Carbides in Cast Irons

(Cr, Fe)7C3 carbides in chromium cast iron
(Cr, Fe)7C3 carbides in chromium cast iron
(Cr,Fe)7C3, Fe3C and Fe23(C,B)6 carbides in white cast irons
(Fe,Cr,Mo)7C3 and (Fe,Cr,Mo)3C carbides in Fe-3.3C-l6Cr-3Mo-lMn-0.5Si alloy
(Mo,Cr)2C carbides in Fe-1.7C-1.2Si-l.1Mn-0.8Ni-3.6Cr-1.7Mo-4.7V alloy
(Nb,Ti)C carbides in Fe-0.07C-1.35Mn-0.047Ti-0.086Nb steel
(V,Ta)C, VC and TaC carbides in Fe-V-Ta-C alloy
Alloy carbide in white cast iron
Alloy carbide in white cast iron
Carbides in 1.93C-20.9Cr-1.35W-0.57V steel
Carbides in 100Cr6 steel
Carbides in Damascus steel
Carbides in Fe-0.5C-0.7Mn steel
Carbides in Fe-30.8Ni-26.6Cr alloy
Carbides in HiCr iron rolls
Carbides in HyperA white cast iron
Carbides in austempered ductile iron (ADI)
Carbides in high speed steel
Cementite in 100Cr6 steel
Cementite in Ni-Hard cast iron
Cementite in Ni-Hard cast iron
Cementite in Nihard cast iron
Cementite in X12Cr13 steel
Cementite in XC50 steel
Cementite in chill cast hypoeutecic gray
Cementite in ductile cast iron
Cementite in ductile cast iron
Cementite in hyper-eutectic white cast iron
Cementite in ledeburite in Ni-Hard cast iron
Cementite in ledeburite in pearlitic ductile iron
Cementite in pearlitic ductile iron
Cementite in unalloyed white iron
Cementite in white cast iron
Cementite in white cast iron
Characteristic carbides (MC, M2C, M3C, M7C3, M23C6) in white cast iron
Chromium carbides in 100Cr6 steel
Coarse acicular chromium carbides in Fe – 2.95% C – 0.61% Mn – 29.3% Cr cast iron
Cr7C3 and Mo2C carbides in high Cr cast iron
Cr7C3 and Mo2C carbides in high chromium cast iron
Dendritic primary carbide NbC in stainless steel
Epsilon and cementite phases in carbon steel
Etchants for cast iron
Eutectic VC, NbC and M6C carbides in steel
Eutectic carbides in alloyed white cast iron
Fe3C and NbC carbides in 3.4C–0.9Si–0.7Mn–4.4Ni–1.8Cr–0.4Mo cast steel roll
Fe3C carbides in Ni Resist
Fe3C, (Cr,Fe)7C3 and Fe23(C,B)6 carbides in chromium white cast iron
Fe3W3C cabides in Fe-30W-4.3C alloy
Ferrite and carbides in 1.28C-1.04Si-24.7Cr-1.14Ni steel
Ledeburite in Fe – 4.0% C – 0.3% Si – 0.16% Mn – 0.91% Cr white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in white cast iron
Ledeburitic carbides ((Fe,Cr,Mo)3C) in nodular cast iron
Ledeburitic carbides in nodular cast iron
Ledeburitic carbides in nodular cast iron
Ledeburitic carbides in nodular cast iron
M(C,N), M2C, M6C carbides in AISI M2 steel
M23C6 and Fe3C carbides in X122Cr13 steel
M23C6 carbides in Fe-0.4C-25Cr-20Ni steel
M23C6 carbides in Fe-0.7C-14.5Cr-0.9Mo steel
M23C6 carbides in Fe-30.8 Ni-26.6 Cr steel
M23C6, M7C3 carbides in alloyed cast iron
M23C6, MC, M7C3 carbides and sigma phase in austenitic stainless steels
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M2C and M7C3 carbides in high-chromium white iron
M3C and M7C3 carbides in white cast iron
M3C carbides in GJN-HV 550 white cast iron
M3C carbides in mottled iron
M3C, M7C3 and M23C6 carbides in Cr white cast iron
M3C, M7C3 carbides in Fe-12Cr-1.6Mn-1.0Ni-0.5Si-4.1C white cast iron
M3C, M7C3 carbides in high-chromium white iron
