Carbides in Cold Work Tool Steels

(Cr) 23C6, V4C3 carbides in X190 CrVMo 20-4 steel - Annealed condition
(Cr) 7C3, V4C3 carbides in X190 CrVMo 20-4 steel - Quenched from 1200 C/5 min
(Cr,Fe)7C3 carbides in K110, PM steel K390 steels
(Cr,Fe)7C3 carbides in X180CrMo12-1 steel
(Fe,Cr)7C3 carbides in 5% chrome steel
Carbide microstructure in PM tool steel
Carbide microstructures in cold work tool steels
Carbide network in 1.2362 steel
Carbide network in 1.2379 steel
Carbides distribution in cold work tool steels
Carbides in 0.17C-1.6Mn-0.52Si-0.083Cr steel
Carbides in 0.79C-0.84Si-4.96Cr-0.31Mo steel
Carbides in 1.06C-7.37Cr-2.29V-1.43Mo steel
Carbides in 1.07C-1.21Si-8.02Cr-2.63V-1.14W-1.53Mo steel
Carbides in 1.0C-10.0Cr-90.25V steel, overheated microstructure
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1000 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1000 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1020 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1020 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1040 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1040 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1060 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1060 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1080 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1080 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1120 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1120 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1160 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1160 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1200 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1200 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1240 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 1240 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 900 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 900 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 940 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 940 C/oil
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 980 C/air
Carbides in 1.0C-10.0Cr-90.25V steel, quenched from 980 C/oil
Carbides in 1.10C-1.0Si-7.90Cr-2.20V-1.15W-1.45Mo steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel
Carbides in 1.2080 steel, quenched from 1000 C/air
Carbides in 1.2080 steel, quenched from 1000 C/oil
Carbides in 1.2080 steel, quenched from 1020 C/air
Carbides in 1.2080 steel, quenched from 1020 C/oil
Carbides in 1.2080 steel, quenched from 1040 C/air
Carbides in 1.2080 steel, quenched from 1040 C/oil
Carbides in 1.2080 steel, quenched from 1060 C/air
Carbides in 1.2080 steel, quenched from 1060 C/oil
Carbides in 1.2080 steel, quenched from 1080 C/air
Carbides in 1.2080 steel, quenched from 1080 C/oil
Carbides in 1.2080 steel, quenched from 1120 C/air
Carbides in 1.2080 steel, quenched from 1120 C/oil
Carbides in 1.2080 steel, quenched from 1160 C/air
Carbides in 1.2080 steel, quenched from 1160 C/oil
Carbides in 1.2080 steel, quenched from 1200 C/air
Carbides in 1.2080 steel, quenched from 1200 C/oil
Carbides in 1.2080 steel, quenched from 1240 C/oil
Carbides in 1.2080 steel, quenched from 1240 C/oil
Carbides in 1.2080 steel, quenched from 900 C/air
Carbides in 1.2080 steel, quenched from 900 C/oil.
Carbides in 1.2080 steel, quenched from 940 C/air
Carbides in 1.2080 steel, quenched from 940 C/oil
Carbides in 1.2080 steel, quenched from 980 C/air
Carbides in 1.2080 steel, quenched from 980 C/oil
Carbides in 1.2369 steel
Carbides in 1.2379 and Universal steels
Carbides in 1.2379 steel
Carbides in 1.2379 steel
Carbides in 1.2379 steel
Carbides in 1.2379 steel
Carbides in 1.2379 steel, quenched and tempered
Carbides in 1.2379 steel, quenched from 1000 C/air
Carbides in 1.2379 steel, quenched from 1000 C/oil
