Carbides in White Cast Irons

(Cr,Fe)7C3, Fe3C and Fe23(C,B)6 carbides in white cast irons
(Mo,Cr)2C carbides in Fe-1.7C-1.2Si-l.1Mn-0.8Ni-3.6Cr-1.7Mo-4.7V alloy
Alloy carbide in white cast iron
Alloy carbide in white cast iron
Carbides in Damascus steel
Carbides in HyperA white cast iron
Cementite in Ni-Hard cast iron
Cementite in chill cast hypoeutecic gray
Cementite in hyper-eutectic white cast iron
Cementite in white cast iron
Cementite in white cast iron
Characteristic carbides (MC, M2C, M3C, M7C3, M23C6) in white cast iron
Eutectic carbides in alloyed white cast iron
Fe3C, (Cr,Fe)7C3 and Fe23(C,B)6 carbides in chromium white cast iron
Ledeburite in Fe – 4.0% C – 0.3% Si – 0.16% Mn – 0.91% Cr white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in eutectic white cast iron
Ledeburite in white cast iron
M23C6, M7C3 carbides in alloyed cast iron
M23C6, MC, M7C3 carbides and sigma phase in austenitic stainless steels
M2C and M3C carbides in Ni-Hard Iron class I Type B white cast iron
M3C and M7C3 carbides in white cast iron
M3C carbides in GJN-HV 550 white cast iron
M3C, M7C3 and M23C6 carbides in Cr white cast iron
M3C, M7C3 carbides in Fe-12Cr-1.6Mn-1.0Ni-0.5Si-4.1C white cast iron
M6C carbides in Fe-W-C alloy
M7C3 and M6C5 carbides in white cast Fe-Cr-C-V alloy
M7C3 carbides in 15Cr-3Mo white cast iron
M7C3 carbides in 16% Cr white cast iron
M7C3 carbides in Cr white cast iron
M7C3 carbides in EutecticA white cast iron
M7C3 carbides in Fe-25Cr-3.1C-2.0Mn-0.7Si and Fe-25Cr-5.2C-2.1Mn-0.4Si high chromium cast irons
M7C3 carbides in HyperA white cast iron
M7C3 carbides in HyperEXP white cast iron
M7C3 carbides in HypoA white cast iron
M7C3 carbides in WeldoverlayA and WeldoverlayB white cast irons
M7C3 carbides in WeldoverlayA white cast iron
M7C3 carbides in WeldoverlayB white cast iron
M7C3 carbides in high-chromium white cast iron
M7C3 carbides in high-chromium white cast iron (17% Cr)
M7C3, (Fe,Cr)23C6 and Mo2C carbides in high alloyed chromium cast iron
MC, M2C and M7C3 carbides in Wear resistant cast iron for rolls
MC, M2C and M7C3 carbides in cast high speed steel roll
MC, M2C, M6C and M7C3 carbides in 2%C–5%Cr–5%V–5%Mo–5%W–5%Co white cast iron
MC, M2C, M7C3 carbides in Fe-5%Cr-5%Mo-5%W-5%V-5%Co-2.0%C cast steel
MC, M3C and M7C3 carbides in high chromium cast iron
Mo2C and (Fe,Cr)7C3 carbides in high Cr white cast iron Fe-21Cr-3Ni-1.7Mo-2.4C
NbC carbide in Nb cast iron
Network of eutectic carbides in alloyed white cast iron
Primary carbides in white cast iron
VC carbides in high vanadium cast iron