M6C and Mo2C carbides in Fe-2.2C-20.5Mo steel
M6C carbides in Fe-0.52C-3.8Cr-0.5Mo-lV-18.8W tool steel
M6C carbides in Fe-23.3Mo-1.1C alloy
M6C carbides in Fe-Mo-C alloy
M6C carbides in Fe-W-C alloy
M6C carbides in Fe-l.3C-12.7Mo PM steel
M7C3 and M23C6 carbides in 18% Cr cast iron
M7C3 and M23C6 carbides in 0.5C-25Cr-24.5Ni-1.8W-1.9Si-1.9Mn alloy
M7C3 and M23C6 carbides in 2.4%C-30%Cr, 2.9% C-27%Cr steels
M7C3 and M23C6 carbides in high chromium cast iron I
M7C3 and M23C6 carbides in high chromium cast iron II
M7C3 and M23C6 carbides in high chromium cast iron III
M7C3 and M23C6 carbides in high chromium white iron
M7C3 and M3C carbides in Fe-1C-4.4Cr-l.6V alloy
M7C3 and M6C5 carbides in white cast Fe-Cr-C-V alloy
M7C3 and Mo2C carbides in Fe-0.9C-11.3Cr-0.7Mn-2.95Mo-0.3Si and Fe-1.33C-6.8Cr-2.4Mo-0.2Si steels
M7C3 and NbC carbides in Fe-2.1C-l4.7Cr-lNb alloy
M7C3 carbides in 15Cr-3Mo white cast iron
M7C3 carbides in 16% Cr white cast iron
M7C3 carbides in Cr white cast iron
M7C3 carbides in EutecticA white cast iron
M7C3 carbides in Fe-0.86C-23.8Cr-1.9Si-2.1 Ni alloy
M7C3 carbides in Fe-25Cr-3.1C-2.0Mn-0.7Si and Fe-25Cr-5.2C-2.1Mn-0.4Si high chromium cast irons
M7C3 carbides in Fe-2C-12Cr tool steel
M7C3 carbides in HyperA white cast iron
M7C3 carbides in HyperEXP white cast iron
M7C3 carbides in HypoA white cast iron
M7C3 carbides in WeldoverlayA and WeldoverlayB white cast irons
M7C3 carbides in WeldoverlayA white cast iron
M7C3 carbides in WeldoverlayB white cast iron
M7C3 carbides in high-chromium white cast iron
M7C3 carbides in high-chromium white cast iron (17% Cr)
M7C3, (Fe,Cr)23C6 and Mo2C carbides in high alloyed chromium cast iron
M8C7 and M6C carbides in high speed steel for the work rolls
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C and M7C3 carbides in cast high speed steel roll
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M7C3 and M23C6 carbides in high speed steel roll
MC, M2C, M7C3 carbides in Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C cast steel
MC, M2C, M7C3, M23C6 carbides in cast HSS roll
MC, M3C and M7C3 carbides in high chromium cast iron
Massive cementite in Ni-Hard cast iron
Mo2C and (Fe,Cr)7C3 carbides in high Cr white cast iron Fe-21Cr-3Ni-1.7Mo-2.4C
Mo2C carbides in Fe-0.35C-0.9Mo steel
Mo2C carbides in Fe-C-Mo steel
NbC carbide in Nb cast iron
NbC in cast irons
Network of eutectic carbides in alloyed white cast iron
Primary and secondary carbides in Cr-Hard (Maxidur) cast iron
Primary carbides in cast irons
Primary carbides in white cast iron
Proeutectic cementite in NiHardcast iron
Proeutectic cementite in heat treated Ni-Hard cast iron
V6C5 carbides in microalloyed steel
VC and M7C3 carbides in Fe-2.4C-5.4Cr-6V alloy
VC and TiC carbides in Fe-0.049C-0.3Mn-0.126V, Fe-0.38C-1.5Mn-0.5Si-O.1V, Fe-0.052C-0.18Mn-0.12Ti steels
VC carbides in Fe-2.4C-0.9Si-0.9Mn-0.1 Ni-2.9Cr-3.4Mo-5-9V alloy
VC carbides in Fe-3.3C-9.2V-2Si steel
VC carbides in high vanadium cast iron
Vanadium rich carbides in cast high speed steels
Widmanstatten cementite in Fe-1.34 C-13.1 Mn steel