Carbides in 1.2379 steel, quenched from 1000 C/oil
Carbides in 1.2379 steel, quenched from 1020 C/air
Carbides in 1.2379 steel, quenched from 1020 C/oil
Carbides in 1.2379 steel, quenched from 1020 C/oil
Carbides in 1.2379 steel, quenched from 1040 C/air
Carbides in 1.2379 steel, quenched from 1040 C/oil
Carbides in 1.2379 steel, quenched from 1040 C/oil
Carbides in 1.2379 steel, quenched from 1060 C/air
Carbides in 1.2379 steel, quenched from 1060 C/oil
Carbides in 1.2379 steel, quenched from 1060 C/oil
Carbides in 1.2379 steel, quenched from 1080 C/air
Carbides in 1.2379 steel, quenched from 1080 C/oil
Carbides in 1.2379 steel, quenched from 1080 C/oil
Carbides in 1.2379 steel, quenched from 1120 C/air
Carbides in 1.2379 steel, quenched from 1120 C/oil
Carbides in 1.2379 steel, quenched from 1120 C/oil
Carbides in 1.2379 steel, quenched from 1160 C/air
Carbides in 1.2379 steel, quenched from 1160 C/oil
Carbides in 1.2379 steel, quenched from 1200 C/air
Carbides in 1.2379 steel, quenched from 1200 C/oil
Carbides in 1.2379 steel, quenched from 1240 C/air
Carbides in 1.2379 steel, quenched from 1240 C/oil
Carbides in 1.2379 steel, quenched from 900 C/air
Carbides in 1.2379 steel, quenched from 900 C/oil
Carbides in 1.2379 steel, quenched from 940 C/air
Carbides in 1.2379 steel, quenched from 940 C/oil
Carbides in 1.2379 steel, quenched from 980 C/air
Carbides in 1.2379 steel, quenched from 980 C/oil
Carbides in 1.2379 steel, quenched from 980 C/oil
Carbides in 1.2436 steel, quenched from 1000 C/air
Carbides in 1.2436 steel, quenched from 1000 C/oil
Carbides in 1.2436 steel, quenched from 1020 C/air
Carbides in 1.2436 steel, quenched from 1020 C/oil
Carbides in 1.2436 steel, quenched from 1040 C/air
Carbides in 1.2436 steel, quenched from 1040 C/oil
Carbides in 1.2436 steel, quenched from 1060 C/air
Carbides in 1.2436 steel, quenched from 1060 C/oil
Carbides in 1.2436 steel, quenched from 1080 C/air
Carbides in 1.2436 steel, quenched from 1080 C/oil
Carbides in 1.2436 steel, quenched from 1120 C/air
Carbides in 1.2436 steel, quenched from 1120 C/oil
Carbides in 1.2436 steel, quenched from 1160 C/air
Carbides in 1.2436 steel, quenched from 1160 C/oil
Carbides in 1.2436 steel, quenched from 1200 C/air
Carbides in 1.2436 steel, quenched from 1200 C/oil
Carbides in 1.2436 steel, quenched from 1240 C/air
Carbides in 1.2436 steel, quenched from 1240 C/oil
Carbides in 1.2436 steel, quenched from 900 C/air
Carbides in 1.2436 steel, quenched from 900 C/oil
Carbides in 1.2436 steel, quenched from 940 C/air
Carbides in 1.2436 steel, quenched from 940 C/oil
Carbides in 1.2436 steel, quenched from 980 C/air
Carbides in 1.2436 steel, quenched from 980 C/oil
Carbides in 1.2510 steel
Carbides in 1.2601 steel, quenched from 1000 C/air
Carbides in 1.2601 steel, quenched from 1000 C/oil
Carbides in 1.2601 steel, quenched from 1020 C/air
Carbides in 1.2601 steel, quenched from 1020 C/oil
Carbides in 1.2601 steel, quenched from 1040 C/air
Carbides in 1.2601 steel, quenched from 1040 C/oil
Carbides in 1.2601 steel, quenched from 1060 C/air
Carbides in 1.2601 steel, quenched from 1060 C/oil
Carbides in 1.2601 steel, quenched from 1080 C/air
Carbides in 1.2601 steel, quenched from 1080 C/oil
Carbides in 1.2601 steel, quenched from 1120 C/air
Carbides in 1.2601 steel, quenched from 1120 C/oil
Carbides in 1.2601 steel, quenched from 1160 C/air
Carbides in 1.2601 steel, quenched from 1160 C/oil
Carbides in 1.2601 steel, quenched from 1200 C/air
Carbides in 1.2601 steel, quenched from 1200 C/oil
Carbides in 1.2601 steel, quenched from 1240 C/air
Carbides in 1.2601 steel, quenched from 1240 C/oil
Carbides in 1.2601 steel, quenched from 900 C/air
Carbides in 1.2601 steel, quenched from 900 C/oil
Carbides in 1.2601 steel, quenched from 940 C/air
Carbides in 1.2601 steel, quenched from 940 C/oil
