Carbides in Structural Steels

(Cr) 23C6, V4C3 carbides in X190 CrVMo 20-4 steel - Annealed condition
(Cr) 7C3, V4C3 carbides in X190 CrVMo 20-4 steel - Quenched from 1200 C/5 min
(Cr,Fe)23C6 carbides in 1.4510 steel
(Cr,Fe)7C3 carbides in K110, PM steel K390 steels
(Cr,Fe)7C3, Fe3C and Fe23(C,B)6 carbides in white cast irons
(Cr,Mn)C carbides in TRIP steel
(Ti,Mo)C, M23C6 carbides in AIM1 steel
Atom maps of manganese and carbon from 1045 steel after tempering at 300°C
Carbide morphology of M2 tool steel
Carbide phases in T25 and P91 creep resisting steels
Carbide phases in high speed steels
Carbides in 0.17C-1.6Mn-0.52Si-0.083Cr steel
Carbides in 0.57C-1.96Si-0.16Mn-1.02Cr steel
Carbides in 1.2379 and UNIVERSAL steels (Acoustic Emission Test)
Carbides in 12Cr and 8Cr steels
Carbides in 16MnCr5 steel - As-received steel
Carbides in 16MnCr5 steel - Heat treated steel I
Carbides in 16MnCr5 steel - Heat treated steel II
Carbides in 16MnCr5 steel - Heat treated steel III
Carbides in 2.25Cr-1Mo steel
Carbides in 2.25Cr-1Mo weld/mild steel interface
Carbides in 51CrV4 steel
Carbides in AISI 2367 steel
Carbides in AISI M1 high speed steels
Carbides in AISI M2 steel
Carbides in AISI M42 steel
Carbides in Cr-Mo-V-B steel
Carbides in Cronidur 30 steel
Carbides in Damascus steel
Carbides in Damascus steel
Carbides in Fe-30.8Ni-26.6Cr alloy
Carbides in HK30 cast steel
Carbides in HP40 steel
Carbides in HiCr iron rolls
Carbides in HyperA white cast iron
Carbides in TRIP steel
Carbides in Vanadis 6 PM steel
Carbides in Vanadis PM steel
Carbides in advanced high strength steel (AHSS)
Carbides in austempered ductile iron (ADI)
Carbides in austenitic stainless steel with Ce
Carbides in carbon, chromium and high speed steel recoreded by AFM
Carbides in cast martensitic stainless steel
Carbides in heat affected zone of tool (HAZ) (1.2379 and 1.4718 steels)
Carbides in high strength spring steel
Carbides in medical drills made from the martensitic stainless steel
Carbides in spray-formed AISI M32 high-speed steel
Carbides in the cryogenic treated AISI M2 steel
Carbides in the white layer of AISI 52100 steel
Cementite (Fe3C) in C130W2 steel
Cementite (Fe3C) in Ck35 steel
Cementite and epsilon carbides in 100Cr6 martensitic bearing steel
Cementite and epsilon carbides in structural steels
Cementite in 100Cr6 steel
Cementite in DP-980 steel
Cementite in Dillidur 690 steel
Cementite in JIS-SCM440 steel
Cementite in Ni-Cr air-hardening steel
Cementite in S10C low carbon steel
Cementite in TWIP steel
Cementite in XC50 steel
Cementite in high strength steel
Cementite precipitation in quench-aged iron
Cementite types I, II and III in ancient wootz steel
Cementite, V(C,N) in 1.6919 steel
Chi carbides in 316L-type austenitic stainless steel
Chi carbides in ADT15 austenitic stainless steel
Cr23C6 and Cr7C3 carbides in heat resistant steel
Cr3C2 carbides in 75Cr3C2-25NiCr coating on P91 steel substrate
Cr3C6 and NbC carbides in 12% Cr ferritic steel
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Annealed condition
Cr7C3, (Cr,Fe) 7C3 carbides in D2 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Annealed condition
Cr7C3, V4C3 carbides in X230CrVMo13 4 steel - Quenched from 1150 C/5 min
Cr7C3, V4C3, V8C7 carbides in X150 CrVMo 8-4 steel - Quenched from 1150 C/15 min
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Annealed condition
Cr7C3, V4C3, V8C7 carbides in X290 VCrMo10-8 steel - Quenched from 1200 C/5 min
Cr7C3, V8C7 carbides in X150 CrVMo 8-4 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Annealed condition
Cr7C3, V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-4 steel - Annealed condition
Cr7C3, V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Annealed condition
Cr7C3, V8C7, V4C3; Mo2C, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Annealed condition
