbides in semi-high-speed steel (HSS)
Carbides in the S 390 PM and S 690 PM steels I
Carbides in the S 390 PM and S 690 PM steels II
Carbides in the S 390 PM and S 690 PM steels III
Carbides in the white layer of AISI 52100 steel
Cementite in martensitic steel
Cementite particles in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Cementite particles in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Chi carbides in 316L-type austenitic stainless steel
Chromium carbides in 3% chromium steel for rolls
Chromium carbides in CB2A creep resistant steel
Cr23C6 and Cr3C2 carbides in low carbon steel
Cr23C6 carbides in ferritic stainless steel
Cr2C, Cr3C2, Cr23C6 and Cr7C3 carbides in AISI 446 steel
Cr3C2 carbides in 75Cr3C2-25NiCr coating on P91 steel substrate
Cr3C2, Cr23C6 and Cr19Fe4C6 carbides in 0.022C-0.15Mn-0.78Cr steel
Cr3C6 and NbC carbides in 12% Cr ferritic steel
Detection of boron nitrides in creep resistant steels (CB2A, CB2 and NPM1)
Electrochemical extraction of microalloy carbides in Nb-steel(SAE 8620)
Eta carbides in 1.23C-0.64Cr-0.34Mn-0.22Si steel
Eta phase in 20Cr-25Ni steel
Fe2MoC carbides in grade P11 SA335 steel
Fe3C and NbC carbides in 3.4C–0.9Si–0.7Mn–4.4Ni–1.8Cr–0.4Mo cast steel roll
Fe3C and V4C3 carbides in 0.10C-1.99Mn-0.56V steel
Fe3C and V4C3 carbides in martensitic steel
Fe3C carbides in 0.6C-10.8Mn-1.44Cr steel
Fe3C carbides in Fe-0.85Mo-2Ni-0.6C PM steel
Fe3C carbides in line pipe steel
Fe3C, Fe7C3, (Fe,Cr)7C3 carbides in AISI O1 and D2 steels
Fe3Nb3C carbides in 19Cr–0.8Nb ferritic stainless steel
Fe3Nb3C carbides in C-Cr-Nb-Ti steel
G-phase in 20Cr-25Ni steel
High-carbon carbides in 20Cr-25Ni steel
Intragranular sub-micron precipitates in 20Cr-25Ni steel
Kappa carbides in Fe-C-Mn-Al steel with high silicon
Laves phase in AISI 441 steel II
Laves phase in AISI 441 steel III
Laves phase in heat resistant steel
Laves phase in heat resistant steel
Low voltage EDS for identification of sub-micron precipitates in 20Cr-25Ni steel
M(C,N), M2C, M6C carbides in AISI M2 steel
M23(CB)6, MX, M6C carbides in T11 and C9 creep resistant steels
M23C6 and M2X carbides in 9Cr-1Mo steel
M23C6 and M3C carbides in 12% chromium steel
M23C6 and TaC carbides in TAC1 creep resisting steel
M23C6 carbides in 0.1C-9Cr-2W-0.2V-0.04N steel
M23C6 carbides in 10Cr creep resistant steel
M23C6 carbides in 11Cr-3.45W steel
M23C6 carbides in 12Cr–2W–Cu–V–Nb creep resistant steel
M23C6 carbides in 15Cr–3W ferritic steel
M23C6 carbides in 20Cr-25Ni steel
M23C6 carbides in ASTM A213–T91 steel
M23C6 carbides in CD3MN cast duplex stainless steel
M23C6 carbides in DT4 series steels
M23C6 carbides in E911 creep resisting steel
M23C6 carbides in E911 steel
M23C6 carbides in Fe-30.8 Ni-26.6 Cr steel
M23C6 carbides in NF709 and NF709R steels
M23C6 carbides in NF709 and NF709R steels
M23C6 carbides in P91 steel
M23C6 carbides in P91 steel
M23C6 carbides in P92 and P91 creep resistant steels
M23C6 carbides in P92 creep resistants steel
M23C6 carbides in P92 steel
M23C6 carbides in Sanicro 25 steel
M23C6 carbides in X10CrMoVNb9-1 creep resisting steel
M23C6 carbides in X22, P91, P92 creep resistant steels
M23C6 carbides in grade 91 steel I
M23C6 carbides in grade 91 steel II
M23C6 carbides in high chromium ferritic steel
M23C6 carbides in welded P91 creep resistang steel
M23C6, M2C and M6C carbides in low alloy Cr-Mo-Ni-V steel
M23C6, M6C and M2C carbides in Cr-Mo-Ni-V steel for turbine rotor
M23C6, M6C and MC carbides in AISI H13 steel
M23C6, NbC and M7C3 carbides in steels for nuclear industry
M23C6, V8C7, MC and M2C carbides in spray formed AISI M2 steel
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M2C and M3C carbides in the cryogenic quenching of AISI A2 steel