Carbides in 1.2601 steel, quenched from 980 C/air
Carbides in 1.2601 steel, quenched from 980 C/oil
Carbides in 1.4034 steel
Carbides in 1.4112 steel
Carbides in 12Cr and 8Cr steels
Carbides in 16MnCr5 steel - As-received steel
Carbides in 16MnCr5 steel - Heat treated steel I
Carbides in 16MnCr5 steel - Heat treated steel II
Carbides in 16MnCr5 steel - Heat treated steel III
Carbides in 1C-1.10Si-8Cr-2.70Mo-0.30V steel
Carbides in 2.25Cr-1Mo heat resistant steel
Carbides in 5% Cr-2% Mo-1% V steel for cold rolling
Carbides in AISI D2 steel
Carbides in AISI D2 steel
Carbides in D2 steel
Carbides in NCWV/D3 steel
Carbides in O6 steel
Carbides in Roltec PM steel
Carbides in SDK11 steel
Carbides in Vanadis 6 PM steel
Carbides in Vanadis 6 steel
Carbides in Vanadis PM steel
Carbides in W1 steel
Carbides in X155CrVMo121 steel
Carbides in X46Cr13 steel
Carbides in cold work tool steel
Carbides in cold work tool steel
Carbides in cold work tool steels (A2, D2, O1, S7, A8 and A11)
Carbides in forged 3.5% Cr and semi high speed steels
Carbides in quenched microstructures of A2 steel
Carbides in quenched microstructures of O1 steel
Carbides in steel 1.0C-10Cr-1Mo-0.25V
Carbides in steel 1.2080
Carbides in steel 1.2312
Carbides in steel 1.2363
Carbides in steel 1.2378
Carbides in steel 1.2379
Carbides in steel 1.2436
Carbides in steel 1.2519
Carbides in steel 1.2552
Carbides in steel 1.2601
Carbides in steel 1.2631
Carbides in steel 1.2690
Carbides in steel 1.2713
Carbides in steel 1.2726
Carbides in steel 1.2747
Carbides in steel 1.2827
Carbides in steel 1.2838
Carbides in steel 1.5C-12Cr
Carbides in steel 1.5C-12Cr
Carbides in steel 1.5C-12Cr-1Mo
Carbides in steel 1.5C-12Cr-1V
Carbides in steel 1.5C-12Cr-1V-1Mo
Carbides in steel 2C-12Cr
Carbides in steel AISI A8
Carbides in steel AISI A8 + W
Carbides in tempered microstructure of D2 steel
Carbides in tool steels with high chromium content
Cementite in W1 steel I
Cementite in W1 steel II
Chi carbides in 316L-type austenitic stainless steel
Chi carbides in ADT15 austenitic stainless steel
Chromium carbides in 3% chromium steel for rolls
Cr7C3 and Cr23C6 carbides in D3 steel
Cr7C3 and Cr3C2 carbides in the chromium carbide coated on AISI D2 steel
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Annealed condition
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Annealed condition
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Quenched from 1150 C/5 min
Cr7C3, V4C3, V8C7 carbides in X150 CrVMo 8-4 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Annealed condition
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Quenched from 1200 C/5 min
Cr7C3, V8C7 carbides in X150 CrVMo 8-4 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-4 steel - Annealed condition
Cr7C3, V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Annealed condition
Cr7C3, V8C7, V4C3; Mo2C, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Annealed condition
Cracking of primary carbides in cold work tool steels
Eta and epsilon carbides in Fe-12.2 wt.%Cr-0.84 wt.% Mo-0.43 wt.V-1.44 wt.% C steel (AISI D2)
Fe3C carbides in W1 steel
Fe3C, Fe7C3, (Fe,Cr)7C3 carbides in AISI O1 and D2 steels
Fine carbides of chromium, molybdenium and vanadium in the microstructure of TENASTEEL steel
Fracture surface of four-point bending test samples of cold work tool steel
Influence of austenitizing temperature on the microstructure of D2 tool steel
Influence of austenitizing temperature on the microstructure of D2 tool steel
Influence of starting microstructure on spheroidize annealed microstructure of W1 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Influence of starting microstructure on the spheroidize annealed microstructure of S5 tool steel
Lamellar pearlite and carbides in 0.82C-5.10Cr-0.28Mo steel
Lamellar pearlite and carbides in 0.95C-3.10Cr-0.14V-0.51Mo steel