Epsilon and M3C carbides in 35MnCrMoV8-6-4-1 steel
Epsilon, M3C, M2C carbides in 30CrMoNiV10-25-6-2 steel
Epsilon, M3C, MC and M2C carbides in 0.30C-2.50Cr-2.60Mo-1.59Ni-0.18V hot work tool steel
Fe2MoC carbides in grade P11 SA335 steel
Fe3C and Mn carbides in Hadfield steel
Fe3C and Mo2C carbides in SA 508 Cl. 3 steel
Fe3C and NbC carbides in 0.14C-1.48Mn-0.78Si-0.052Nb steel
Fe3C and V4C3 carbides in 60CrV7 steel
Fe3C carbides in Fe-0.85Mo-2Ni-0.6C PM steel
Fe3C carbides in TRIP steel
Fe3C carbides in high strength steel (7 wt. % Ni and 2 wt. % Mn)
Fe3C carbides in line pipe steel
Fe3C, (Cr,Fe)7C3 and Fe23(C,B)6 carbides in chromium white cast iron
Fe3C, Cr7C3, Mo2C, and (Mn,Mo)2C carbides in 20MoCrS4 steel
Fe3C, M23C6 and VC carbides in X20CrMoV121 and P91 steels
Fe3C, VC, M7C3 and M23C6 carbides in heat resistant 12Kh1MF steel
Fine spherical cementite in 51100 steel
Grain boundary carbides in ultrahigh strength steel
Laves phase in AISI 441 steel I
Laves phase in AISI 441 steel II
Laves phase in AISI 441 steel III
Laves phase in AISI 441 steel IV
Laves phase in heat resistant steel
Laves phase in heat resistant steel
M(C,N), M2C, M6C carbides in AISI M2 steel
M23(C,B)6 carbides in microalloyed constructional steel
M23(CB)6, MX, M6C carbides in T11 and C9 creep resistant steels
M23C6 and Laves phase in HCM12A steel
M23C6 and M2X carbides in 9Cr-1Mo steel
M23C6 and M7C3 carbides in 2.25Cr–1.0Mo steel
M23C6 and VC carbides in HCM12 steel
M23C6 carbides in 11Cr-3.45W steel
M23C6 carbides in 11Cr–0.4Mo–2W–Cu–V–Nb steels
M23C6 carbides in 12Cr–2W–Cu–V–Nb creep resistant steel
M23C6 carbides in 15Cr–3W ferritic steel
M23C6 carbides in CB8 (9-12% Cr) steel
M23C6 carbides in DT4 series steels
M23C6 carbides in E911 creep resisting steel
M23C6 carbides in E911 steel
M23C6 carbides in FB2 steel
M23C6 carbides in Fe-18Mn-0.75C-1.7Al-0.5Si steel
M23C6 carbides in Fe-30.8 Ni-26.6 Cr steel
M23C6 carbides in HCM12A steel
M23C6 carbides in NF709 and NF709R steels
M23C6 carbides in NF709 and NF709R steels
M23C6 carbides in P9, P91, P92 and EP911 steels
M23C6 carbides in P91 creep resistant steel
M23C6 carbides in P91 steel
M23C6 carbides in P91 steel
M23C6 carbides in P91 steel
M23C6 carbides in P92 and P91 creep resistant steels
M23C6 carbides in P92 creep resistants steel
M23C6 carbides in P92 steel
M23C6 carbides in TENARIS grade 91 and 911 steels
M23C6 carbides in TWIP steel
M23C6 carbides in UNS S31803 steel
M23C6 carbides in X10CrMoVNb9-1 creep resisting steel
M23C6 carbides in X20, P91 steels
M23C6, M2C and M6C carbides in low alloy Cr-Mo-Ni-V steel
M23C6, M3C, M2C and M6C carbides in ASTM A387-22-CL2 steel
M23C6, M6C and M2C carbides in Cr-Mo-Ni-V steel for turbine rotor
M23C6, M6C and MC carbides in AISI 316, AISI 304, X6CrNiMoTi 17-12-2 steels
M23C6, M7C3 and VC carbides in 12X1M0 heat resistant steel
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M2C and M3C carbides in the cryogenic quenching of AISI A2 steel
M2C and M6C carbides in M42 steel
M2C, M3C, M23C6 and Cr7C3 carbides in 2.25Cr–1Mo (ASTM A387-22-CL2) steel
M2C, M3C, M23C6 and M7C3 carbides in 13CrMo4-5 steel
M2C, M6C carbides M23C6 in 10% Cr steel
M2C6 cabides in P92 martensitic chromium steel
M3C, M23C6 carbides in P91, P92 and E91 creep resistant steels
M3C, M7C3 and M23C6 carbides in Cr white cast iron
M6C carbides in AISI 347 steel
M6C carbides in HS6-5-2 high speed steel
M6C, M23C6 and NbC carbides in 347, HR120 and NF709 steels
M6C, M2C, M23C6 and M7C3 carbides in T24 creep resistant steel
M7C3 and M23C6 carbides in 2.25Cr-1.0Mo steel
M7C3 and M23C6 carbides in 2.4%C-30%Cr, 2.9% C-27%Cr steels
M7C3 and M23C6 carbides in high chromium cast iron I
M7C3 and M23C6 carbides in high chromium cast iron II
M7C3 and M23C6 carbides in high chromium cast iron III