M2C and M7C3 carbides in high-chromium white iron
M2C, M6C and M7C3 carbides in Fe3Al alloy
M2C, M6C carbides in AISI M2 steel
M2C, M6C, M7C3 carbides in Fe3Al-based alloy
M2C, M6C, TiC, VC and NbC carbides in AISI M7 cast high speed steel
M2C, M7C3, M23C6 and M6C carbides in 2.25Cr-1Mo steel
M2C, MC and M6C carbides in AISI M2 high speed steel
M3C and M7C3 carbides in 0.1C-0.9Cr-V steels
M3C, M6C, M7C3, M23C6 carbides in 2.25Cr-1.5W steel
M3C, M7C3 and M23C6 carbides in X150CrMoV12-1 steel
M6C and M7C3 carbides in Cr and semi HSS steels for rolls
M6C, VC, (CrFeMoW)7C3 and M23C6 carbides in high speed steels
M7C3 and M23C6 carbides in MANET steel
M7C3 and M23C6 carbides in Manet steel
M7C3 and M23C6 carbides in Stellites 6 and 21
M7C3 and M6C carbides in high Cr and semi high speed steels
M7C3 and M6C5 carbides in white cast Fe-Cr-C-V alloy
M7C3 carbides in 1.2379 steel
M7C3 carbides in PM Vanadis 6 steel
M7C3 carbides in SKD11 steel
M7C3 carbides in X210CrW12 steel
M7C3 carbides in high-chromium white cast iron
M7C3, (Fe,Cr)23C6 and Mo2C carbides in high alloyed chromium cast iron
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 carbides in AISI 440A steel
M7C3, M8C7, M23C6 carbides in 4Cr5MoSiV1 steel
M7C3, MC and M2C carbides in hardfacing steel
M7C3, MC, M23C6 and M3C carbides in AISI H11 steel
MC (or M4C3), M23C6 and M6C carbides in AISI M2 steel
MC and M3C carbides in cast AISI D3 steel
MC and M6C carbides in AISI M2 high speed steel
MC and M6C carbides in PM Sinter 23 tool steel
MC and M6C carbides in cast M2 high speed steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC, M2C and M6C carbides in K390 steel
MC, M2C and M6C carbides in AISI M2 high speed steel manufactured by different casting technologies
MC, M2C and M6C carbides in semi high speed steel for rolls
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel II
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M3C and M7C3 carbides in high chromium cast iron
MC, M3C, M6C and M7C3 carbides in SS2541, THG2000, QRO90 and MCG 4M steels
MC, M6C and M23C6 carbides in H13 hot work tool steel
MC, M6C and M23C6 carbides in AISI H13 hot work tool steel
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M7C3 and M2C carbides in cast high speed steel roll
MX and M23C6 carbides in 100Cr creep resistant steel
MX, M3C and M7C3 phases in Cr-V low-alloyed steel
Mo2C and (Fe,Cr)7C3 carbides in high Cr white cast iron Fe-21Cr-3Ni-1.7Mo-2.4C
Mo2C and Ksi carbides in SA508 Gr3 nuclear reactor steel
Mo2C carbides in JAC590R steel
Mo2C, (V,Ti)C, (Fe,Mo)6C, Fe7C3, Fe3C carbides in austempered ductile iron (ADI)
Nanoscale precipitates in 13% Cr martensitic stainless steel
Nb and V carbides in 12Cr-2.5Ni-2Mo-0.2V-0.08Nb-N creep resistant steel
NbC and Cr23C6 carbides in high Cr (11 wt.%) tempered martensitic steel
NbC carbides in HSLA steel
NbC carbides in microalloyed Nb-Mo steel
NbC in cast irons
NbC, M23(B,C)6 and M2,3C carbides in hardfacing alloys
Precipitates in 9% Cr steel with Co
Precipitates in SAE 8620 steel
Precipitates in heat resistant steel
Precipitates in micro alloyed steel
Precipitates in solution annealed 20Cr-25Ni steel
Residual phase sub-micron particles in 20Cr-25Ni steel
Retained austenite in AISI D2 steel
Sigma phase and carbides heat resistant steel
TiC carbides in 440C–TiC composite steel
TiC carbides in 0.42C–0.30Ti steel
TiC carbides in TiNb and IF steels
V4C3, F2.4C and Fe3C carbides in high strength spring steel
V6C5 carbides in Fe-C-V microalloyed steel
VC and M3C carbides in JIS SKS3 and BSBO1 steels
VC and W3Fe3C carbides in HSS6-5-2C high speed steel
VC carbides in cast high speed steel

Copyright © 2024 by Steel Data. All Rights Reserved.