Ledeburitic and secondary carbides in 1.2379 steel
Ledeburitic and secondary carbides in the low tempered microstructure of 1.2379 steel
M23C6 carbides in 1.4057 steel - Quenched from 1020 C
M23C6 carbides in 1.4057 steel - Quenched from 1020 C + slow cooling in the furnace
M23C6 carbides in 1.4057 steel - Soft annealed condition
M23C6 carbides in 316 and 316 L stainless steels
M23C6 carbides in AISI 304 austenitic stainless steel
M23C6 carbides in AISI 420 steel
M2C, M3C and M7C3 carbides in Caldie hot work tool steel
M3C carbides in 2CR steel
M3C carbides in 3CR steel
M3C carbides in 3CR50C steel
M3C carbides in 3CRMO steel
M3C, M7C3 and M23C6 carbides in X150CrMoV12-1 steel
M3C/M7C3 carbides in 4CRMO steel
M7C3 and M23C6 carbides in NCWV/D3 tool steel
M7C3 and M23C6 carbides in TENASTEEL steel
M7C3 carbides in 1.2379 steel
M7C3 carbides in 1.2379 steel
M7C3 carbides in 5CR steel
M7C3 carbides in 5CR80MO steel
M7C3 carbides in 5CRDH steel
M7C3 carbides in 5CRMO steel
M7C3 carbides in AISI D2 steel (bar diameters of 25.4, 70 and 210 mm)
M7C3 carbides in AISI D3 steel
M7C3 carbides in D2 steel
M7C3 carbides in D3 steel
M7C3 carbides in D3 tool steel
M7C3 carbides in PM Vanadis 6 steel
M7C3 carbides in SKD11 steel
M7C3 carbides in X155CrVMo12-1 steel
M7C3, M23C6 carbides in AISI 440A steel
M7C3, M23C6, VC and Mo2C carbides in forged steel rolls
MC and M3C carbides in cast AISI D3 steel
MC and M7C3 carbides in Thyrospray 2399 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in tool steels made by spray forming
MC, M2C and M6C carbides in K390 steel
MC, M6C, M7C3 and M23C6 carbides in 1.2690 steel
MC, M7C3 and M6C carbides in PM cold work tool steel
MC, M7C3 carbides in ROLTEC,TOUGHTEC, WEARTEC, AISI A2, D2 and D6 steels
Martensite and carbides in 0.82C-5.10Cr-0.28Mo steel
Martensite and carbides in 1.2436 steel
Martensite and carbides in 1.4112 steel
Martensite, primary and secondary carbides in 0.8C-8Cr-1.6Mo-0.6V steel
Microstructures of D2 steel vs. bar diameters
Network of eutectic carbides in alloyed white cast iron
Pearlite, primary and secondary carbides in 0.80C-0.85Si-3.0Cr-0.18Mo-0.20V steel
Precipitates in X2NiCoMo13-15-10 steel
Precipitates in austenitic steels
Precipitates in solution annealed 20Cr-25Ni steel
Primary and secondary carbides in 1.2363 steel
Primary and secondary carbides in 1.2379 steel
Primary carbides in D3 steel
Retained austenite in AISI D2 steel
Retained austenite in steel 1.2550
Retained austenite in steel 1.2842
SEM images of fracture surfaces in PM tool steel
Sigma phase and carbides heat resistant steel
Some properties of metallic hard materials
Spheroidized pearlite and carbides in 1.2631 steel
Spheroidized pearlite and carbides in 1.34C-0.85Si-0.67Mn-0.21Mo steel
Spheroidized pearlite and carbides in OH236NI steel
Spheroidized pearlite in S5 steel
Spheroidized pearlite in S5 steel
Tempered martensite and carbides in 0.85C-3.00Cr-0.13V-0.48Mo steel
Tempered martensite and carbides in 1.2235 steel
Tempered martensite and carbides in 1.2327 steel
Tempered martensite and carbides in 1.2375 steel
Tempered martensite and carbides in 1.2842 steel
Tempered martensite and carbides in 1.4125 steel
Tempered martensite and carbides in 1.4304 steel
Tempered martensite and carbides in X48CrMoV8-1-1 steel
Tempered martensite and primary and secondary carbides in 1.2379 steel
V8C7, (Fe3W3)C- (Fe4W2)C carbides in HS6-5-4 steel - Quenched from 1200 C/5 min
V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Quenched from 1200 C/5 min
V8C7, Mo2C, (Fe3W3)C - (Fe4W2)C carbides in 1.3344 steel - Annealed condition
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in 1.3344 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Quenched from 1200 C/5 min

Copyright © 2024 by Steel Data. All Rights Reserved.