M7C3 and M6C5 carbides in white cast Fe-Cr-C-V alloy
M7C3 carbides in 16% Cr white cast iron
M7C3 carbides in AISI D2 steel (bar diameters of 25.4, 70 and 210 mm)
M7C3 carbides in Cr white cast iron
M7C3 carbides in EutecticA white cast iron
M7C3 carbides in Fe-25Cr-3.1C-2.0Mn-0.7Si and Fe-25Cr-5.2C-2.1Mn-0.4Si high chromium cast irons
M7C3 carbides in HyperA white cast iron
M7C3 carbides in HyperEXP white cast iron
M7C3 carbides in HypoA white cast iron
M7C3 carbides in PM Vanadis 6 steel
M7C3 carbides in SKD11 steel
M7C3 carbides in WeldoverlayA and WeldoverlayB white cast irons
M7C3 carbides in WeldoverlayA white cast iron
M7C3 carbides in WeldoverlayB white cast iron
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6 and M6C carbides in 13HMF steel
M7C3, M23C6, MC and M3C carbides in G21CrMoV4 – 6 (L21HMF) low alloy cast steel
M7C3, M2C and MC carbides in semi-HSS grades
M7C3, M8C7, M23C6 carbides in 4Cr5MoSiV1 steel
M7C3, MC, M23C6 and M3C carbides in AISI H11 steel
MC (or M4C3), M23C6 and M6C carbides in AISI M2 steel
MC and M23C6 carbides in Armour steel
MC and M6C carbides in cast M2 high speed steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 PM steel
MC and M7C3 carbides in Vanadis 6 steel
MC and M7C3 carbides in Vanadis 6 steel
MC, M23C6 carbides in G-X 10CrNiMoNb18-10 steel
MC, M23C6 carbides in hot work tool steel
MC, M2C and M6C carbides in AISI M2 high speed steel manufactured by different casting technologies
MC, M2C carbides in HSS7 steel for rolls
MC, M2C, M3C, M7C3 and M23C6 carbides in 2CrMoNiWV creep resistant steel III
MC, M2C, M3C, M7C3 and M23C6 carbides in G21CrMoV4 – 6 (L21HMF) cast steel
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel IV
MC, M2C, M3C, M7C3, M23C6 and M6C carbides in 2CrMoNiWV creep resistant steel V
MC, M2C, M6C, M7C3 carbides in cast high speed steels (HSS) for rolls
MC, M2C, M7C3 and M23C6 carbides in cast high speed roll
MC, M7C3 and M2C carbides in cast high speed steel roll
MX, M3C carbides in 1.6957 steel
MX, M3C carbides in 1.8817 steel
MX, MX2, M23C6 carbides in 1.7734 steel
Mo2C and Ksi carbides in SA508 Gr3 nuclear reactor steel
Nanoscale precipitates in 13% Cr martensitic stainless steel
NbC and Cr23C6 carbides in high Cr (11 wt.%) tempered martensitic steel
NbC carbides in 347 and AL347HP steels
NbC, M23(B,C)6 and M2,3C carbides in hardfacing alloys
Pearlite-free and low-pearlite steel
Precipitates in 1.7279 steel
Precipitates in 20Cr-25Ni steel
Precipitates in 9% Cr steel with Co
Precipitates in AISI 347 stainless steel
Precipitates in HSLA steel
Precipitates in heat resistant steel
Primary and secondary carbides in the HAZ of 1.2379-1.4718 steels
Sigma phase and carbides heat resistant steel
Sigma phase in ASTM A890/A890M Grade 6A steel
Sigma phase in Mo stainless steel
TiC carbides in 0.42C–0.30Ti steel
Undissolved carbides in 0.062C-1.56Mn-0.36Cr low carbon steel
V(C, N) precipitates in fine-grained structural steel
V4C3 carbides in 2CrMoNiWV creep resistant steel I
V4C3, F2.4C and Fe3C carbides in high strength spring steel
V8C7, (Fe3W3)C- (Fe4W2)C carbides in HS6-5-4 steel - Quenched from 1200 C/5 min
V8C7, (Fe3W3)C-(Fe4W2)C carbides in HS10-2-5-8 steel - Quenched from 1200 C/5 min
V8C7, Mo2C, (Fe3W3)C – (Fe4W2)C carbides in 1.3344 steel - Annealed condition
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in 1.3344 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS6-5-3-9 steel - Quenched from 1200 C/5 min
V8C7, V4C3, (Fe3W3)C-(Fe4W2)C carbides in HS7-7-7-10 - Quenched from 1200 C/5 min
VC and M23C6 carbides in HCM12 steel
VC and W3Fe3C carbides in HSS6-5-2C high speed steel
VC carbides in Fe–1V–0.2C steels
VC carbides in cast high speed steel
VC carbides in high vanadium cast iron
VC, Fe3C, M7C3 and M23C6 carbides in 12X1MO steel
Vanadium carbides in H13 steel
Z-Phase in heat resistant steels